METHOD AND APPARATUS FOR CALCINING SALT SOLUTIONS
Patent
·
OSTI ID:4069858
A method is given for converting uranyl nitrate solution into solid UO/ sub 3/, The solution is sprayed horizontally into a fluidized bed of UO/sub 3/ particles at 310 to 350 deg C by a nozzle of the coaxial air jet type at about 26 psig, Under these conditions the desired conversion takes place, and caking in the bed is avoided.
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-15-012989
- Assignee:
- U.S. Atomic Energy Commission
- Patent Number(s):
- US 2981592
- OSTI ID:
- 4069858
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-61
- Country of Publication:
- United States
- Language:
- English
Similar Records
DESCRIPTION OF AN INSTALLATION FOR THE PRODUCTION OF URANIUM TRIOXIDE BY CALCINATION IN FLUIDIZED BED OF SOLUTIONS OF URANYL NITRATE
Development of an Immobilisation Technology for Radioactive Waste Solution from Mo-99 Production
HOMOGENEOUS REACTOR PROGRAM PROGRESS REPORT FOR PERIOD FROM AUGUST 1 TO NOVEMBER 30, 1960
Journal Article
·
Mon Apr 01 00:00:00 EST 1963
· Energia Nucl. (Madrid)
·
OSTI ID:4069858
Development of an Immobilisation Technology for Radioactive Waste Solution from Mo-99 Production
Conference
·
Sat Jul 01 00:00:00 EDT 2006
·
OSTI ID:4069858
HOMOGENEOUS REACTOR PROGRAM PROGRESS REPORT FOR PERIOD FROM AUGUST 1 TO NOVEMBER 30, 1960
Technical Report
·
Wed Mar 01 00:00:00 EST 1961
·
OSTI ID:4069858