A process is given for anodically treating the surface of uranium articles, prior to metal plating. The metal is electrolyzed in an aqueous solution of about 10% polycarboxylic acid, preferably oxalic acid, from 1 to 5% by weight of glycerine and from 1 to 5% by weight of hydrochloric acid at from 20 to 75 deg C for from 30 seconds to 15 minutes. A current density of from 60 to 100 amperes per square foot is used.
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-15-016895
- Assignee:
- U.S. Atomic Energy Commission
- Patent Number(s):
- US 2982702
- OSTI ID:
- 4038167
- Country of Publication:
- United States
- Language:
- English
Similar Records
METHOD OF ELECTROPOLISHING URANIUM
TREATMENT OF URANIUM SURFACES
ANODIC TREATMENT OF URANIUM
Patent
·
Tue Jul 14 00:00:00 EDT 1959
·
OSTI ID:4206340
TREATMENT OF URANIUM SURFACES
Patent
·
Sat Jan 31 23:00:00 EST 1959
·
OSTI ID:4264402
ANODIC TREATMENT OF URANIUM
Patent
·
Sat Jan 31 23:00:00 EST 1959
·
OSTI ID:4253449