Minimum bar size for flexure testing of irradiated SiC/SiC composite
- Pacific Northwest National Lab., Richland, WA (United States)
This report covers material presented at the IEA/Jupiter Joint International Workshop on SiC/SiC Composites for Fusion structural Applications held in conjunction with ICFRM-8, Sendai, Japan, Oct. 23-24, 1997. The minimum bar size for 4-point flexure testing of SiC/SiC composite recommended by PNNL for irradiation effects studies is 30 {times} 6 {times} 2 mm{sup 3} with a span-to-depth ratio of 10/1.
- Research Organization:
- Oak Ridge National Lab., TN (United States)
- Sponsoring Organization:
- USDOE, Washington, DC (United States)
- DOE Contract Number:
- AC06-76RL01830
- OSTI ID:
- 335386
- Report Number(s):
- DOE/ER--0313/23; ON: DE98004697
- Country of Publication:
- United States
- Language:
- English
Similar Records
Methods of radiation effects evaluation of SiC/SiC composite and SiC fibers
High thermal conductivity SiC/SiC composites for fusion applications -- 2
Summary Report on the US/Japan Jupiter Collaboration Integrated Focus on Fundamental Studies - Vanadium Initiative
Technical Report
·
Sat Feb 28 23:00:00 EST 1998
·
OSTI ID:335383
High thermal conductivity SiC/SiC composites for fusion applications -- 2
Technical Report
·
Sat Feb 28 23:00:00 EST 1998
·
OSTI ID:335385
Summary Report on the US/Japan Jupiter Collaboration Integrated Focus on Fundamental Studies - Vanadium Initiative
Book
·
Mon Oct 01 00:00:00 EDT 2001
·
OSTI ID:984269