Li-alloy electrode for Li-alloy/metal sulfide cells
Patent
·
OSTI ID:264559
A method of making a negative electrode is described, the electrode made thereby and a secondary electrochemical cell using the electrode. Lithium, silicon and nickel is alloyed in a prescribed proportion forming an electroactive material, to provide an improved electrode and cell. 7 figs.
- Research Organization:
- University of Chicago
- DOE Contract Number:
- W-31109-ENG-38
- Assignee:
- PTO; SCA: 250903; PA: EDB-96:119556; SN: 96001625920
- Patent Number(s):
- US 5,536,600/A/
- Application Number:
- PAN: 8-311,627
- OSTI ID:
- 264559
- Country of Publication:
- United States
- Language:
- English
Similar Records
Li-alloy electrode for Li-alloy/metal sulfide cells
Lithium aluminum/iron sulfide battery having lithium aluminum and silicon as negative electrode
Lithium aluminum/iron sulfide battery having lithium aluminum and silicon as negative electrode
Patent
·
Sun Dec 31 23:00:00 EST 1995
·
OSTI ID:870512
Lithium aluminum/iron sulfide battery having lithium aluminum and silicon as negative electrode
Patent
·
Sat Dec 31 23:00:00 EST 1983
·
OSTI ID:865285
Lithium aluminum/iron sulfide battery having lithium aluminum and silicon as negative electrode
Patent
·
Mon Dec 17 23:00:00 EST 1984
·
OSTI ID:5869673