Key results from examinations of seven high burnup pressurized water reactor spent nuclear fuel rods

Journal Article · · Frontiers in Nuclear Engineering

At present, spent nuclear fuel (SNF) assemblies discharged from US commercial power plants are placed into dry storage following a short cooling time (<10 years) in the plant’s spent fuel pool. The process of packaging the spent fuel into dry-storage canisters includes a drying step to remove residual water from the canister. During the drying process, the fuel rod cladding may reach temperatures as high as 400°C. Oak Ridge National Laboratory (ORNL) is performing destructive examinations of high burnup (HBU) (>45 GWd/MTU) SNF rods to address knowledge and data gaps related to extended interim storage and eventual transportation for disposal. The rods examined include four different kinds of fuel rod cladding: standard Zircaloy-4 (Zirc-4), low-tin (LT) Zirc-4, ZIRLO, and M5. Three rods were subjected to a thermal transient to assess the effects of decay-heat-driven high temperatures expected during vacuum drying of the fuel as it is prepared for interim dry storage. The examinations focus on the composite fuel rod performance, as compared with the performance of defueled rod cladding, and establish the baseline mechanical properties of a fuel rod before interim dry storage. The key results of these examinations are presented, including the measured mechanical and fatigue properties, observations of cladding hydrogen pickup and hydride reorientation effects on rod performance, effects of the simulated drying temperatures on rod performance, and general conclusions of SNF performance in extended interim dry storage and transport. The rods were found to be strong and durable in the expected loading conditions, even considering the formation of radial hydrides associated with vacuum drying. The combined testing provides a broad body of data supporting extended interim storage and transportation performance of HBU spent fuel.

Sponsoring Organization:
USDOE
OSTI ID:
2326244
Alternate ID(s):
OSTI ID: 2349209
Journal Information:
Frontiers in Nuclear Engineering, Journal Name: Frontiers in Nuclear Engineering Vol. 3; ISSN 2813-3412
Publisher:
Frontiers Media SACopyright Statement
Country of Publication:
Switzerland
Language:
English

References (11)

Pellet-clad interaction (PCI) failures of zirconium alloy fuel cladding — A review journal August 1990
Fission recoil-induced microstructural evolution of the fuel-cladding interface [FCI] in high burnup BWR fuel journal August 2019
Measurement and modeling of the gas permeability of high burnup pressurized water reactor fuel rods journal September 2019
Metallographic examinations and hydrogen measurements of high-burnup spent nuclear fuel cladding journal February 2024
High burn-up spent nuclear fuel transport reliability investigation journal April 2018
Key Results from Detailed Nondestructive Examinations of 25 Pressurized Water Reactor High Burnup Spent Nuclear Fuel Rods journal February 2019
Corrosion of Zirconium Alloys Used for Nuclear Fuel Cladding journal July 2015
Fatigue Design Basis for Zircaloy Components journal September 1964
Post Irradiation Examination Plan for High-Burnup Demonstration Project Sister Rods report April 2016
Sister Rod Nondestructive Examination Final Report report May 2018
Sister Rod Destructive Examinations (FY22) report January 2023

Similar Records

Sister Rod Destructive Examinations (FY2021) Appendix B: Segmentation, Defueling, Metallographic Data and Total Cladding Hydrogen
Technical Report · Thu Mar 31 00:00:00 EDT 2022 · OSTI ID:1864439

Sister Rod Destructive Examinations (FY23)
Technical Report · Tue Jan 30 23:00:00 EST 2024 · OSTI ID:2502196

Related Subjects