Thermoelectric properties of Bi{sub 2}Te{sub 2.4}Se{sub 0.6} solid solutions of different particle-size composition
- Russian Academy of Sciences, Baikov Institute of Metallurgy and Materials Science (Russian Federation)
- Scientific-Production Association “Crystal” (Russian Federation)
The thermoelectric properties of n-type Bi{sub 2}Te{sub 2.4}Se{sub 0.6} solid solution prepared by the vacuum hot pressing of powder mixtures with different particle sizes are investigated. The powders were prepared by the mechanical grinding of ingots and melt spinning. The microstructure and fracture pattern of a sample cleavage surface are analyzed using scanning electron microscopy and optical microscopy. The thermoelectric characteristics (the Seebeck coefficient, electrical conductivity, and thermal conductivity) are measured at room temperature and in the temperature range of 100–700 K.
- OSTI ID:
- 22756426
- Journal Information:
- Semiconductors, Journal Name: Semiconductors Journal Issue: 8 Vol. 51; ISSN SMICES; ISSN 1063-7826
- Country of Publication:
- United States
- Language:
- English
Similar Records
Thermoelectric properties of the hot-pressed (Bi,Sb){sub 2}(Te,Se){sub 3} alloys
Anisotropy analysis of thermoelectric properties of Bi{sub 2}Te{sub 2.9}Se{sub 0.1} prepared by SPS method
Thermoelectric properties of sintered {ital n} and {ital p} type Bi{sub 2}Te{sub 3}
Journal Article
·
Fri Mar 31 23:00:00 EST 2000
· Scripta Materialia
·
OSTI ID:20075952
Anisotropy analysis of thermoelectric properties of Bi{sub 2}Te{sub 2.9}Se{sub 0.1} prepared by SPS method
Journal Article
·
Tue Jun 26 00:00:00 EDT 2012
· AIP Conference Proceedings
·
OSTI ID:22068986
Thermoelectric properties of sintered {ital n} and {ital p} type Bi{sub 2}Te{sub 3}
Journal Article
·
Wed Aug 10 00:00:00 EDT 1994
· AIP Conference Proceedings
·
OSTI ID:172174