X-ray micro-tomography investigation of the foaming process in the system of waste glass–silica mud–MnO{sub 2}
- ZAG Ljubljana, Dimičeva 12, 1000 Ljubljana (Slovenia)
- NTF, Aškerčeva 12, 1000 Ljubljana (Slovenia)
In case of foamed lightweight aggregates (LWAs), porosity is introduced by the addition of a foaming agent to the glassy matrix, which degasses at an elevated temperature, so that the resulting gases remain trapped inside the glassy structure. The efficiency of action of MnO{sub 2} as a foaming agent in waste glass and waste glass/silica mud systems was studied. Samples were fired at different temperatures and with different dwelling times at a certain temperature, and the development of porosity was investigated by means of X-ray micro-tomography. It was found that, with the prolongation in dwelling times, the number of pores decreased, while, on the other hand, the volume of these pores increased, and that the addition of silica mud increases the foaming temperature and slows down the foaming process. - Highlights: • Preparation of lightweight aggregate from waste glass, silica sludge, and MnO{sub 2} • DTA/TG investigation of MnO{sub 2} • Characterization of pore-forming process by means of X-ray micro-tomography (μcT)
- OSTI ID:
- 22288716
- Journal Information:
- Materials Characterization, Vol. 86; Other Information: Copyright (c) 2013 Elsevier Science B.V., Amsterdam, The Netherlands, All rights reserved.; Country of input: International Atomic Energy Agency (IAEA); ISSN 1044-5803
- Country of Publication:
- United States
- Language:
- English
Similar Records
The distribution and mechanism of pore formation in copper foams fabricated by Lost Carbonate Sintering method
Preparation of amine-impregnated silica foams using agar as the gelling agent