Theoretical and experimental foundations for preparing coke for blast-furnace smelting
Journal Article
·
· Metallurgist (English Translation)
- Enakievo Metallurgical Plant, Enakievo (Ukraine)
This article examines the preparation of coke for blast-furnace smelting by a method that most fully meets the requirements of blast-furnace technology: screening of the -36 mm fraction, the separation of nut coke of the 15-36 mm fraction, and its charging into the furnace in a mixture with the iron-ore-bearing charge components. An analysis is made of trial use of coke of the Premium class on blast furnace No. 5 at the Enakievo Metallurgical Plant. Use of this coke makes it possible to reduce the consumption of skip coke by 3.2-4.1%.
- OSTI ID:
- 21262001
- Journal Information:
- Metallurgist (English Translation), Vol. 53, Issue 5/6; ISSN 0026-0894
- Country of Publication:
- United States
- Language:
- English
Similar Records
Blast-furnace operation on cokes made under differing carbonizing temperature conditions. [950 to 1050/sup 0/C coke finishing temperature]
Size and mechanical strength of blast-furnace coke
Production and blast-furnace smelting of boron-alloyed iron-ore pellets
Journal Article
·
Sat Jan 01 00:00:00 EST 1977
· Coke Chem., USSR (Engl. Transl.); (United States)
·
OSTI ID:21262001
+7 more
Size and mechanical strength of blast-furnace coke
Journal Article
·
Sat Jan 01 00:00:00 EST 1977
· Coke Chem., USSR (Engl. Transl.); (United States)
·
OSTI ID:21262001
Production and blast-furnace smelting of boron-alloyed iron-ore pellets
Journal Article
·
Fri Aug 15 00:00:00 EDT 2008
· Steel in Translation
·
OSTI ID:21262001