Temporal evolution of a model Co-Al-W superalloy aged at 650 °C and 750 °C
Journal Article
·
· Acta Materialia
- Sponsoring Organization:
- USDOE Office of Science (SC), Basic Energy Sciences (BES)
- Grant/Contract Number:
- FG02-98ER45721
- OSTI ID:
- 1694061
- Journal Information:
- Acta Materialia, Journal Name: Acta Materialia Vol. 159 Journal Issue: C; ISSN 1359-6454
- Publisher:
- ElsevierCopyright Statement
- Country of Publication:
- United States
- Language:
- English
Cited by: 24 works
Citation information provided by
Web of Science
Web of Science
Similar Records
Temporal evolution of a model Co-Al-W superalloy aged at 650 °C and 750 °C
Energetics of antiphase boundaries in γ′ Co3(Al,W)-based superalloys
Effect of tungsten concentration on microstructures of Co-10Ni-6Al-(0,2,4,6)W-6Ti (at%) cobalt-based superalloys
Journal Article
·
Mon Oct 01 00:00:00 EDT 2018
· Acta Materialia
·
OSTI ID:1694061
+1 more
Energetics of antiphase boundaries in γ′ Co3(Al,W)-based superalloys
Journal Article
·
Fri Jan 01 00:00:00 EST 2016
· Acta Materialia
·
OSTI ID:1694061
Effect of tungsten concentration on microstructures of Co-10Ni-6Al-(0,2,4,6)W-6Ti (at%) cobalt-based superalloys
Journal Article
·
Sat Jul 01 00:00:00 EDT 2017
· Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing
·
OSTI ID:1694061
+3 more