The ultimate mineral processing challenge: Recovery of rare earths, phosphorus and uranium from Florida phosphatic clay

Journal Article · · Minerals and Metallurgical Processing
DOI:https://doi.org/10.19150/mmp.7858· OSTI ID:1439932
 [1];  [1];  [1];  [2]
  1. Florida Industrial and Phosphate Research Institute, Bartow, FL (United States)
  2. Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
We report phosphate beneficiation in Florida generates more than one tonne of phosphatic clay, or slime, per tonne of phosphate rock produced. Since the start of the practice of large-scale washing and desliming for phosphate beneficiation, more than 2 Gt of slime has accumulated, containing approximately 600 Mt of phosphate rock, 600 kt of rare earth elements (REEs) and 80 million kilograms of uranium. The recovery of these valuable elements from the phosphatic clay is one of the most challenging endeavors in mineral processing, because the clay is extremely dilute, with an average solids concentration of 3 percent, and fine in size, with more than 50 percent having particle size smaller than 2 μm, and it contains nearly 50 percent clay minerals as well as large amounts of magnesium, iron and aluminum. With industry support and under funding from the Critical Materials Institute, the Florida Industrial and Phosphate Research Institute in conjunction with the Oak Ridge National Laboratory undertook the task to recover phosphorus, rare earths and uranium from Florida phosphatic clay. This paper presents the results from the preliminary testing of two approaches. The first approach involves three-stage cycloning using cyclones with diameters of 12.4 cm (5 in.), 5.08 cm (2 in.) and 2.54 cm (1 in.), respectively, to remove clay minerals followed by flotation and leaching. The second approach is a two-step leaching process. In the first step, selective leaching was conducted to remove magnesium, thus allowing the production of phosphoric acid suitable for the manufacture of diammonium phosphate (DAP) in the second leaching step. The results showed that multistage cycloning with small cyclones is necessary to remove clay minerals. Finally, selective leaching at about pH 3.2 using sulfuric acid was found to be effective for removing more than 80 percent of magnesium from the feed with minimal loss of phosphorus.
Research Organization:
Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
Sponsoring Organization:
USDOE Office of Energy Efficiency and Renewable Energy (EERE)
Grant/Contract Number:
AC05-00OR22725
OSTI ID:
1439932
Journal Information:
Minerals and Metallurgical Processing, Journal Name: Minerals and Metallurgical Processing Journal Issue: 4 Vol. 34; ISSN 0747-9182
Publisher:
Society for Mining, Metallurgy & ExplorationCopyright Statement
Country of Publication:
United States
Language:
English

Similar Records

Fluorine and uranium in phosphate rock processing and waste materials. Report of investigations/1981
Technical Report · Thu Dec 31 23:00:00 EST 1981 · OSTI ID:5140439

Rare-earth leaching from Florida phosphate rock in wet-process phosphoric acid production
Journal Article · Mon Jul 31 20:00:00 EDT 2017 · Minerals and Metallurgical Processing · OSTI ID:1394450

The Recovery of uranium from phosphatic sources in relation to the E. E. C
Technical Report · · OSTI ID:6860618

Related Subjects