Stabilization of [Ru(bpy)2 (4,4'-(PO3 H2)bpy)]2+ on Mesoporous TiO2 with Atomic Layer Deposition of Al2 O3
- Department of Chemistry, University of North Carolina at Chapel Hill, Chapel Hill, North Carolina 27599, United States
- Department of Chemical and Biomolecular Engineering, North Carolina State University, Raleigh, North Carolina 27695, United States
- Research Organization:
- Energy Frontier Research Centers (EFRC) (United States). Center for Solar Fuels (UNC EFRC)
- Sponsoring Organization:
- USDOE Office of Science (SC), Basic Energy Sciences (BES)
- DOE Contract Number:
- SC0001011
- OSTI ID:
- 1387191
- Journal Information:
- Chemistry of Materials, Vol. 25, Issue 1; Related Information: UNC partners with University of North Carolina (lead); Duke University; University of Florida; Georgia Institute of Technology; University; North Carolina Central University; Research Triangle Institute; ISSN 0897-4756
- Publisher:
- American Chemical Society (ACS)
- Country of Publication:
- United States
- Language:
- English
Similar Records
Interfacial Electron Transfer Dynamics for [Ru(bpy) 2 ((4,4'-PO 3 H 2 ) 2 bpy)] 2+ Sensitized TiO 2 in a Dye-Sensitized Photoelectrosynthesis Cell: Factors Influencing Efficiency and Dynamics
Interfacial Electron Transfer Dynamics for [Ru(bpy)2((4,4'-PO3H2)2 bpy)]2+ Sensitized TiO2 in a Dye-Sensitized Photoelectrosynthesis Cell: Factors Influencing Efficiency and Dynamics
Copper uranyl phosphate and arsenate incorporating an organic ligand with a pillared layer structure: [Cu(4,4 Prime -bpy)(UO{sub 2}){sub 0.5}(HPO{sub 4})(H{sub 2}PO{sub 4})]{center_dot}H{sub 2}O and [Cu(4,4 Prime -bpy)(UO{sub 2}){sub 0.5}(HAsO{sub 4})(H{sub 2}AsO{sub 4})]{center_dot}1.5H{sub 2}O
Journal Article
·
Thu Apr 14 00:00:00 EDT 2011
· Journal of Physical Chemistry. C
·
OSTI ID:1387191
+6 more
Interfacial Electron Transfer Dynamics for [Ru(bpy)2((4,4'-PO3H2)2 bpy)]2+ Sensitized TiO2 in a Dye-Sensitized Photoelectrosynthesis Cell: Factors Influencing Efficiency and Dynamics
Journal Article
·
Thu Apr 14 00:00:00 EDT 2011
· Journal of Physical Chemistry. C
·
OSTI ID:1387191
+6 more
Copper uranyl phosphate and arsenate incorporating an organic ligand with a pillared layer structure: [Cu(4,4 Prime -bpy)(UO{sub 2}){sub 0.5}(HPO{sub 4})(H{sub 2}PO{sub 4})]{center_dot}H{sub 2}O and [Cu(4,4 Prime -bpy)(UO{sub 2}){sub 0.5}(HAsO{sub 4})(H{sub 2}AsO{sub 4})]{center_dot}1.5H{sub 2}O
Journal Article
·
Tue Jan 15 00:00:00 EST 2013
· Journal of Solid State Chemistry
·
OSTI ID:1387191