Mesoporous carbons and polymers
A polymer is prepared by polymerizing a polymerizable component from a mixture containing the polymerizable component and a surfactant, the surfactant and the polymerizable component being present in the mixture in a molar ratio of at least 0.2:1, having an average pore size greater than 4 nm and a density greater than 0.1 g/cc. The polymerizable component can comprise a resorcinol/formaldehyde system and the mixture can comprise an aqueous solution or the polymerizable component can comprise a divinylbenzene/styrene system and the mixture can comprise an organic solution. Alternatively, the polymerizable component can comprise vinylidene chloride or a vinylidene chloride/divinylbenzene system. The polymer may be monolithic, have a BET surface area of at least about 50 m.sup.2 /g., include a quantity of at least one metal powder, or have an electrical conductivity greater than 10 Scm.sup.-1.
- Research Organization:
- TDA Research, Inc., Wheat Ridge, CO (Unites States)
- Sponsoring Organization:
- USDOE
- DOE Contract Number:
- FG03-92ER81320
- Assignee:
- TDA Research, Inc. (Wheat Ridge, CO)
- Patent Number(s):
- 6,737,445
- Application Number:
- 09/933,521
- OSTI ID:
- 1174850
- Country of Publication:
- United States
- Language:
- English
Similar Records