Impact of Superalloy Composition, Bond Coat Roughness and Water Vapor on TBC Lifetime with HVOF NiCoCrAlYHfSi Bond Coatings
Conference
·
OSTI ID:1113157
- ORNL
- Research Organization:
- Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
- Sponsoring Organization:
- FE USDOE - Office of Fossil Energy (FE)
- DOE Contract Number:
- DE-AC05-00OR22725
- OSTI ID:
- 1113157
- Resource Relation:
- Conference: International Conference for Metallurgical Coatings and Thin Films, San Diego, CA, USA, 20130429, 20130503
- Country of Publication:
- United States
- Language:
- English
Similar Records
APS TBC performance on directionally-solidified superalloy substrates with HVOF NiCoCrAlYHfSi bond coatings
The Effect of Cycle Frequency, H2O and CO2 on TBC Lifetime with NiCoCrAlYHfSi Bond Coatings
Effect of Superalloy Substrate and Bond Coating on TBC Lifetime
Journal Article
·
Fri Sep 04 00:00:00 EDT 2015
· Surface and Coatings Technology
·
OSTI ID:1113157
+1 more
The Effect of Cycle Frequency, H2O and CO2 on TBC Lifetime with NiCoCrAlYHfSi Bond Coatings
Conference
·
Wed Jan 01 00:00:00 EST 2014
·
OSTI ID:1113157
+1 more
Effect of Superalloy Substrate and Bond Coating on TBC Lifetime
Conference
·
Fri Jan 01 00:00:00 EST 2010
·
OSTI ID:1113157