Title: General Corrosion and Localized Corrosion of the Drip Shield

Abstract

The recommended waste package (WP) design is described in BSC (2001a). The design includes a double-wall WP underneath a protective drip shield (DS) (BSC 2003a). The purpose of the process-level models developed in this report is to model dry oxidation (DOX), general corrosion (GC) and localized corrosion (LC) of the DS plate material, which is made of Ti Grade 7. The DS design also includes structural supports fabricated from Ti Grade 24. Degradation of Ti Grade 24 is not considered in this report. The DS provides protection for the waste package outer barrier (WPOB) both as a barrier to seepage water contact and a physical barrier to potential rockfall. This Model Report (MR) serves as a feed to the Integrated Waste Package Degradation Model (IWPD) analyses, and was developed in accordance with the Technical Work Plan (TWP) (BSC 2002a). The models contained in this report serve as a basis to determine whether or not the performance requirements for the DS can be met.

Authors:
;
Publication Date:
Research Org.:
Yucca Mountain Project, Las Vegas, NV (United States)
Sponsoring Org.:
US Department of Energy (US)
OSTI Identifier:
836516
Report Number(s):
ANL-EBS-MD-000004, Rev. 01
DOC.20030626.0001, DC33936; TRN: US0500916
Resource Type:
Technical Report
Resource Relation:
Other Information: PBD: 24 Jun 2003
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; 12 MANAGEMENT OF RADIOACTIVE WASTES, AND NON-RADIOACTIVE WASTES FROM NUCLEAR FACILITIES; CONTAINERS; WASTE FORMS; CORROSION; DESIGN; OXIDATION; PERFORMANCE; PLATES; SHIELDS; TITANIUM; RADIOACTIVE WASTE DISPOSAL

Citation Formats

Hua, F, and Mon, K. General Corrosion and Localized Corrosion of the Drip Shield. United States: N. p., 2003. Web. doi:10.2172/836516.
Hua, F, & Mon, K. General Corrosion and Localized Corrosion of the Drip Shield. United States. https://doi.org/10.2172/836516
Hua, F, and Mon, K. 2003. "General Corrosion and Localized Corrosion of the Drip Shield". United States. https://doi.org/10.2172/836516. https://www.osti.gov/servlets/purl/836516.
@article{osti_836516,
title = {General Corrosion and Localized Corrosion of the Drip Shield},
author = {Hua, F and Mon, K},
abstractNote = {The recommended waste package (WP) design is described in BSC (2001a). The design includes a double-wall WP underneath a protective drip shield (DS) (BSC 2003a). The purpose of the process-level models developed in this report is to model dry oxidation (DOX), general corrosion (GC) and localized corrosion (LC) of the DS plate material, which is made of Ti Grade 7. The DS design also includes structural supports fabricated from Ti Grade 24. Degradation of Ti Grade 24 is not considered in this report. The DS provides protection for the waste package outer barrier (WPOB) both as a barrier to seepage water contact and a physical barrier to potential rockfall. This Model Report (MR) serves as a feed to the Integrated Waste Package Degradation Model (IWPD) analyses, and was developed in accordance with the Technical Work Plan (TWP) (BSC 2002a). The models contained in this report serve as a basis to determine whether or not the performance requirements for the DS can be met.},
doi = {10.2172/836516},
url = {https://www.osti.gov/biblio/836516}, journal = {},
number = ,
volume = ,
place = {United States},
year = {Tue Jun 24 00:00:00 EDT 2003},
month = {Tue Jun 24 00:00:00 EDT 2003}
}