Title: High thermal conductivity SiC/SiC composites for fusion applications -- 2

Technical Report ·
DOI:https://doi.org/10.2172/335385· OSTI ID:335385
; ;  [1];  [2]
  1. MER Corp., Tucson, AZ (United States)
  2. Pacific Northwest National Lab., Richland, WA (United States)

This report covers material presented at the IEA/Jupiter Joint International Workshop on SiC/SiC Composites for Fusion Structural Applications held in conjunction with ICFRM-8, Sendai, Japan, Oct. 23--24, 1997. An unirradiated SiC/SiC composite made with MER-developed CVR SiC fiber and a hybrid PIP/CVI SiC matrix exhibited room temperature transverse thermal conductivity of 45 W/mK. An unirradiated SiC/SiC composite made from C/C composite totally CVR-converted to a SiC/SiC composite exhibited transverse thermal conductivity values of 75 and 35 W/mK at 25 and 1000 C, respectively. Both types of SiC/SiC composites exhibited non-brittle failure in flexure testing.

Research Organization:
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Sponsoring Organization:
USDOE, Washington, DC (United States)
DOE Contract Number:
AC06-76RL01830
OSTI ID:
335385
Report Number(s):
DOE/ER-0313/23; ON: DE98004697; TRN: 99:005175
Resource Relation:
Other Information: PBD: Mar 1998; Related Information: Is Part Of Fusion materials semiannual progress report for the period ending December 31, 1997; Burn, G. [ed.] [comp.]; PB: 390 p.