Title: Single versus successive pop-in modes in nanoindentation tests of single crystals

From recent nanoindentation experiments, two types of pop-in modes have been identified: a single pop-in with a large displacement excursion, or a number of pop-ins with comparable and small displacement excursions. Theoretical analyses are developed here to study the roles played by indenter tip radius, pre-existing defect density, heterogeneous nucleation source type, and lattice resistance on the pop-in modes. The evolution of dislocation structures in earlier pop-ins provides input to modeling a stochastic, heterogeneous mechanism that may be responsible for the subsequent pop-ins. It is found that when the first pop-in occurs near theoretical shear stress, the pop-in mode is determined by the lattice resistance and tip radius. When the first pop-in occurs at low shear stress, whether the successive pop-in mode occurs depends on how the heterogeneous dislocation nucleation source density increases as compared to the increase of the total dislocation density. Lastly, the above transitions are found to correlate well with the ratio of indenter tip radius to the mean spacing of dislocation nucleation sources.
Authors:
 [1] ;  [2] ;  [2] ;  [3]
  1. Univ. of Tennessee, Knoxville, TN (United States). Dept. of Materials Science and Engineering
  2. Univ. of Tennessee, Knoxville, TN (United States). Dept. of Materials Science and Engineering; Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States). Materials Science & Technology Division
  3. Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States). Materials Science & Technology Division
Publication Date:
OSTI Identifier:
1324059
Grant/Contract Number:
AC05-00OR22725
Type:
Accepted Manuscript
Journal Name:
Journal of Materials Research
Additional Journal Information:
Journal Volume: 31; Journal Issue: 14; Journal ID: ISSN 0884-2914
Publisher:
Materials Research Society
Research Org:
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Sponsoring Org:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; nanoindentation; defects