Title: In situ nanoindentation study of plastic Co-deformation in Al-TiN nanocomposites

We performed in situ indentation in a transmission electron microscope on Al-TiN multilayers with individual layer thicknesses of 50 nm, 5 nm and 2.7 nm to explore the effect of length scales on the plastic co-deformability of a metal and a ceramic. At 50 nm, plasticity was confined to the Al layers with easy initiation of cracks in the TiN layers. At 5 nm and below, cracking in TiN was suppressed and post mortem measurements indicated a reduction in layer thickness in both layers. Our results demonstrate the profound size effect in enhancing plastic co-deformability in nanoscale metal-ceramic multilayers.
Authors:
 [1] ;  [2] ;  [3] ;  [2]
  1. Los Alamos National Lab. (LANL), Los Alamos, NM (United States). Materials Physics and Applications Division
  2. Los Alamos National Lab. (LANL), Los Alamos, NM (United States). Materials Science and Technology Division
  3. Los Alamos National Lab. (LANL), Los Alamos, NM (United States). Materials Physics and Applications Division; Univ. of Michigan, Ann Arbor, MI (United States). Dept. of Materials Science and Engineering
Publication Date:
OSTI Identifier:
1259289
Grant/Contract Number:
AC52-06NA25396
Type:
Accepted Manuscript
Journal Name:
Scientific Reports
Additional Journal Information:
Journal Volume: 4; Journal ID: ISSN 2045-2322
Publisher:
Nature Publishing Group
Research Org:
Los Alamos National Laboratory (LANL), Los Alamos, NM (United States)
Sponsoring Org:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22); USDOE National Nuclear Security Administration (NNSA)
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE materials science; structural properties