Title: Yield strength of Ni–Al–Cr superalloy under pressure

Authors:
; ; ; ;  [1]
  1. LBNL
Publication Date:
OSTI Identifier:
1229893
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Alloys and Compounds; Journal Volume: 657
Publisher:
Elsevier
Research Org:
Advanced Photon Source (APS), Argonne National Laboratory (ANL), Argonne, IL (US)
Sponsoring Org:
U.S. AIR FORCE- OFFICE OF SCIENTIFIC RESEARCH
Country of Publication:
United States
Language:
ENGLISH