Title: Analytic expressions for atomic layer deposition: Coverage, throughput, and materials utilization in cross-flow, particle coating, and spatial atomic layer deposition

Authors:
;
Publication Date:
OSTI Identifier:
1210314
DOE Contract Number:
SC0001059
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Vacuum Science & Technology A; Journal Volume: 32; Related Information: ANSER partners with Northwestern University (lead); Argonne National Laboratory; University of Chicago; University of Illinois, Urbana-Champaign; Yale University
Research Org:
Energy Frontier Research Centers (EFRC); Argonne-Northwestern Solar Energy Research Center (ANSER)
Sponsoring Org:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
Country of Publication:
United States
Language:
English
Subject:
catalysis (homogeneous), catalysis (heterogeneous), solar (photovoltaic), solar (fuels), photosynthesis (natural and artificial), bio-inspired, hydrogen and fuel cells, electrodes - solar, defects, charge transport, spin dynamics, membrane, materials and chemistry by design, optics, synthesis (novel materials), synthesis (self-assembly)