Title: Plasmonic Three-Dimensional Transparent Conductor Based on Al-Doped Zinc Oxide-Coated Nanostructured Glass Using Atomic Layer Deposition

Transparent nanostructured glass coatings, fabricated on glass substrates, with a unique three-dimensional (3D) architecture were utilized as the foundation for the design of plasmonic 3D transparent conductors. Transformation of the non-conducting 3D structure to a conducting 3D network was accomplished through atomic layer deposition of aluminum-doped zinc oxide (AZO). After AZO growth, gold nanoparticles (AuNPs) were deposited by electronbeam evaporation to enhance light trapping and decrease the overall sheet resistance. Field emission scanning electron microscopy and atomic force microcopy images revealed the highly porous, nanostructured morphology of the AZO coated glass surface along with the in-plane dimensions of the deposited AuNPs. Sheet resistance measurements conducted on the coated samples verified that the electrical properties of the 3D network are comparable to that of the untextured two-dimensional AZO coated glass substrates. In addition, transmittance measurements of the glass samples coated with various AZO thicknesses showed preservation of the highly transparent nature of each sample, while the AuNPs demonstrated enhanced light scattering as well as light-trapping capability.
Authors:
 [1] ;  [2] ;  [1] ;  [1]
  1. Univ. of Kansas, Lawrence, KS (United States). Dept. of Physics and Astronomy
  2. Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Publication Date:
OSTI Identifier:
1185885
Grant/Contract Number:
AC05-00OR22725; NNX13AD42A; W911NF-12-1-0412; NSF-DMR-1105986; NSF-EPSCoR- 0903806
Type:
Accepted Manuscript
Journal Name:
ACS Applied Materials and Interfaces
Additional Journal Information:
Journal Volume: 7; Journal Issue: 16; Journal ID: ISSN 1944-8244
Publisher:
American Chemical Society (ACS)
Research Org:
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Sponsoring Org:
Work for Others (WFO)
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; transparent conductor; atomic layer deposition; nanostructured glass; plasmonic effect; three-dimensional electrode; aluminum-doped zinc oxide