Title: High Pressure Steam Oxidation of Ni-base Superalloys in Advanced Ultra-Supercritical Steam Boilers and Turbines

Authors:
Publication Date:
OSTI Identifier:
1178108
Report Number(s):
NETL-PUB-830
Resource Type:
Conference
Resource Relation:
Conference: “High Pressure Steam Oxidation of Ni-base Superalloys in Advanced Ultra-Supercritical Steam Boilers and Turbines,” invited presentation at the 8th International Symposium on Superalloy 718 and Derivatives, September 28-October 1, 2014, Pittsburgh, PA.
Research Org:
National Energy Technology Lab. (NETL), Pittsburgh, PA, and Morgantown, WV (United States). In-house Research
Sponsoring Org:
USDOE Office of Fossil Energy (FE)
Country of Publication:
United States
Language:
English
Subject:
Steam, Oxidation, Superalloy, Pressure, Advanced Ultra-supercritical