Title: Nanoscale Investigation of Solid Electrolyte Interphase Inhibition on Li-ion Battery MnO Electrodes via Atomic Layer Deposition of Al2O3

Authors:
; ; ; ; ; ;
Publication Date:
OSTI Identifier:
1161042
DOE Contract Number:
AC02-06CH11357
Resource Type:
Journal Article
Resource Relation:
Journal Name: Chem. Mater.; Related Information: CEES partners with Argonne National Laboratory (lead); University of Illinois, Urbana-Champaign; Northwest University
Research Org:
Energy Frontier Research Centers (EFRC); Center for Electrical Energy Storage (CEES)
Sponsoring Org:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
Country of Publication:
United States
Language:
English
Subject:
energy storage (including batteries and capacitors), charge transport, materials and chemistry by design, synthesis (novel materials)