Title: Self-Assembly Based Plasmonic Arrays Tuned by Atomic Layer Deposition for Extreme Visible Light Absorption

Authors:
; ; ; ; ; ;
Publication Date:
OSTI Identifier:
1136670
Report Number(s):
SLAC-REPRINT-2014-219
Journal ID: ISSN 1530-6984
DOE Contract Number:
AC02-76SF00515
Resource Type:
Journal Article
Resource Relation:
Journal Name: Nano Letters; Journal Volume: 13; Journal Issue: 7
Publisher:
American Chemical Society
Research Org:
SLAC National Accelerator Lab., Menlo Park, CA (United States)
Sponsoring Org:
USDOE Office of Science (SC)
Country of Publication:
United States
Language:
English
Subject:
CHEM