Title: Electromechanical Tuning of Nanoscale MIM Diodes by Nanoindentation

Authors:
; ; ; ; ; ;
Publication Date:
OSTI Identifier:
1097900
DOE Contract Number:
AC36-08GO28308
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Materials Research; Journal Volume: 28; Journal Issue: 14, 28 July 2013
Research Org:
National Renewable Energy Laboratory (NREL), Golden, CO.
Sponsoring Org:
USDOE Office of Energy Efficiency and Renewable Energy; USDOE Office of Science, Center for Revolutionary Solar Photoconversion; National Science Foundation; National Renewable Energy Laboratory LDRD Program
Country of Publication:
United States
Language:
English
Subject:
14 SOLAR ENERGY; 77 NANOSCIENCE AND NANOTECHNOLOGY Chemical and Material Sciences