Title: Direct characterization of interface sites in Au/TiO2 catalysts prepared using atomic layer deposition

Journal Article · · Chem Catalysis

Not Available

Sponsoring Organization:
USDOE
OSTI ID:
2566602
Journal Information:
Chem Catalysis, Journal Name: Chem Catalysis Journal Issue: 5 Vol. 4; ISSN 2667-1093
Publisher:
ElsevierCopyright Statement
Country of Publication:
United States
Language:
English

References (77)

A Yolk@Shell Nanoarchitecture for Au/TiO2 Catalysts journal April 2011
On the Simple Complexity of Carbon Monoxide on Oxide Surfaces: Facet-Specific Donation and Backdonation Effects Revealed on TiO 2 Anatase Nanoparticles journal April 2016
CO Oxidation over Supported Gold Catalysts—“Inert” and “Active” Support Materials and Their Role for the Oxygen Supply during Reaction journal January 2001
Investigation of the active site and the mode of Au/TiO2 catalyst deactivation using Diffuse Reflectance Infrared Fourier Transform Spectroscopy (DRIFTS) journal March 2010
Nickel Supported on Mesoporous Zirconium Oxide by Atomic Layer Deposition: Initial Fixed-Bed Reactor Study journal January 2019
Atomic Layer Deposition (ALD) as a Way to Prepare New Mixed-Oxide Catalyst Supports: The Case of Alumina Addition to Silica-Supported Platinum for the Selective Hydrogenation of Cinnamaldehyde journal March 2019
Chemisorption of CO on the Pt(111) surface journal May 1977
Au/TiO2 nanostructured catalyst: pressure and temperature effects on the FTIR spectra of CO adsorbed at 90 K journal April 2002
CO chemisorption on Au(110) investigated under elevated pressures by polarized reflection absorption infrared spectroscopy and scanning tunneling microscopy journal December 2002
FT-IR characterization of the surface acidity of different titanium dioxide anatase preparations journal January 1985
Infrared study of Ti-containing zeolites using CO as a probe molecule book January 1995
Lewis acid and base sites at the surface of microcrystalline TiO2 anatase: relationships between surface morphology and chemical behaviour journal August 2000
FTIR study of low-temperature adsorption and co-adsorption of 12CO and 13CO on a TiO2–SiO2 mixed oxide journal November 1999
Catalytic activity of Au nanoparticles journal August 2007
Infrared study on room-temperature atomic layer deposition of TiO2 using tetrakis(dimethylamino)titanium and remote-plasma-excited water vapor journal July 2014
Aerobic oxidative esterification of primary alcohols over Pd-Au bimetallic catalysts supported on mesoporous silica nanoparticles journal May 2018
Spectroscopic features and reactivity of CO adsorbed on different Au/CeO2 catalysts journal January 2007
Study of the surface acidity of TiO2/SiO2 catalysts by means of FTIR measurements of CO and NH3 adsorption journal March 2007
Activity, stability, and deactivation behavior of supported Au/TiO2 catalysts in the CO oxidation and preferential CO oxidation reaction at elevated temperatures journal October 2009
Support effects in the Au-catalyzed CO oxidation – Correlation between activity, oxygen storage capacity, and support reducibility journal December 2010
Catalytic oxidation of carbon monoxide at cryogenic temperatures journal November 2014
Effect of titania surface modification of mesoporous silica SBA-15 supported Au catalysts: Activity and stability in the CO oxidation reaction journal December 2017
Chemisorption of ALD precursors in and on porous low-k films journal June 2013
Synthesis of high-surface area tungstated zirconia by atomic layer deposition on mesoporous silica journal April 2022
Catalysis by gold: New insights into the support effect journal August 2013
Surface chemistry of Au/TiO2: Thermally and photolytically activated reactions journal March 2016
The adsorption of CO on Au(111) at elevated pressures studied by STM, RAIRS and DFT calculations journal September 2004
Au@Void@TiO2 yolk–shell nanostructures as catalysts for the promotion of oxidation reactions at cryogenic temperatures journal June 2016
On the initial growth of atomic layer deposited TiO2 films on silicon and copper surfaces journal September 2012
Atomic layer deposition of TiO 2 from tetrakis(dimethylamino)titanium and H 2 O journal October 2013
Growth of ZrO2 films on mesoporous silica sieve via atomic layer deposition journal March 2023
Importance of Size and Contact Structure of Gold Nanoparticles for the Genesis of Unique Catalytic Processes journal December 2019
Probing Surface Structures of CeO 2 , TiO 2 , and Cu 2 O Nanocrystals with CO and CO 2 Chemisorption journal September 2016
Redox Properties of TiO2 Thin Films Grown on Mesoporous Silica by Atomic Layer Deposition journal May 2023
Nucleation and Initial Stages of Growth during the Atomic Layer Deposition of Titanium Oxide on Mesoporous Silica journal August 2020
Metal–Support Interactions in Metal/Oxide Catalysts and Oxide–Metal Interactions in Oxide/Metal Inverse Catalysts journal January 2022
Sub-Monolayer Control of Mixed-Oxide Support Composition in Catalysts via Atomic Layer Deposition: Selective Hydrogenation of Cinnamaldehyde Promoted by (SiO 2 -ALD)-Pt/Al 2 O 3 journal August 2018
Controlling Selectivity in Unsaturated Aldehyde Hydrogenation Using Single-Site Alloy Catalysts journal September 2019
Structure and Chemical Properties of Oxide Nanoparticles Determined by Surface-Ligand IR Spectroscopy journal November 2019
Gold Atoms Stabilized on Various Supports Catalyze the Water–Gas Shift Reaction journal November 2013
Heterogeneous Gold-Based Catalysis for Green Chemistry:  Low-Temperature CO Oxidation and Propene Oxidation journal June 2007
Atomic Layer Deposition: An Overview journal January 2010
Catalyst Design with Atomic Layer Deposition journal February 2015
The Determination of Pore Volume and Area Distributions in Porous Substances. I. Computations from Nitrogen Isotherms journal January 1951
Adsorption of Gases in Multimolecular Layers journal February 1938
FTIR Study of CO Oxidation on Au/TiO 2 at 90 K and Room Temperature. An Insight into the Nature of the Reaction Centers journal June 2000
Effect of Supporting Surface Layers on Catalytic Activities of Gold Nanoparticles in CO Oxidation journal July 2005
Preparation of Highly Active Silica-Supported Au Catalysts for CO Oxidation by a Solution-Based Technique journal June 2006
Well-Defined Negatively Charged Gold Carbonyls on Au/SiO 2 journal October 2011
Surface Modification of Au/TiO 2 Catalysts by SiO 2 via Atomic Layer Deposition journal May 2008
Interaction of Gold with Cerium Oxide Supports: CeO 2 (111) Thin Films vs CeO x Nanoparticles journal March 2009
The Surface Chemistry of Atomic Layer Depositions of Solid Thin Films journal May 2012
Thermodynamic and spectroscopic characterization of heterogeneity among adsorption sites: carbon monoxide on anatase at ambient temperature journal July 1989
FTIR Spectroscopic Study of Titanium-Containing Mesoporous Silicate Materials journal November 2005
Catalysis of Gold Nanoparticles Deposited on Metal Oxides journal January 2002
Tunable gold catalysts for selective hydrocarbon oxidation under mild conditions journal October 2005
Gold catalysts for pure hydrogen production in the water–gas shift reaction: activity, structure and reaction mechanism journal January 2006
Characterisation of gold catalysts journal January 2016
Atomic layer deposition for nanomaterial synthesis and functionalization in energy technology journal January 2017
Sub-monolayer control of the growth of oxide films on mesoporous materials journal January 2018
Enhancing the activity of gold supported catalysts by oxide coating: towards efficient oxidations journal January 2021
Genesis of a highly active cerium oxide-supported gold catalyst for CO oxidation journal January 2007
Supported gold nanoparticles as catalysts for organic reactions journal January 2008
Catalytically active gold on ordered titania supports journal January 2008
Thermodynamic and vibrational characterization of CO adsorption on variously pretreated anatase
  • Bolis, Vera; Fubini, Bice; Garrone, Edoardo
  • Journal of the Chemical Society, Faraday Transactions 1: Physical Chemistry in Condensed Phases, Vol. 85, Issue 6 https://doi.org/10.1039/f19898501383
journal January 1989
Adsorption of carbon monoxide on the gold(332) surface journal January 1996
Catalysis by Gold journal January 1999
Molecular interactions on surfaces
  • Wei, D. H.; Skelton, D. C.; Kevan, S. D.
  • Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Vol. 12, Issue 4 https://doi.org/10.1116/1.579132
journal July 1994
The Structure of Catalytically Active Gold on Titania journal October 2004
Spectroscopic Observation of Dual Catalytic Sites During Oxidation of CO on a Au/TiO2 Catalyst journal August 2011
Triblock Copolymer Syntheses of Mesoporous Silica with Periodic 50 to 300 Angstrom Pores journal January 1998
Restructuring of titanium oxide overlayers over nickel nanoparticles during catalysis journal May 2023
Effect of the titanium oxide stoichiometry on the efficiency of CO oxidation on the Au/TiOx system surface journal October 2000
Novel Gold Catalysts for the Oxidation of Carbon Monoxide at a Temperature far Below 0 °C journal February 1987
Reporting physisorption data for gas/solid systems with special reference to the determination of surface area and porosity (Recommendations 1984) journal January 1985
CO Oxidation Catalyzed by Au Dispersed on SBA-15 Modified with TiO2 Films Grown via Atomic Layer Deposition (ALD) journal July 2023
A Review: Mesoporous Santa Barbara Amorphous-15, Types, Synthesis and Its Applications towards Biorefinery Production journal December 2010

Similar Records

Related Subjects