Title: Direct modification of pelletized 13X zeolite by atomic layer deposition toward effective CO2 capture from flue gas

Journal Article · · Chemical Engineering Journal

Not Available

Sponsoring Organization:
USDOE
Grant/Contract Number:
FE0031730
OSTI ID:
2434331
Journal Information:
Chemical Engineering Journal, Journal Name: Chemical Engineering Journal Journal Issue: C Vol. 497; ISSN 1385-8947
Publisher:
ElsevierCopyright Statement
Country of Publication:
Switzerland
Language:
English

References (52)

CO 2 capture from dry flue gas by vacuum swing adsorption: A pilot plant study journal March 2014
ChemInform Abstract: CONCENTRATION AND LOCATION OF HYDROXY GROUPS IN HYDRATED ZEOLITE LINDE 13X, HYDROLYSIS BY WASHING AS DETERMINED BY PROTON MAGNETIC RESONANCE AT 90 K journal April 1981
A Method for Screening the Potential of MOFs as CO2 Adsorbents in Pressure Swing Adsorption Processes journal March 2012
CO2 capture by amine-functionalized nanoporous materials: A review journal October 2014
Non-isobaric adsorption analysis of SO2 on molecular sieve 13X and activated carbon by dynamic technique journal January 1999
Advances in CO2 capture technology—The U.S. Department of Energy's Carbon Sequestration Program journal January 2008
Energy minimization of MEA-based CO2 capture process journal May 2016
How much can novel solid sorbents reduce the cost of post-combustion CO2 capture? A techno-economic investigation on the cost limits of pressure–vacuum swing adsorption journal January 2022
Titanium tetrachloride as novel working fluid for high temperature Rankine Cycles: Thermodynamic analysis and experimental assessment of the thermal stability journal August 2016
A model-based approach for the evaluation of new zeolite 13X-based adsorbents for the efficient post-combustion CO2 capture using P/VSA processes journal March 2018
CO2 capture via adsorption in amine-functionalized sorbents journal May 2016
CO2 capture by adsorption with nitrogen enriched carbons journal September 2007
Do adsorbent screening metrics predict process performance? A process optimisation based study for post-combustion capture of CO2 journal March 2016
Review of Polybed pressure swing adsorption for hydrogen purification journal March 2022
From laboratory to industrial scale: a scale-up framework for chemical processes in life cycle assessment studies journal November 2016
Novel nitrogen enriched porous carbon adsorbents for CO 2 capture: Breakthrough adsorption study journal March 2016
Ultrathin, fine-tuned microporous coating modified 5A zeolite for propane/propylene adsorptive separation journal June 2019
Cryogenic-based CO2 capture technologies: State-of-the-art developments and current challenges journal March 2019
A review on production of metal organic frameworks (MOF) for CO2 adsorption journal March 2020
Techno-economic assessment of optimised vacuum swing adsorption for post-combustion CO2 capture from steam-methane reformer flue gas journal February 2021
Adsorption of Carbon Dioxide, Water Vapor, Nitrogen, and Sulfur Dioxide on Activated Carbon for Capture from Flue Gases: Competitive Adsorption and Selectivity Aspects journal March 2021
Prediction of MOF Performance in Vacuum Swing Adsorption Systems for Postcombustion CO 2 Capture Based on Integrated Molecular Simulations, Process Optimizations, and Machine Learning Models journal February 2020
MIL-101(Cr) Polymeric Fiber Adsorbents for Sub-Ambient Post-Combustion CO2 Capture journal September 2022
Adsorbent Screening for Postcombustion CO 2 Capture: A Method Relating Equilibrium Isotherm Characteristics to an Optimum Vacuum Swing Adsorption Process Performance journal February 2016
Measurement and Prediction of the Heat of Adsorption and Equilibrium Concentration of CO 2 on Zeolite 13X journal April 2018
Equilibrium Adsorption Study of CO2 and N2 on Synthesized Zeolites 13X, 4A, 5A, and Beta journal December 2019
CO2 Adsorption/Desorption in FAU Zeolite Nanocrystals: In Situ Synchrotron X-ray Powder Diffraction and in Situ Fourier Transform Infrared Spectroscopic Study journal January 2019
Do New MOFs Perform Better for CO2 Capture and H2 Purification? Computational Screening of the Updated MOF Database journal August 2020
Molecular Layer Deposition-Modified 5A Zeolite for Highly Efficient CO 2 Capture journal December 2017
Open and Hierarchical Carbon Framework with Ultralarge Pore Volume for Efficient Capture of Carbon Dioxide journal September 2018
Review on CO2 Capture Using Amine-Functionalized Materials journal October 2022
Toward Sustainable Metal–Organic Frameworks for Post-Combustion Carbon Capture by Life Cycle Assessment and Molecular Simulation journal September 2021
Development of a General Evaluation Metric for Rapid Screening of Adsorbent Materials for Postcombustion CO 2 Capture journal May 2019
Process Optimization-Based Screening of Zeolites for Post-Combustion CO 2 Capture by Vacuum Swing Adsorption journal October 2019
Adsorption of CO 2 on Molecular Sieves and Activated Carbon journal March 2001
In Situ Fourier Transform Infrared (FTIR) Investigation of CO 2 Adsorption onto Zeolite Materials journal September 2008
A Technical, Economic, and Environmental Assessment of Amine-Based CO 2 Capture Technology for Power Plant Greenhouse Gas Control journal October 2002
Comparison of Activated Carbon and Zeolite 13X for CO2 Recovery from Flue Gas by Pressure Swing Adsorption journal February 1995
The Effect of Water on the Adsorption of CO 2 and C 3 H 8 on Type X Zeolites journal December 2004
Post-Combustion CO2 Capture Using Solid Sorbents: A Review journal September 2011
Isosteric Heats of Adsorption on Carbon Predicted by Density Functional Theory journal February 1998
Adsorption Equilibrium of Binary Mixtures of Carbon Dioxide and Water Vapor on Zeolites 5A and 13X journal September 2010
Revealing the Structure–Property Relationships of Metal–Organic Frameworks for CO 2 Capture from Flue Gas journal August 2012
Continuously Adjustable, Molecular-Sieving “Gate” on 5A Zeolite for Distinguishing Small Organic Molecules by Size journal September 2015
Composite 5A zeolite with ultrathin porous TiO 2 coating for selective gas adsorption journal January 2015
Solvothermal synthesis of hierarchically nanoporous organic polymers with tunable nitrogen functionality for highly selective capture of CO 2 journal January 2016
An overview of molecular layer deposition for organic and organic–inorganic hybrid materials: mechanisms, growth characteristics, and promising applications journal January 2017
Process-level modelling and optimization to evaluate metal–organic frameworks for post-combustion capture of CO2 journal January 2020
Latest trends in the large-scale production of MOFs in accordance with the principles of green chemistry journal January 2022
Desorption characteristics and kinetic parameters determination of molecular sieve by thermogravimetric analysis/differential thermogravimetric analysis technique journal May 2018
Temperature Dependence of the Isosteric Heat of Adsorption journal December 2001
Study of the Temperature-Programmed Desorption of Carbon Dioxide (CO2) on Zeolites X Modified with Bivalent Cations journal January 2023

Similar Records

Related Subjects