DOE PAGES title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Rapid subsurface analysis of frequency-domain thermoreflectance images with K-means clustering

Journal Article · · Journal of Applied Physics
DOI: https://doi.org/10.1063/5.0201473 · OSTI ID:2341386

K-means clustering analysis is applied to frequency-domain thermoreflectance (FDTR) hyperspectral image data to rapidly screen the spatial distribution of thermophysical properties at material interfaces. Performing FDTR while raster scanning a sample consisting of 8.6 μm of doped-silicon (Si) bonded to a doped-Si substrate identifies spatial variation in the subsurface bond quality. Routine thermal analysis at select pixels quantifies this variation in bond quality and allows assignment of bonded, partially bonded, and unbonded regions. Performing this same routine thermal analysis across the entire map, however, becomes too computationally demanding for rapid screening of bond quality. To address this, K-means clustering was used to reduce the dimensionality of the dataset from more than 20 000 pixel spectra to just K = 3 component spectra. The three component spectra were then used to express every pixel in the image through a least-squares minimized linear combination providing continuous interpolation between the components across spatially varying features, e.g., bonded to unbonded transition regions. Fitting the component spectra to the thermal model, thermal properties for each K cluster are extracted and then distributed according to the weighting established by the regressed linear combination. Thermophysical property maps are then constructed and capture significant variation in bond quality over 25 μm length scales. The use of K-means clustering to achieve these thermal property maps results in a 74-fold speed improvement over explicit fitting of every pixel.

Research Organization:
Sandia National Laboratories (SNL-NM), Albuquerque, NM (United States)
Sponsoring Organization:
USDOE National Nuclear Security Administration (NNSA); USDOE Laboratory Directed Research and Development (LDRD) Program
Grant/Contract Number:
NA0003525
OSTI ID:
2341386
Report Number(s):
SAND--2024-05105J
Journal Information:
Journal of Applied Physics, Journal Name: Journal of Applied Physics Journal Issue: 16 Vol. 135; ISSN 0021-8979
Publisher:
American Institute of Physics (AIP)Copyright Statement
Country of Publication:
United States
Language:
English

References (45)

A Review of Experimental and Computational Advances in Thermal Boundary Conductance and Nanoscale Thermal Transport across Solid Interfaces journal August 2019
Microscale Imaging of Thermal Conductivity Suppression at Grain Boundaries journal July 2023
Energy dissipation and transport in nanoscale devices journal March 2010
Anisotropic thermal and electrical conductivities of individual polyacrylonitrile-based carbon fibers journal September 2022
Thermal conductivity mapping of pyrolytic carbon and silicon carbide coatings on simulated fuel particles by time-domain thermoreflectance journal August 2008
High spatial resolution thermal conductivity mapping of SiC/SiC composites journal December 2020
Thermal conductivity mapping of the Ni–Al system and the beta-NiAl phase in the Ni–Al–Cr system journal June 2012
Direct Visualization of Thermal Conductivity Suppression Due to Enhanced Phonon Scattering Near Individual Grain Boundaries journal April 2018
Thermal Visualization of Buried Interfaces Enabled by Ratio Signal and Steady-State Heating of Time-Domain Thermoreflectance journal June 2021
A Critical Review of Thermal Boundary Conductance across Wide and Ultrawide Bandgap Semiconductor Interfaces journal June 2023
Inversion for Thermal Properties with Frequency Domain Thermoreflectance journal January 2024
Thermal Transport and Mechanical Stress Mapping of a Compression Bonded GaN/Diamond Interface for Vertical Power Devices journal February 2024
Interfacial Thermal Conductance across Room-Temperature-Bonded GaN/Diamond Interfaces for GaN-on-Diamond Devices journal January 2020
Thermal conductance of metal–diamond interfaces at high pressure journal March 2015
Thermal conductivity measurement from 30 to 750 K: the 3ω method journal February 1990
Analysis of heat flow in layered structures for time-domain thermoreflectance journal December 2004
Pulse accumulation, radial heat conduction, and anisotropic thermal conductivity in pump-probe transient thermoreflectance journal November 2008
A frequency-domain thermoreflectance method for the characterization of thermal properties journal September 2009
Thermal conductance and phonon transmissivity of metal–graphite interfaces journal May 2010
Instrumentation of broadband frequency domain thermoreflectance for measuring thermal conductivity accumulation functions journal June 2013
Thermal property microscopy with frequency domain thermoreflectance journal October 2013
Nanoscale thermal transport. II. 2003–2012 journal March 2014
Thermal conductance imaging of graphene contacts journal July 2014
Uncertainty analysis of thermoreflectance measurements journal January 2016
Tutorial: Time-domain thermoreflectance (TDTR) for thermal property characterization of bulk and thin film materials journal October 2018
A steady-state thermoreflectance method to measure thermal conductivity journal February 2019
Wide bandwidth frequency-domain thermoreflectance: Volumetric heat capacity, anisotropic thermal conductivity, and thickness measurements journal December 2020
Simultaneous thickness and thermal conductivity measurements of thinned silicon from 100 nm to 17 μm journal May 2021
Machine learning-based data processing technique for time-domain thermoreflectance (TDTR) measurements journal August 2021
Perspective on thermal conductance across heterogeneously integrated interfaces for wide and ultrawide bandgap electronics journal January 2022
Sensing depths in frequency domain thermoreflectance journal June 2022
Machine learning reconstruction of depth-dependent thermal conductivity profile from pump–probe thermoreflectance signals journal April 2023
Kapitza conductance and heat flow between solids at temperatures from 50 to 300 K journal December 1993
Thermal conductance of epitaxial interfaces journal February 2003
Thermal conductance of metal-metal interfaces journal December 2005
Thermal conductance of interfaces between highly dissimilar materials journal April 2006
Thermal conductance of strongly bonded metal-oxide interfaces journal March 2015
Heat Generation and Transport in Nanometer-Scale Transistors journal August 2006
Recent Advances and Trends in Advanced Packaging journal February 2022
Least squares quantization in PCM journal March 1982
On the Determination of Thermal Conductivity From Frequency Domain Thermoreflectance Experiments journal November 2021
Thermal Boundary Conductance: A Materials Science Perspective journal July 2016
Heterogeneous Integration of Compound Semiconductors journal June 2010
Measurement of the μm sized radius of Gaussian laser beam using the scanning knife-edge journal January 1975
Thermal-conductivity measurement by time-domain thermoreflectance journal October 2018