Title: Towards understanding stress corrosion cracking of austenitic stainless steels exposed to realistic sea salt brines

Journal Article · · Corrosion Science

Not Available

Sponsoring Organization:
USDOE National Nuclear Security Administration (NNSA)
Grant/Contract Number:
NA0003525
OSTI ID:
2331333
Journal Information:
Corrosion Science, Journal Name: Corrosion Science Journal Issue: C Vol. 232; ISSN 0010-938X
Publisher:
ElsevierCopyright Statement
Country of Publication:
United Kingdom
Language:
English

References (78)

SCC Testing and Data Quality Considerations other August 1999
On the calibration of the electrical potential technique for monitoring crack growth using finite element methods journal February 1979
The threshold stress intensity for hydrogen-induced crack growth journal June 1981
Stress corrosion cracking of stainless steels in NaCl solutions journal May 1981
A mechanistic study of transgranular stress corrosion cracking of type 304 stainless steel journal June 1991
Measurement and Modeling of Hydrogen Environment-Assisted Cracking in Monel K-500 journal May 2014
The Effect of Microstructural Variation on the Hydrogen Environment-Assisted Cracking of Monel K-500 journal April 2016
Effect of Strain Rate on Stress Corrosion Cracking of 316L Austenitic Stainless Steel in Boiling MgCl2 Environment journal December 2012
Stress corrosion cracking of cold-worked austenitic stainless steels journal January 1982
A coupled environment model for stress corrosion cracking in sensitized type 304 stainless steel in LWR environments journal January 1991
Discussion on “Determination of the fate of the current in the SCC of sensitized type 304 SS in high temperature aqueous systems” journal December 1995
Response to “ On the modeling of stress corrosion cracking of iron and nickel base alloys in high temperature aqueous environments” journal June 1996
On the relationship between critical tensile stress and fracture toughness in mild steel journal November 1973
Life prediction by mechanistic modeling and system monitoring of environmental cracking of iron and nickel alloys in aqueous systems journal August 1988
Clarification of issues raised by P.L. Andresen and F.P. Ford in their response to “On the modeling of stress corrosion cracking of iron and nickel base alloys in high temperature aqueous environments” journal August 1997
Modelling of crack chemistry in sensitized stainless steel in boiling water reactor environments journal April 1997
Using capillary electrophoresis to study the chemical conditions within cracks in aluminum alloys journal July 1999
Theoretical and experimental study on the temperature distribution of H-shaped steel members under solar radiation journal May 2012
Experimental and numerical investigation of temperature effects on steel members due to solar radiation journal December 2017
The effect of test temperature on SCC behavior of austenitic stainless steels in boiling saturated magnesium chloride solution journal December 2006
Crack tip chemistry and electrochemistry of environmental cracks in AA 7050 journal June 2007
The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solutions journal July 2007
Film rupture model for aqueous stress corrosion cracking under constant and variable stress intensity factor journal February 2009
Critique of the Ford–Andresen film rupture model for aqueous stress corrosion cracking journal May 2009
Experimental and numerical investigation of stress corrosion cracking of sensitized type 304 stainless steel under high-temperature and high-purity water journal August 2015
Effect of machining-induced surface residual stress on initiation of stress corrosion cracking in 316 austenitic stainless steel journal July 2016
On the stress corrosion crack growth behaviour in high temperature water of 316L stainless steel made by laser powder bed fusion additive manufacturing journal November 2017
Importance of the hydrogen evolution reaction in magnesium chloride solutions on stainless steel journal December 2020
Atmospheric stress corrosion crack growth rates of 316 L stainless steel for nuclear waste containment journal December 2020
On the loading rate dependence of environment-assisted cracking in sensitized AA5456-H116 exposed to marine environments journal June 2022
Insights from electrochemical crack tip modeling of atmospheric stress corrosion cracking journal December 2022
Spatial determination of diffusible hydrogen concentrations proximate to pits in a Fe–Cr–Ni–Mo steel using the Scanning Kelvin Probe journal February 2016
Pitting and stress corrosion cracking behavior in welded austenitic stainless steel journal January 2005
Nitrate on localized corrosion of carbon steel and stainless steel in aqueous solutions journal February 2021
Predicting the influence of strain on crack length measurements performed using the potential drop method journal September 2017
Effect of microstructural and environmental variables on ductility of austenitic stainless steels journal March 2021
Development of a fundamental crack tip strain rate equation and its application to quantitative prediction of stress corrosion cracking of stainless steels in high temperature oxygenated water journal January 2004
Corrosion and stress corrosion cracking in supercritical water journal September 2007
Microstructural changes in AISI 304L stainless steel due to surface machining: Effect on its susceptibility to chloride stress corrosion cracking journal August 2010
dK/da effects on the SCC growth rates of nickel base alloys in high-temperature water journal May 2018
Role of residual stresses induced by industrial fabrication on stress corrosion cracking susceptibility of austenitic stainless steel journal August 2011
Physical and chemical properties of sea salt deliquescent brines as a function of temperature and relative humidity journal June 2022
Chemical and electrochemical conditions within stress corrosion and corrosion fatigue cracks journal October 2017
Crystallographic effects on transgranular chloride-induced stress corrosion crack propagation of arc welded austenitic stainless steel journal May 2022
Application of Fracture Mechanics Techniques to the Environmentally Assisted Cracking of Aluminium 2024 journal November 1989
Effect of Rising and Falling K Profiles on SCC Growth Rates in High-Temperature Water journal November 2006
Pitting Corrosion of Metals journal January 1998
Long-Term Effects of Humidity on Stainless Steel Pitting in Sea Salt Exposures journal February 2021
Influence of Realistic, Cyclic Atmospheric Cycles on the Pitting Corrosion of Austenitic Stainless Steels journal April 2023
Oxygen Reduction on Stainless Steel in Concentrated Chloride Media journal January 2018
Humidity Effects on Pitting of Ground Stainless Steel Exposed to Sea Salt Particles journal January 2019
Effect of Nitrate and Sulfate on Atmospheric Corrosion of 304L and 316L Stainless Steels journal January 2017
Evaluating Localized Corrosion Susceptibility of Austenitic Stainless Steels Exposed to Varying Nitrate to Chloride Ratio Droplets journal October 2022
Effect of Atmospheric Conditions on Galvanic Corrosion and Environmental Cracking of an Aerospace Aluminum Alloy book May 2023
Gap Analysis to Guide DOE R&D in Supporting Extended Storage and Transportation of Spent Nuclear Fuel: An FY2019 Assessment (Final Report) report December 2019
FY21 Status Report: Probabilistic SCC Model for SNF Dry Storage Canisters report July 2021
SNF Interim Storage Canister Corrosion and Surface Environment Investigations (FY21 Status Report) report September 2021
Stress Corrosion Cracking of Austenitic Stainless Steels: Correlating in-situ crack tip chemistry and crack growth rate measurements. conference October 2022
Engineering approach for elastic-plastic fracture analysis report July 1981
Stress Corrosion Cracking Growth Rates of Candidate Canister Materials for Spent Nuclear Fuel Storage in Chloride-Containing Atmosphere journal January 2007
The Effect of Loading Rate on the Environment-Assisted Cracking Behavior of AA7075-T651 in Aqueous NaCl Solution journal July 2021
The Effect of Cold Work on the Stress-Corrosion Cracking of Type 302 Austenitic Stainless Steel journal October 1965
Mechanism of Chloride Stress Corrosion Cracking of Austenitic Stainless Steels journal November 1969
Stress Corrosion Crack Growth in Austenitic Stainless Steel journal June 1977
Effect of Loading Rate on Environmentally Controlled Cracking of Sensitized 304 Stainless Steel in High Purity Water journal November 1980
Stress Corrosion Crack Growth in Type 316 Stainless Steel in Supercritical Water journal November 2007
Emerging Issues and Fundamental Processes in Environmental Cracking in Hot Water journal May 2008
Effects of Temperature on Crack Growth Rate in Sensitized Type 304 Stainless Steel and Alloy 600 journal September 1993
Influence of Nitrate on Pit Stability in Austenitic Stainless Steel journal July 2010
Intergranular Stress Corrosion Cracking of Austenitic Stainless Steel at Temperatures Below 100 C — A Review journal August 1982
Effects of Transients in Water Chemistry, Temperature, and Loading on Intergranular Stress Corrosion Cracking of AISI 304 Stainless Steel journal March 1986
Probabilistic Fracture Mechanics Simulation of Stress Corrosion Cracking Using Accelerated Laboratory Testing and Multi-Scale Modeling journal July 2016
Stress Corrosion Cracking and Localized Corrosion of Carbon Steel in Nitrate Solutions journal July 2016
Mechanistic Studies of Intergranular Stress Corrosion Cracking in Al-Mg Alloys under Atmospheric Exposure Conditions journal July 2018
A Brief History of Environmental Cracking in Hot Water journal July 2018
Atmospheric Stress Corrosion Cracking of Stainless Steel Rock Climbing Anchors, Part 2: Laboratory Experiments journal August 2019
Investigation of IG-SCC Growth Kinetics in Al-Mg Alloys in Thin Film Environments journal May 2021
A Review of the Governing Factors in Pit-to-Crack Transitions of Metallic Structures journal November 2022