Nanocavity-Mediated Purcell Enhancement of Er in TiO 2 Thin Films Grown via Atomic Layer Deposition
- Pritzker School of Molecular Engineering, University of Chicago, Chicago, Illinois 60637, United States, Materials Science Division, Argonne National Laboratory, Lemont, Illinois 60439, United States
- Pritzker School of Molecular Engineering, University of Chicago, Chicago, Illinois 60637, United States, Materials Science Division, Argonne National Laboratory, Lemont, Illinois 60439, United States, Center for Molecular Engineering, Argonne National Laboratory, Lemont, Illinois 60439, United States
- Pritzker School of Molecular Engineering, University of Chicago, Chicago, Illinois 60637, United States
- Center for Nanoscale Materials, Argonne National Laboratory, Lemont, Illinois 60439, United States
- Materials Science Division, Argonne National Laboratory, Lemont, Illinois 60439, United States, Center for Molecular Engineering, Argonne National Laboratory, Lemont, Illinois 60439, United States
- Pritzker School of Molecular Engineering, University of Chicago, Chicago, Illinois 60637, United States, Materials Science Division, Argonne National Laboratory, Lemont, Illinois 60439, United States, Center for Molecular Engineering, Argonne National Laboratory, Lemont, Illinois 60439, United States, Department of Physics, University of Chicago, Chicago, Illinois 60637, United States
- Center for Molecular Engineering, Argonne National Laboratory, Lemont, Illinois 60439, United States, Center for Nanoscale Materials, Argonne National Laboratory, Lemont, Illinois 60439, United States, Nanoscience and Technology Division, Argonne National Laboratory, Lemont, Illinois 60439, United States
Not Available
- Sponsoring Organization:
- USDOE
- OSTI ID:
- 2329336
- Alternate ID(s):
- OSTI ID: 2335703; OSTI ID: 2477756
- Journal Information:
- ACS Nano, Journal Name: ACS Nano Journal Issue: 14 Vol. 18; ISSN 1936-0851
- Publisher:
- American Chemical SocietyCopyright Statement
- Country of Publication:
- United States
- Language:
- English
Similar Records
Enhanced photocatalytic performance in atomic layer deposition grown TiO{sub 2} thin films via hydrogen plasma treatment
Redox Properties of TiO 2 Thin Films Grown on Mesoporous Silica by Atomic Layer Deposition
Laser damage properties of TiO{sub 2}/Al{sub 2}O{sub 3} thin films grown by atomic layer deposition
Journal Article
·
2015
· Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films
·
OSTI ID:22392124
+2 more
Redox Properties of TiO 2 Thin Films Grown on Mesoporous Silica by Atomic Layer Deposition
Journal Article
·
2023
· Journal of Physical Chemistry Letters
·
OSTI ID:1973532
+4 more
Laser damage properties of TiO{sub 2}/Al{sub 2}O{sub 3} thin films grown by atomic layer deposition
Journal Article
·
2011
· Applied Optics
·
OSTI ID:22036707
+3 more