Title: Tailoring the Surface of Metal Halide Perovskites to Enable the Atomic Layer Deposition of Metal Oxide Contacts

Journal Article · · ACS Applied Energy Materials

Replacing organic contact layers with inorganic counterparts, such as metal oxides, is one strategy for improving long-term device stability in metal halide perovskite solar cells. Often, the methods used to deposit metal oxide thin films are incompatible with metal halide perovskites, creating challenges for the fabrication of contacts above the perovskite absorber layer. In this study, we utilize a one-step, solution treatment of the top surface of Cs0.25FA0.75Pb(Br0.20I0.80)3 to create a thin (~1 nm) overlayer of lead sulfide (PbS) to protect the underlying perovskite during subsequent deposition. X-ray characterization of the surface region shows that the PbS overlayer limits undesirable changes to the perovskite structure and stoichiometry during atomic layer deposition (ALD) of SnO2. This protection enables ALD growth of SnO2 electron contacts on top of the perovskite without an organic transport layer (e.g., C60), resulting in a solar cell with a power conversion efficiency of 5.8%. This result is a marked improvement over devices with ALD SnO2 grown directly on the perovskite without a PbS overlayer, which produce no power output. Furthermore, the interface characterization and device results in this study highlight some of the key challenges associated with ALD metal oxide growth on perovskite materials and can help inform the future design of inorganic contact layer deposition in solar photovoltaic technologies.

Research Organization:
Stanford University, CA (United States)
Sponsoring Organization:
USDOE Office of Energy Efficiency and Renewable Energy (EERE), Renewable Power Office. Solar Energy Technologies Office
Grant/Contract Number:
EE0008084
OSTI ID:
2307830
Journal Information:
ACS Applied Energy Materials, Journal Name: ACS Applied Energy Materials Journal Issue: 9 Vol. 4; ISSN 2574-0962
Publisher:
American Chemical Society (ACS)Copyright Statement
Country of Publication:
United States
Language:
English

References (56)

The Thickogram: a method for easy film thickness measurement in XPS journal January 2000
Perovskite Solar Cells with Inorganic Electron- and Hole-Transport Layers Exhibiting Long-Term (≈500 h) Stability at 85 °C under Continuous 1 Sun Illumination in Ambient Air journal May 2018
State‐of‐the‐Art Electron‐Selective Contacts in Perovskite Solar Cells journal August 2018
Interfacial Effects of Tin Oxide Atomic Layer Deposition in Metal Halide Perovskite Photovoltaics journal June 2018
The Role of Charge Selective Contacts in Perovskite Solar Cell Stability journal December 2018
Enhanced Nucleation of Atomic Layer Deposited Contacts Improves Operational Stability of Perovskite Solar Cells in Air journal October 2019
Hole Transport Materials in Conventional Structural (n–i–p) Perovskite Solar Cells: From Past to the Future journal January 2020
Recent Progress in Organic Electron Transport Materials in Inverted Perovskite Solar Cells journal April 2019
Atomic Layer Deposition of Functional Layers in Planar Perovskite Solar Cells journal October 2019
Effect of F, Cl and Br doping on electrical properties of sprayed SnO2 films journal January 1996
Properties of oxidized silicon as determined by angular-dependent X-ray photoelectron spectroscopy journal December 1976
Interfacial Contact Passivation for Efficient and Stable Cesium-Formamidinium Double-Cation Lead Halide Perovskite Solar Cells journal January 2020
Stabilizing the MAPbI3 perovksite via the in-situ formed lead sulfide layer for efficient and robust solar cells journal August 2020
Cost Analysis of Perovskite Tandem Photovoltaics journal August 2018
Overcoming Redox Reactions at Perovskite-Nickel Oxide Interfaces to Boost Voltages in Perovskite Solar Cells journal August 2020
Sources of Pb(0) artefacts during XPS analysis of lead halide perovskites journal September 2019
A brief review of atomic layer deposition: from fundamentals to applications journal June 2014
Sputtered rear electrode with broadband transparency for perovskite solar cells journal October 2015
C 60 as an Efficient n-Type Compact Layer in Perovskite Solar Cells journal June 2015
Photoluminescence and Photoconductivity to Assess Maximum Open-Circuit Voltage and Carrier Transport in Hybrid Perovskites and Other Photovoltaic Materials journal June 2018
Reaction Temperature and Partial Pressure Induced Etching of Methylammonium Lead Iodide Perovskite by Trimethylaluminum journal April 2019
SnO x Atomic Layer Deposition on Bare Perovskite—An Investigation of Initial Growth Dynamics, Interface Chemistry, and Solar Cell Performance journal January 2021
Charge Transport Layers Limiting the Efficiency of Perovskite Solar Cells: How To Optimize Conductivity, Doping, and Thickness journal July 2019
Atomic Layer Deposition of Electron Selective SnO x and ZnO Films on Mixed Halide Perovskite: Compatibility and Performance journal August 2017
Chemical Analysis of the Interface between Hybrid Organic–Inorganic Perovskite and Atomic Layer Deposited Al 2 O 3 journal January 2019
Extremely Robust Gas-Quenching Deposition of Halide Perovskites on Top of Hydrophobic Hole Transport Materials for Inverted (p–i–n) Solar Cells by Targeting the Precursor Wetting Issue journal September 2019
The Molybdenum Oxide Interface Limits the High-Temperature Operational Stability of Unencapsulated Perovskite Solar Cells journal June 2020
Low-Temperature Nb-Doped SnO 2 Electron-Selective Contact Yields over 20% Efficiency in Planar Perovskite Solar Cells journal March 2018
Barrier Design to Prevent Metal-Induced Degradation and Improve Thermal Stability in Perovskite Solar Cells journal June 2018
Minimizing Current and Voltage Losses to Reach 25% Efficient Monolithic Two-Terminal Perovskite–Silicon Tandem Solar Cells journal August 2018
Thermally Stable Perovskite Solar Cells by Systematic Molecular Design of the Hole-Transport Layer journal January 2019
21.6%-Efficient Monolithic Perovskite/Cu(In,Ga)Se 2 Tandem Solar Cells with Thin Conformal Hole Transport Layers for Integration on Rough Bottom Cell Surfaces journal January 2019
Not All That Glitters Is Gold: Metal-Migration-Induced Degradation in Perovskite Solar Cells journal May 2016
Atomic Layer Deposition of Lead Sulfide Thin Films for Quantum Confinement journal August 2009
Electron Injection from Colloidal PbS Quantum Dots into Titanium Dioxide Nanoparticles journal October 2008
Suppressed decomposition of organometal halide perovskites by impermeable electron-extraction layers in inverted solar cells journal January 2017
Origin and elimination of photocurrent hysteresis by fullerene passivation in CH3NH3PbI3 planar heterojunction solar cells journal December 2014
Perovskite–fullerene hybrid materials suppress hysteresis in planar diodes journal May 2015
Perovskite solar cells employing organic charge-transport layers journal December 2013
Tailored interfaces of unencapsulated perovskite solar cells for >1,000 hour operational stability journal January 2018
Fully textured monolithic perovskite/silicon tandem solar cells with 25.2% power conversion efficiency journal June 2018
Hybrid perovskite films approaching the radiative limit with over 90% photoluminescence quantum efficiency journal April 2018
Surface passivation of perovskite film for efficient solar cells journal April 2019
Efficient perovskite solar cells via improved carrier management journal February 2021
Highly efficient planar perovskite solar cells through band alignment engineering journal January 2015
Self limiting atomic layer deposition of Al 2 O 3 on perovskite surfaces: a reality? journal January 2016
Stabilizing hybrid perovskites against moisture and temperature via non-hydrolytic atomic layer deposited overlayers journal January 2015
Atomic layer deposition for perovskite solar cells: research status, opportunities and challenges journal January 2017
Monolithic perovskite/silicon-homojunction tandem solar cell with over 22% efficiency journal January 2017
Atomic layer deposition for efficient and stable perovskite solar cells journal January 2019
Applications of atomic layer deposition and chemical vapor deposition for perovskite solar cells journal January 2020
The chemistry and energetics of the interface between metal halide perovskite and atomic layer deposited metal oxides journal December 2020
Efficient and stable large-area perovskite solar cells with inorganic charge extraction layers journal October 2015
Stabilizing halide perovskite surfaces for solar cell operation with wide-bandgap lead oxysalts journal August 2019
Monolithic perovskite/silicon tandem solar cell with >29% efficiency by enhanced hole extraction journal December 2020
Optical modeling of wide-bandgap perovskite and perovskite/silicon tandem solar cells using complex refractive indices for arbitrary-bandgap perovskite absorbers journal January 2018