DOE PAGES title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Elevated temperature nanoscratch of Inconel 617 Superalloy

Journal Article · · Mechanics Research Communications
 [1];  [2];  [3]; ORCiD logo [2]
  1. George Mason Univ., Fairfax, VA (United States); OSTI
  2. Texas A & M Univ., College Station, TX (United States)
  3. George Mason Univ., Fairfax, VA (United States)

Inconel 617 superalloy is a main candidate to be used for mechanical and tribo-components in high temperature helium-cooled reactors. Recent findings show that it grows a unique surface oxide, especially under high temperature helium with distinct wear, friction, and contact properties. Here, this study reports the elevated temperature nanoscratch behavior of Inconel 617 and further utilizes it to understand the effect of temperature on contact friction constituent contributors, adhesion and plowing at small scales. Inconel 617 is aged in high temperature helium, and consequently, the total kinetic friction coefficient of the alloy surface oxide is obtained in temperatures ranging from 25 °C to 400 °C. A finite element model is developed and validated based on the experimental results. The model is then utilized along with previously established techniques to determine the adhesion and plowing components of the friction coefficient. At small scale, the experimental results show that with increasing temperature the friction coefficient increases. It was inferred that this increase is mainly due to the increased contribution of plowing friction at high levels of deformation.

Research Organization:
Texas A & M Univ., College Station, TX (United States). Texas A & M Engineering Experiment Station
Sponsoring Organization:
USDOE; USDOE Office of Nuclear Energy (NE)
Grant/Contract Number:
NE0008549
OSTI ID:
1977431
Journal Information:
Mechanics Research Communications, Journal Name: Mechanics Research Communications Vol. 121; ISSN 0093-6413
Publisher:
ElsevierCopyright Statement
Country of Publication:
United States
Language:
English

References (25)

High temperature corrosion of structural materials under gas-cooled reactor helium journal February 2006
Analysis of the apparent friction of polymeric surfaces journal October 2006
A Review on Micro- and Nanoscratching/Tribology at High Temperatures: Instrumentation and Experimentation journal July 2018
A theory of friction and wear during the abrasion of metals journal March 1962
Review of the tribology of diamond-like carbon journal September 1993
Investigation of the overall friction coefficient in single-pass scratch test journal January 2002
Influences of grain size and temperature on tribological characteristics of CuAlNi alloys under nanoindentation and nanoscratch journal November 2020
Plastic activity in nanoscratch molecular dynamics simulations of pure aluminium journal February 2014
On fracture in finite strain gradient plasticity journal May 2016
Multiscale mechanical and tribological characterizations of additively manufactured polyamide 12 parts with different print orientations journal April 2019
High-temperature tribological behavior of structural materials after conditioning in impure-helium environments for high-temperature gas-cooled reactor applications journal August 2019
Effects of mechanical properties and surface friction on elasto-plastic sliding contact journal April 2008
High temperature nanoscratching of single crystal silicon under reduced oxygen condition journal January 2017
Elevated temperature mechanical properties of Inconel 617 surface oxide using nanoindentation journal June 2020
Surface reliability of annealed and tempered solar protective glasses: Indentation and scratch behavior journal January 2017
High temperature scratch testing of hard PVD coatings deposited on surface treated tool steel. journal September 2014
Prediction of friction coefficients in nanoscratch testing of metals based on material flow lines journal April 2018
The effect of Berkovich tip orientations on friction coefficient in nanoscratch testing of metals journal November 2016
Elevated temperature tribology of Ni alloys under helium environment for nuclear reactor applications journal July 2018
Nanoscratch study of hard HfB2 thin films using experimental and finite element techniques journal February 2010
Study of wear mechanisms at high temperature scratch testing journal October 2017
In-situ friction and fretting wear measurements of Inconel 617 at elevated temperatures journal September 2018
Yield Maps for Single and Bilayer Thin Films Under Scratch journal April 2016
TiN coating adhesion studies using the scratch test method journal November 1985
Surface deformation and friction characteristic of nano scratch at ductile-removal regime for optical glass BK7 journal January 2016