Title: Modeling lattice rotation fields from discrete crystallographic slip bands in superalloys

Journal Article · · Extreme Mechanics Letters

Here in this work, we investigate the relationship between an intense slip band (ISB) and the zone of large lattice rotations that forms ahead of the tip of the ISB. We develop a crystal plasticity finite element model of a discrete ISB lying within an oligocrystalline assembly and calculate the local crystalline stress and lattice rotation fields generated by the ISB. The calculations demonstrate that, first, a region of severe lattice rotations, commonly referred to as a microvolume, does not form without the ISB, and second, large amounts of accumulated slip in the ISB are required to enlarge the microvolume to sizes and rotation magnitudes observed experimentally. Ahead of the ISB tip, the quintessential plastic zone always forms, but the atypical microvolume forms when non-concentrated and spatially diffuse slip is activated by the ISB-induced stress field. This result suggests that the detrimental ISB/microvolume pair will likely appear in pairs of crystals in which transmission of the slip from the ISB is severely blocked by the grain boundary, a hypothesis that we verify with a few target cases.

Research Organization:
University of California, Santa Barbara, CA (United States)
Sponsoring Organization:
USDOE Office of Science (SC), Basic Energy Sciences (BES)
Grant/Contract Number:
SC0018901
OSTI ID:
1977078
Journal Information:
Extreme Mechanics Letters, Journal Name: Extreme Mechanics Letters Journal Issue: C Vol. 49; ISSN 2352-4316
Publisher:
ElsevierCopyright Statement
Country of Publication:
United States
Language:
English

References (38)

Effect of the form of the stressed condition on the character of distribution of the microdeformations in metals journal June 1976
Microstructural statistics for fatigue crack initiation in polycrystalline nickel-base superalloys journal September 2017
Review on slip transmission criteria in experiments and crystal plasticity models journal November 2015
Competing Modes for Crack Initiation from Non-metallic Inclusions and Intrinsic Microstructural Features During Fatigue in a Polycrystalline Nickel-Based Superalloy journal July 2018
Crystallographic texture evolution in bulk deformation processing of FCC metals journal January 1992
Dislocation pile-up and grain boundary interactions in 304 stainless steel journal June 1986
Prediction of slip transfer mechanisms across grain boundaries journal May 1989
The role of annealing twin boundaries in the cyclic deformation of f.c.c. materials journal September 1992
The analysis of shear banding with a dislocation based gradient plasticity model journal November 2000
Analysis of the different slip systems activated by tension in a α/β titanium alloy in relation with local crystallographic orientation journal February 2005
Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature journal December 2009
Simulation of slip band evolution in duplex Ti–6Al–4V journal February 2010
Slip band–grain boundary interactions in commercial-purity titanium journal September 2014
Grain boundary–slip bands interactions: Impact on the fatigue crack initiation in a polycrystalline forged Ni-based superalloy journal October 2015
Crystal plasticity investigation of the microstructural factors influencing dislocation channeling in a model irradiated bcc material journal May 2016
Measurements of plastic localization by heaviside-digital image correlation journal September 2018
Intragranular localization induced by softening crystal plasticity: Analysis of slip and kink bands localization modes from high resolution FFT-simulations results journal August 2019
Direct measurements of slip irreversibility in a nickel-based superalloy using high resolution digital image correlation journal March 2020
Slip band characteristics in the presence of grain boundaries in nickel-based superalloy journal July 2020
Grain boundaries and interfaces in slip transfer journal August 2014
Fatigue crack initiation, slip localization and twin boundaries in a nickel-based superalloy journal August 2014
Micro-scale fatigue mechanisms in metals: Insights gained from small-scale experiments and discrete dislocation dynamics simulations journal October 2019
Finite element simulation of PSB macroband nucleation and propagation in single crystal nickel cycled at low plastic strain amplitudes journal July 2006
Investigation of three-dimensional aspects of grain-scale plastic surface deformation of an aluminum oligocrystal journal December 2008
A crystal plasticity study of heterophase interface character stability of Cu/Nb bicrystals journal September 2013
FFT-based simulations of slip and kink bands formation in 3D polycrystals: Influence of strain gradient crystal plasticity journal April 2021
TEM observations and finite element modelling of channel deformation in pre-irradiated austenitic stainless steels – Interactions with free surfaces and grain boundaries journal November 2010
Continuum modeling of localized deformation in irradiated bcc materials journal January 2013
Measurement of elastic and rotation fields during irreversible deformation using Heaviside-digital image correlation journal November 2020
Characterisation of strain localisation processes during fatigue crack initiation and early crack propagation by SEM-DIC in an advanced disc alloy journal June 2017
Slip transfer across grain/twin boundaries in polycrystalline Ni-based superalloys journal July 2017
A criterion for slip transfer at grain boundaries in Al journal March 2020
Grain boundary slip transfer classification and metric selection with artificial neural networks journal August 2020
Insight into microstructure-sensitive elastic strain concentrations from integrated computational modeling and digital image correlation journal February 2021
A quantitative study of stress fields ahead of a slip band blocked by a grain boundary in unalloyed magnesium journal February 2020
TEM in situ deformation study of the interaction of lattice dislocations with grain boundaries in metals journal July 1990
Xi. The origin of fatigue fracture in copper journal February 1956
Microstructural mechanisms of cyclic deformation, fatigue crack initiation and early crack growth journal March 2015