Title: Crystallographic effects on transgranular chloride-induced stress corrosion crack propagation of arc welded austenitic stainless steel

Journal Article · · npj Materials Degradation

Abstract The effect of crystallography on transgranular chloride-induced stress corrosion cracking (TGCISCC) of arc welded 304L austenitic stainless steel is studied on >300 grains along crack paths. Schmid and Taylor factor mismatches across grain boundaries (GBs) reveal that cracks propagate either from a hard to soft grain, which can be explained merely by mechanical arguments, or soft to hard grain. In the latter case, finite element analysis reveals that TGCISCC will arrest at GBs without sufficient mechanical stress, favorable crystallographic orientations, or crack tip corrosion. GB type does not play a significant role in determining TGCISCC cracking behavior nor susceptibility. TGCISCC crack behaviors at GBs are discussed in the context of the competition between mechanical, crystallographic, and corrosion factors.

Research Organization:
Sandia National Laboratories (SNL-NM), Albuquerque, NM (United States)
Sponsoring Organization:
Purdue University; USDOE; USDOE National Nuclear Security Administration (NNSA)
Grant/Contract Number:
NA0003525; NE0008759
OSTI ID:
1870052
Report Number(s):
SAND2022-5221J; 43; PII: 252
Journal Information:
npj Materials Degradation, Journal Name: npj Materials Degradation Journal Issue: 1 Vol. 6; ISSN 2397-2106
Publisher:
Nature Publishing GroupCopyright Statement
Country of Publication:
United Kingdom
Language:
English

References (66)

Stacking fault energies of seven commercial austenitic stainless steels journal July 1975
Role of Anisotropic Strength and Stiffness in Governing the Initiation and Propagation of Yielding in Polycrystalline Solids journal January 2019
Marine Atmospheric SCC of Unsensitized Stainless Steel Rock Climbing Protection journal August 2008
The structure of high-angle grain boundaries journal November 1966
Chromium depletion and martensite formation at grain boundaries in sensitised austenitic stainless steel journal March 1986
The influence of chloride content, pH and temperature of test solution on the occurrence of stress corrosion cracking with austenitic stainless steel journal January 1977
The effect of chloride ions on stress corrosion cracking of type 304 and type 316 austenitic stainless steels in sulfuric acid solution journal November 1993
On the finite element method in linear fracture mechanics journal July 1970
Microstructural and microchemical mechanisms controlling intergranular stress corrosion cracking in light-water-reactor systems journal October 1994
Dislocation pile-up and grain boundary interactions in 304 stainless steel journal June 1986
Stress corrosion microcleavage in a ductile f.c.c. alloy journal May 1993
Mechanism of brittle fracture in a ductile 316 alloy during stress corrosion journal July 1990
The corrosion-enhanced plasticity model for stress corrosion cracking in ductile fcc alloys journal April 1996
Taylor factors in materials with many deformation modes journal August 1996
In situ TEM study of stress corrosion cracking of austenitic stainless steel journal July 2003
Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys journal May 2001
Numerical simulations of hydrogen–dislocation interactions in fcc stainless steels. journal April 2002
A dislocation-based model for all hardening stages in large strain deformation journal September 1998
A finite-element computational model of chloride-induced transgranular stress-corrosion cracking of austenitic stainless steel journal September 2008
Simulation of inter- and transgranular crack propagation in polycrystalline aggregates due to stress corrosion cracking journal August 2009
Fundamental studies on stress-corrosion cracking in iron and underlying mechanisms journal September 2010
Orientation dependence of twinning and strain hardening behaviour of a high manganese twinning induced plasticity steel with polycrystalline structure journal December 2011
Grain-scale measurement of slip resistances in aluminum polycrystals using spherical nanoindentation journal May 2015
A mechanistic study of the temperature dependence of the stress corrosion crack growth rate in SUS316 stainless steels exposed to PWR primary water journal August 2016
On the relationship between grain boundary connectivity, coincident site lattice boundaries, and intergranular stress corrosion cracking journal October 2004
A model to predict the evolution of pitting corrosion and the pit-to-crack transition incorporating statistically distributed input parameters journal August 2006
The effect of test temperature on SCC behavior of austenitic stainless steels in boiling saturated magnesium chloride solution journal December 2006
The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solutions journal July 2007
A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies journal January 2009
A new aspect on intergranular hydrogen embrittlement mechanism of solution annealed types 304, 316 and 310 austenitic stainless steels journal September 2009
New insight into the pit-to-crack transition from finite element analysis of the stress and strain distribution around a corrosion pit journal April 2010
Discontinuous surface cracks during stress corrosion cracking of stainless steel single crystal journal November 2011
Stress corrosion cracking under low stress: Continuous or discontinuous cracks? journal March 2014
The initiation and propagation of chloride-induced transgranular stress-corrosion cracking (TGSCC) of 304L austenitic stainless steel under atmospheric conditions journal November 2014
Stress corrosion cracking at low loads: Surface slip and crystallographic analysis journal November 2015
Crystallographic orientation data from chloride-induced stress corrosion crack (CISCC) paths in gas tungsten arc welded (GTAW) austenitic stainless steel 304L journal June 2022
Pitting and stress corrosion cracking behavior in welded austenitic stainless steel journal January 2005
Failure analysis of a stainless steel pipeline journal July 2008
Stress corrosion cracking in 316L stainless steel bellows of a pressure safety valve journal January 2014
Verification of crack opening criterion deduced by newly derived micro-crack evolution equation journal February 2017
Three dimensional observations and modelling of intergranular stress corrosion cracking in austenitic stainless steel journal June 2006
Stress corrosion cracking of stainless-steel canister for concrete cask storage of spent fuel journal September 2008
Stress corrosion cracking of austenitic weld deposits in a salt spray environment journal October 2015
Chloride-induced stress corrosion cracking of used nuclear fuel welded stainless steel canisters: A review journal November 2015
On residual stress analysis and microstructural evolution for stainless steel type 304 spent nuclear fuel canisters weld joint: Numerical and experimental studies journal June 2020
Effect of Salt Composition and Microstructure on Stress Corrosion Cracking of 316L Austenitic Stainless Steel for Dry Storage Canisters journal March 2021
Effect of heat input on the microstructure, residual stresses and corrosion resistance of 304L austenitic stainless steel weldments journal July 2014
Role of residual stresses induced by industrial fabrication on stress corrosion cracking susceptibility of austenitic stainless steel journal August 2011
A new method for predicting susceptibility of austenitic stainless steels to intergranular stress corrosion cracking journal February 2020
Relationship between localized strain and irradiation assisted stress corrosion cracking in an austenitic alloy journal April 2011
The effect of salt loading on chloride-induced stress corrosion cracking of 304L austenitic stainless steel under atmospheric conditions journal December 2019
Modelling of the evolution of stress corrosion cracks from corrosion pits journal February 2006
Rates of intergranular environment assisted cracking in three-dimensional model microstructures journal December 2007
Mechanical Behavior of Materials book January 2009
Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys journal September 2018
In Situ Investigation of High Humidity Stress Corrosion Cracking of 7075 Aluminum Alloy by Three-Dimensional (3D) X-ray Synchrotron Tomography journal May 2014
Observations of Intergranular Stress Corrosion Cracking in a Grain-Mapped Polycrystal journal July 2008
Stress corrosion cracking: 1965–1990 journal January 1990
Assessing the risk of under-deposit chloride-induced stress corrosion cracking in austenitic stainless steel nuclear waste containers journal June 2014
X-ray microtomographic observation of intergranular stress corrosion cracking in sensitised austenitic stainless steel journal September 2006
Fracture Mechanics book March 2017
Final Report: Characterization of Canister Mockup Weld Residual Stresses report December 2016
Boiling Temperatures of Mg Cl Solutions -Their Application in Stress Corrosion Studies journal October 1967
Role of Slip Step Emergence in the Early Stages of Stress Corrosion Cracking in Face Centered Iron-Nickel-Chromium Alloys journal May 1967
Environment-Induced Deformation Localization During Transgranular Stress Corrosion Cracking journal May 1996
Toward Understanding the Effects of Strain and Chloride Deposition Density on Atmospheric Chloride-Induced Stress Corrosion Cracking of Type 304 Austenitic Stainless Steel Under MgCl 2 and FeCl 3 :MgCl 2 Droplets journal October 2018