Title: Additive manufacturing of high-strength multiphase nanostructures in the binary Ni–Nb system for the discovery of new types of superalloys

Journal Article · · Journal of Materials Research

Abstract Ni-based superalloys have been studied extensively due to their impressive mechanical properties, including strength and creep resistance at high temperatures. Growing interest surrounding additive manufacturing (AM) methods has led to recent investigations of alloys that are traditionally difficult to process, including Ni-based superalloys. Recent work has shown that AM methods enable high-throughput materials discovery and optimization of difficult- or impractical-to-process alloys, including those with high or even majority refractory element compositions. This work focuses on AM-enabled investigations of composition-dependent mechanical and microstructural properties for Ni–Nb binary alloys. Specifically, we report on the mechanical behavior of compositionally-graded Ni x Nb 1− x and uniform composition Ni 59.5 Nb 40.5 specimens made with AM. The AM fabrication process resulted in extraordinarily high strength, attributed to the formation of a dual-phase microstructure consisting of δ-Ni 3 Nb and µ-Ni 6 Nb 7 intermetallic compounds with nanostructured and multimodal grain size and eutectic lamellar spacing. Graphic Abstract

Sponsoring Organization:
USDOE National Nuclear Security Administration (NNSA)
OSTI ID:
1813879
Journal Information:
Journal of Materials Research, Journal Name: Journal of Materials Research Journal Issue: 16 Vol. 36; ISSN 0884-2914
Publisher:
Cambridge University Press (CUP)Copyright Statement
Country of Publication:
United States
Language:
English

References (78)

Fabrication of Binary Ni-Nb Bulk Metallic Glass with High Strength and Compressive Plasticity journal October 2006
The balance of mechanical and environmental properties of a multielement niobium-niobium silicide-basedIn Situ composite journal December 1996
Coherency strengthening in Ni base alloys hardened by DO22 γ′ precipitates journal January 1974
The effect of hydrogen on fracture toughness of the Fe-Ni-Co superalloy IN903 journal August 1987
Linking microstructural evolution and macro-scale friction behavior in metals journal November 2016
Study on crystallization phenomenon and thermal stability of binary Ni–Nb amorphous alloy journal August 2016
Tensile Properties of Ni-Based Superalloy 720Li: Temperature and Strain Rate Effects journal July 2008
Strengthening Mechanisms in Polycrystalline Multimodal Nickel-Base Superalloys journal May 2009
Studies of Standard Heat Treatment Effects on Microstructure and Mechanical Properties of Laser Net Shape Manufactured INCONEL 718 journal August 2009
Characterization of Strain-Rate Sensitivity and Grain Boundary Structure in Nanocrystalline Gold-Copper Alloys journal September 2009
Modeling solid solution strengthening in nickel alloys journal June 1997
Metal Additive Manufacturing: A Review journal April 2014
Plastic deformation of single crystals of sapphire: Basal slip and twinning journal September 1957
Toughening mechanisms for ceramic materials journal January 1992
The formation and thermal stability of amorphous Ni-Nb alloy powder synthesized by mechanical alloying journal October 1987
Indentation size effects in crystalline materials: A law for strain gradient plasticity journal March 1998
Metal Fabrication by Additive Manufacturing Using Laser and Electron Beam Melting Technologies journal January 2012
Solidification kinetics and phase formation of undercooled eutectic Ni–Nb melts journal August 1999
Toward a quantitative understanding of mechanical behavior of nanocrystalline metals journal July 2007
Mechanical behavior of amorphous alloys journal July 2007
The Hall–Petch breakdown in nanocrystalline metals: A crossover to glass-like deformation journal October 2007
Enhanced solid solution effects on the strength of nanocrystalline alloys journal February 2011
On the structure of defects in the Fe7Mo6 μ-Phase journal April 2019
Achieving high strength and ductility in traditionally brittle soft magnetic intermetallics via additive manufacturing journal November 2019
Additive manufacturing of an iron-based bulk metallic glass larger than the critical casting thickness journal June 2018
High-throughput additive manufacturing and characterization of refractory high entropy alloys journal June 2020
Scratch test model for the determination of fracture toughness journal January 2011
Hall–Petch relationship in nanocrystalline Ni and Be–B alloys journal March 2005
High strength ultrafine eutectic Fe–Nb–Al composites with enhanced plasticity journal May 2008
Steady state flow of the FeCoNiCrMn high entropy alloy at elevated temperatures journal December 2014
Grain size softening effect in intermetallics journal July 2016
The microstructure and hardness of Ni-Co-Al-Ti-Cr quinary alloys journal December 2016
Effect of precipitates on high-temperature tensile strength of a high W-content cast Ni-based superalloy journal August 2019
Characterization, corrosion resistance and hardness of rapidly solidified Ni–Nb alloys journal July 2020
Effect of microstructural constituents on mechanical properties and fracture toughness of Inconel 718 with anomalous deformation behavior at 650 °C journal December 2020
High-throughput stochastic tensile performance of additively manufactured stainless steel journal March 2017
Structure relaxation effect on hardness and shear transformation zone volume of a Ni Nb metallic glassy film journal November 2018
Ultrasonic additive manufacturing of bulk Ni-based metallic glass journal February 2019
A critical assessment of the effect of indentation spacing on the measurement of hardness and modulus using instrumented indentation testing journal February 2019
Selective laser melting of a Ti-based bulk metallic glass journal February 2018
Effect of nanocrystalline and ultrafine grain sizes on the strain rate sensitivity and activation volume: fcc versus bcc metals journal September 2004
General relationship between strength and hardness journal November 2011
Loading rate effect on the creep behavior of metallic glassy films and its correlation with the shear transformation zone journal January 2015
On the strain rate sensitivity of plastic flow in metallic glasses journal February 2015
Effect of solution heat treatment on the precipitation behavior and strengthening mechanisms of electron beam smelted Inconel 718 superalloy journal March 2017
Microstructure and hardness studies of Inconel 718 manufactured by selective laser melting before and after solution heat treatment journal March 2017
Strain rate sensitivity of a novel refractory high entropy alloy: Intrinsic versus extrinsic effects journal October 2019
Influence of post-heat-treatment on the microstructure and fracture toughness properties of Inconel 718 fabricated with laser directed energy deposition additive manufacturing journal November 2020
Microtwinning and other shearing mechanisms at intermediate temperatures in Ni-based superalloys journal August 2009
The use of high-entropy alloys in additive manufacturing journal April 2015
3D printing of high-strength aluminium alloys journal September 2017
Nanostructuring of metals by severe plastic deformation for advanced properties journal August 2004
Alloy design for aircraft engines journal July 2016
High-entropy alloys journal June 2019
Intermetallic eutectic alloys in the Ni-Al-Zr system with attractive high temperature properties journal January 2014
Binary Ni–Nb bulk metallic glasses journal January 2006
Six decades of the Hall–Petch effect – a survey of grain-size strengthening studies on pure metals journal June 2016
Inverse Hall–Petch like behaviour in a mechanically milled nanocrystalline Al 5 Fe 2 intermetallic phase journal July 2016
Stress-driven crystallization via shear-diffusion transformations in a metallic glass at very low temperatures journal June 2015
Ultimate Strength of Metals journal March 2020
Low friction in bcc metals via grain boundary sliding journal June 2020
The quantitative analysis of thin specimens journal March 1975
A fracture-resistant high-entropy alloy for cryogenic applications journal September 2014
Effect of heat treatment on the fine structure and properties of a niobium-base superalloy journal December 2016
Metal Additive Manufacturing: A Review of Mechanical Properties journal July 2016
Strengthening mechanisms in Inconel 718 superalloy journal March 1983
An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments journal June 1992
Structure and Mechanical Behavior of Bulk Nanocrystalline Materials journal February 1999
Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodology journal January 2004
Experimental determination of the fracture toughness via microscratch tests: Application to polymers, ceramics, and metals journal January 2012
Grain boundary relaxation strengthening of nanocrystalline Ni–W alloys journal March 2012
Additive manufacturing of Ni-based superalloys: The outstanding issues journal October 2016
Influence of microstructure and processing on mechanical properties of advanced Nb-silicide alloys journal January 2012
Effect of Alloy Chemistry on the High Temperature Strengths and Room Temperature Fracture Toughness of Advanced Nb-Based Alloys journal January 2004
Strain Rate Dependence on Nanoindentation Responses of Interfacial Intermetallic Compounds in Electronic Solder Joints with Cu and Ag Substrates journal January 2009
Niobium Base Superalloys: Achievement of a Coherent Ordered Precipitate Structure in the Nb Solid-Solution journal July 2019
High Entropy Alloys Manufactured by Additive Manufacturing journal May 2020
Microstructural Properties of Nb-Si Based Alloys Manufactured by Powder Metallurgy journal July 2011

Similar Records

Characterization of Refractory Alloys Produced by Laser Additive Manufacturing
Journal Article · Thu Nov 24 00:00:00 UTC 2022 · Material Design & Processing Communications · OSTI ID:1899723

Utilizing a Dynamic Segmentation Convolutional Neural Network for Microstructure Analysis of Additively Manufactured Superalloy 718
Conference · Thu Jul 01 04:00:00 UTC 2021 · OSTI ID:1813217

Design of quaternary Ir-Nb-Ni-Al refractory superalloys
Journal Article · Sat Jan 01 04:00:00 UTC 2000 · Metallurgical and Materials Transactions. A, Physical Metallurgy and Materials Science · OSTI ID:20014054

Related Subjects