Optimization of B2/L21 hierarchical precipitate structure to improve creep resistance of a ferritic Fe-Ni-Al-Cr-Ti superalloy via thermal treatments
- Authors:
- Publication Date:
- Sponsoring Org.:
- USDOE Office of Fossil Energy and Carbon Management (FECM)
- OSTI Identifier:
- 1636959
- Grant/Contract Number:
- FE0005868
- Resource Type:
- Publisher's Accepted Manuscript
- Journal Name:
- Scripta Materialia
- Additional Journal Information:
- Journal Name: Scripta Materialia Journal Volume: 161 Journal Issue: C; Journal ID: ISSN 1359-6462
- Publisher:
- Elsevier
- Country of Publication:
- United States
- Language:
- English
Citation Formats
Song, Gian, Hong, Soon Jik, Lee, Jin Kyu, Song, Sung Ho, Hong, Sung Hwan, Kim, Ki Buem, and Liaw, Peter K. Optimization of B2/L21 hierarchical precipitate structure to improve creep resistance of a ferritic Fe-Ni-Al-Cr-Ti superalloy via thermal treatments. United States: N. p., 2019.
Web. doi:10.1016/j.scriptamat.2018.10.004.
Song, Gian, Hong, Soon Jik, Lee, Jin Kyu, Song, Sung Ho, Hong, Sung Hwan, Kim, Ki Buem, & Liaw, Peter K. Optimization of B2/L21 hierarchical precipitate structure to improve creep resistance of a ferritic Fe-Ni-Al-Cr-Ti superalloy via thermal treatments. United States. https://doi.org/10.1016/j.scriptamat.2018.10.004
Song, Gian, Hong, Soon Jik, Lee, Jin Kyu, Song, Sung Ho, Hong, Sung Hwan, Kim, Ki Buem, and Liaw, Peter K. Fri .
"Optimization of B2/L21 hierarchical precipitate structure to improve creep resistance of a ferritic Fe-Ni-Al-Cr-Ti superalloy via thermal treatments". United States. https://doi.org/10.1016/j.scriptamat.2018.10.004.
@article{osti_1636959,
title = {Optimization of B2/L21 hierarchical precipitate structure to improve creep resistance of a ferritic Fe-Ni-Al-Cr-Ti superalloy via thermal treatments},
author = {Song, Gian and Hong, Soon Jik and Lee, Jin Kyu and Song, Sung Ho and Hong, Sung Hwan and Kim, Ki Buem and Liaw, Peter K.},
abstractNote = {},
doi = {10.1016/j.scriptamat.2018.10.004},
journal = {Scripta Materialia},
number = C,
volume = 161,
place = {United States},
year = {Fri Mar 01 00:00:00 EST 2019},
month = {Fri Mar 01 00:00:00 EST 2019}
}
Free Publicly Available Full Text
Publisher's Version of Record
https://doi.org/10.1016/j.scriptamat.2018.10.004
https://doi.org/10.1016/j.scriptamat.2018.10.004
Other availability
Cited by: 27 works
Citation information provided by
Web of Science
Web of Science
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.
Works referenced in this record:
The description of elevated temperature deformation in terms of threshold stresses and back stresses: A review
journal, September 1980
- Gibeling, J. C.; Nix, W. D.
- Materials Science and Engineering, Vol. 45, Issue 2
Creep properties and microstructure of a precipitation-strengthened ferritic Fe–Al–Ni–Cr alloy
journal, June 2014
- Vo, Nhon Q.; Liebscher, Christian H.; Rawlings, Michael J. S.
- Acta Materialia, Vol. 71
Neutron-diffraction study and modeling of the lattice parameters of a NiAl-precipitate-strengthened Fe-based alloy
journal, August 2012
- Teng, Z. K.; Ghosh, G.; Miller, M. K.
- Acta Materialia, Vol. 60, Issue 13-14
Materials for Ultrasupercritical Coal Power Plants - Boiler Materials: Part 1
journal, February 2001
- Viswanathan, R.; Bakker, W.
- Journal of Materials Engineering and Performance, Vol. 10, Issue 1
Nano-sized precipitate stability and its controlling factors in a NiAl-strengthened ferritic alloy
journal, November 2015
- Sun, Zhiqian; Song, Gian; Ilavsky, Jan
- Scientific Reports, Vol. 5, Issue 1
Optimal precipitate shapes in nickel-base γ–γ′ alloys
journal, February 2012
- Van Sluytman, J. S.; Pollock, T. M.
- Acta Materialia, Vol. 60, Issue 4
Primary and secondary precipitates in a hierarchical-precipitate-strengthened ferritic alloy
journal, June 2017
- Song, Gian; Sun, Zhiqian; Poplawsky, Jonathan D.
- Journal of Alloys and Compounds, Vol. 706
Elastically induced shape bifurcations of inclusions
journal, November 1984
- Johnson, W. C.; Cahn, J. W.
- Acta Metallurgica, Vol. 32, Issue 11
A hierarchical microstructure due to chemical ordering in the bcc lattice: Early stages of formation in a ferritic Fe–Al–Cr–Ni–Ti alloy
journal, June 2015
- Liebscher, C. H.; Radmilović, V. R.; Dahmen, U.
- Acta Materialia, Vol. 92
Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys
journal, September 2002
- Seidman, David N.; Marquis, Emmanuelle A.; Dunand, David C.
- Acta Materialia, Vol. 50, Issue 16
The effect of long-term creep on particle coarsening in tempered martensite ferritic steels
journal, December 1989
- Eggeler, G.
- Acta Metallurgica, Vol. 37, Issue 12
Coarsening kinetics of coherent NiAl-type precipitates in FeNiAl and FeNiAlMo alloys
journal, January 1984
- Calderon, H.; Fine, M. E.
- Materials Science and Engineering, Vol. 63, Issue 2
U.S. Program on Materials Technology for Ultra-Supercritical Coal Power Plants
journal, June 2005
- Viswanathan, R.; Henry, J. F.; Tanzosh, J.
- Journal of Materials Engineering and Performance, Vol. 14, Issue 3
Creep behavior of a β′(NiAl) precipitation strengthened ferritic Fe–Cr–Ni–Al alloy
journal, May 1998
- Zhu, S. M.; Tjong, S. C.; Lai, J. K. L.
- Acta Materialia, Vol. 46, Issue 9
On the contribution of carbides and micrograin boundaries to the creep strength of tempered martensite ferritic steels
journal, January 2007
- Kostka, A.; Tak, K.; Hellmig, R.
- Acta Materialia, Vol. 55, Issue 2
Increasing the creep resistance of Fe-Ni-Al-Cr superalloys via Ti additions by optimizing the B2/L21 ratio in composite nano-precipitates
journal, September 2018
- Baik, Sung-Il; Wang, Shao-Yu; Liaw, Peter K.
- Acta Materialia, Vol. 157
Microstructural evolution of single Ni2TiAl or hierarchical NiAl/Ni2TiAl precipitates in Fe-Ni-Al-Cr-Ti ferritic alloys during thermal treatment for elevated-temperature applications
journal, April 2017
- Song, Gian; Sun, Zhiqian; Poplawsky, Jonathan D.
- Acta Materialia, Vol. 127
On the modulated structure of aged Ni-Al alloys
journal, October 1966
- Ardell, A. J.; Nicholson, R. B.
- Acta Metallurgica, Vol. 14, Issue 10
Microstructural stability and creep rupture strength of the martensitic steel P92 for advanced power plant
journal, December 1997
- Ennis, P. J.; Zielinska-Lipiec, A.; Wachter, O.
- Acta Materialia, Vol. 45, Issue 12
Modeling the creep threshold stress due to climb of a dislocation in the stress field of a misfitting precipitate
journal, August 2011
- Krug, Matthew E.; Dunand, David C.
- Acta Materialia, Vol. 59, Issue 13
The dynamics of precipitate evolution in elastically stressed solids—II. Particle alignment
journal, May 1996
- Su, C. H.; Voorhees, P. W.
- Acta Materialia, Vol. 44, Issue 5
Characterization of nanoscale NiAl-type precipitates in a ferritic steel by electron microscopy and atom probe tomography
journal, July 2010
- Teng, Z. K.; Miller, M. K.; Ghosh, G.
- Scripta Materialia, Vol. 63, Issue 1
New NiAl-strengthened ferritic steels with balanced creep resistance and ductility designed by coupling thermodynamic calculations with focused experiments
journal, October 2012
- Teng, Z. K.; Zhang, F.; Miller, M. K.
- Intermetallics, Vol. 29
The strengthening effect of (Ni,Fe)Al precipitates on the mechanical properties at high temperatures of ferritic Fe–Al–Ni–Cr alloys
journal, December 2005
- Stallybrass, C.; Schneider, A.; Sauthoff, G.
- Intermetallics, Vol. 13, Issue 12
Atom probe tomography study of Fe-Ni-Al-Cr-Ti ferritic steels with hierarchically-structured precipitates
journal, February 2018
- Baik, Sung-Il; Rawlings, Michael J. S.; Dunand, David C.
- Acta Materialia, Vol. 144
Ferritic Alloys with Extreme Creep Resistance via Coherent Hierarchical Precipitates
journal, November 2015
- Song, Gian; Sun, Zhiqian; Li, Lin
- Scientific Reports, Vol. 5, Issue 1
NIH Image to ImageJ: 25 years of image analysis
journal, June 2012
- Schneider, Caroline A.; Rasband, Wayne S.; Eliceiri, Kevin W.
- Nature Methods, Vol. 9, Issue 7
New design aspects of creep-resistant NiAl-strengthened ferritic alloys
journal, March 2013
- Sun, Z.; Liebscher, C. H.; Huang, S.
- Scripta Materialia, Vol. 68, Issue 6
On the formation of hierarchically structured L2 1 -Ni2TiAl type precipitates in a ferritic alloy
journal, November 2012
- Liebscher, C. H.; Radmilovic, V.; Dahmen, U.
- Journal of Materials Science, Vol. 48, Issue 5
The role of elastic energy in the morphological development of a NiTiAl alloy
journal, January 1988
- Bendersky, L. A.; Voorhees, P. W.; Boettinger, W. J.
- Scripta Metallurgica, Vol. 22, Issue 7