Study of dendrite growth with natural convection in superalloy directional solidification via a multiphase-field-lattice Boltzmann model
Journal Article
·
· Computational Materials Science
Not Available
- Sponsoring Organization:
- USDOE Office of Electricity (OE), Advanced Grid Research & Development. Power Systems Engineering Research
- OSTI ID:
- 1636589
- Journal Information:
- Computational Materials Science, Journal Name: Computational Materials Science Journal Issue: C Vol. 158; ISSN 0927-0256
- Publisher:
- ElsevierCopyright Statement
- Country of Publication:
- Netherlands
- Language:
- English
Similar Records
A Phase-Field Lattice-Boltzmann Study on Dendritic Growth of Al-Cu Alloy Under Convection
Equiaxed dendritic solidification with convection. Part 1: Multiscale/multiphase modeling
A multiphase solute diffusion model for dendritic alloy solidification
Journal Article
·
2018
· Metallurgical and Materials Transactions. B, Process Metallurgy and Materials Processing Science
·
OSTI ID:22931894
+2 more
Equiaxed dendritic solidification with convection. Part 1: Multiscale/multiphase modeling
Journal Article
·
1996
· Metallurgical and Materials Transactions. A, Physical Metallurgy and Materials Science
·
OSTI ID:382525
A multiphase solute diffusion model for dendritic alloy solidification
Journal Article
·
1993
· Metallurgical Transactions, A
·