Title: Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization

Abstract

Improvements in energy-water systems will necessitate fabrication of high-performance separation membranes. To this end, interface engineering is a powerful tool for tailoring properties, and atomic layer deposition (ALD) has recently emerged as a promising and versatile approach. However, most non-polar polymeric membranes are not amenable to ALD processing due to the absence of nucleation sites. Here, a sensitization strategy for ALD-coating is presented, illustrated by membrane interface hydrophilization. Facile dip-coating with polyphenols effectively sensitizes hydrophobic polymer membranes to TiO2 ALD coating. Tannic acid-sensitized ALD-coated membranes exhibit outstanding underwater crude oil repulsion and rigorous mechanical stability through bending and rinsing tests. As a result, these membranes demonstrate outstanding crude oil-in-water separation and reusability compared to untreated membranes or those treated with ALD without polyphenol pretreatment. A possible polyphenol-sensitized ALD mechanism is proposed involving initial island nucleation followed by film intergrowth. This polyphenol sensitization strategy enriches the functionalization toolbox in material science, interface engineering, and environmental science.

Authors:
 [1];  [2];  [3];  [4];  [4];  [3];  [3];  [5]; ORCiD logo [4]
  1. Argonne National Lab. (ANL), Lemont, IL (United States); Univ. of Chicago, IL (United States); Harbin Inst. of Technology (China)
  2. Univ. of Chicago, IL (United States)
  3. Argonne National Lab. (ANL), Lemont, IL (United States)
  4. Argonne National Lab. (ANL), Lemont, IL (United States); Univ. of Chicago, IL (United States)
  5. Harbin Inst. of Technology (China)
Publication Date:
Research Org.:
Energy Frontier Research Centers (EFRC) (United States). Advanced Materials for Energy-Water Systems (AMEWS); Argonne National Lab. (ANL), Argonne, IL (United States)
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES)
OSTI Identifier:
1633727
Alternate Identifier(s):
OSTI ID: 1599926
Grant/Contract Number:  
AC02-06CH11357
Resource Type:
Accepted Manuscript
Journal Name:
Advanced Functional Materials
Additional Journal Information:
Journal Volume: 30; Journal Issue: 15; Journal ID: ISSN 1616-301X
Publisher:
Wiley
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; atomic layer deposition; interface engineering; membrane interface hydrophilization; membrane separation; polyphenols; polyphenol; hydrophilization

Citation Formats

Yang, Xiaobin, Sun, Pan, Zhang, Huiru, Xia, Zijing, Waldman, Ruben Z., Mane, Anil U., Elam, Jeffrey W., Shao, Lu, and Darling, Seth B. Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization. United States: N. p., 2020. Web. doi:10.1002/adfm.201910062.
Yang, Xiaobin, Sun, Pan, Zhang, Huiru, Xia, Zijing, Waldman, Ruben Z., Mane, Anil U., Elam, Jeffrey W., Shao, Lu, & Darling, Seth B. Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization. United States. https://doi.org/10.1002/adfm.201910062
Yang, Xiaobin, Sun, Pan, Zhang, Huiru, Xia, Zijing, Waldman, Ruben Z., Mane, Anil U., Elam, Jeffrey W., Shao, Lu, and Darling, Seth B. Sun . "Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization". United States. https://doi.org/10.1002/adfm.201910062. https://www.osti.gov/servlets/purl/1633727.
@article{osti_1633727,
title = {Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization},
author = {Yang, Xiaobin and Sun, Pan and Zhang, Huiru and Xia, Zijing and Waldman, Ruben Z. and Mane, Anil U. and Elam, Jeffrey W. and Shao, Lu and Darling, Seth B.},
abstractNote = {Improvements in energy-water systems will necessitate fabrication of high-performance separation membranes. To this end, interface engineering is a powerful tool for tailoring properties, and atomic layer deposition (ALD) has recently emerged as a promising and versatile approach. However, most non-polar polymeric membranes are not amenable to ALD processing due to the absence of nucleation sites. Here, a sensitization strategy for ALD-coating is presented, illustrated by membrane interface hydrophilization. Facile dip-coating with polyphenols effectively sensitizes hydrophobic polymer membranes to TiO2 ALD coating. Tannic acid-sensitized ALD-coated membranes exhibit outstanding underwater crude oil repulsion and rigorous mechanical stability through bending and rinsing tests. As a result, these membranes demonstrate outstanding crude oil-in-water separation and reusability compared to untreated membranes or those treated with ALD without polyphenol pretreatment. A possible polyphenol-sensitized ALD mechanism is proposed involving initial island nucleation followed by film intergrowth. This polyphenol sensitization strategy enriches the functionalization toolbox in material science, interface engineering, and environmental science.},
doi = {10.1002/adfm.201910062},
journal = {Advanced Functional Materials},
number = 15,
volume = 30,
place = {United States},
year = {2020},
month = {2}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record

Citation Metrics:
Cited by: 1 work
Citation information provided by
Web of Science

Save / Share:

Works referenced in this record:

Effect of water dose on the atomic layer deposition rate of oxide thin films
journal, June 2000


Bioadhesion-inspired surface engineering constructing robust, hydrophilic membranes for highly-efficient wastewater remediation
journal, December 2019


Robust Underwater Oil-Repellent Material Inspired by Columnar Nacre
journal, August 2016


Atomic Layer Deposition for Membranes: Basics, Challenges, and Opportunities
journal, October 2018


GROMACS 4:  Algorithms for Highly Efficient, Load-Balanced, and Scalable Molecular Simulation
journal, February 2008

  • Hess, Berk; Kutzner, Carsten; van der Spoel, David
  • Journal of Chemical Theory and Computation, Vol. 4, Issue 3
  • DOI: 10.1021/ct700301q

Mussel-Inspired Surface Engineering for Water-Remediation Materials
journal, July 2019


Mitigating oil spills in the water column
journal, January 2018

  • Barry, Edward; Libera, Joseph A.; Mane, Anil U.
  • Environmental Science: Water Research & Technology, Vol. 4, Issue 1
  • DOI: 10.1039/C7EW00265C

Hygro-responsive membranes for effective oil–water separation
journal, January 2012

  • Kota, Arun K.; Kwon, Gibum; Choi, Wonjae
  • Nature Communications, Vol. 3, Issue 1
  • DOI: 10.1038/ncomms2027

Plant‐Inspired Pyrogallol‐Containing Functional Materials
journal, August 2019

  • Shin, Mikyung; Park, Eunsook; Lee, Haeshin
  • Advanced Functional Materials, Vol. 29, Issue 43
  • DOI: 10.1002/adfm.201903022

A Robust Polyionized Hydrogel with an Unprecedented Underwater Anti-Crude-Oil-Adhesion Property
journal, May 2016


Wettability of porous surfaces
journal, January 1944

  • Cassie, A. B. D.; Baxter, S.
  • Transactions of the Faraday Society, Vol. 40, p. 546-551
  • DOI: 10.1039/tf9444000546

Characterization of low temperature deposited atomic layer deposition TiO 2 for MEMS applications
journal, January 2013

  • Huang, Yujian; Pandraud, Gregory; Sarro, Pasqualina M.
  • Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Vol. 31, Issue 1
  • DOI: 10.1116/1.4772664

Crude-Oil-Repellent Membranes by Atomic Layer Deposition: Oxide Interface Engineering
journal, August 2018


One-Step Assembly of Coordination Complexes for Versatile Film and Particle Engineering
journal, July 2013


Perspective: Interfacial materials at the interface of energy and water
journal, July 2018

  • Darling, Seth B.
  • Journal of Applied Physics, Vol. 124, Issue 3
  • DOI: 10.1063/1.5040110

Constant pressure molecular dynamics simulation: The Langevin piston method
journal, September 1995

  • Feller, Scott E.; Zhang, Yuhong; Pastor, Richard W.
  • The Journal of Chemical Physics, Vol. 103, Issue 11
  • DOI: 10.1063/1.470648

Rapid parameterization of small molecules using the force field toolkit
journal, September 2013

  • Mayne, Christopher G.; Saam, Jan; Schulten, Klaus
  • Journal of Computational Chemistry, Vol. 34, Issue 32
  • DOI: 10.1002/jcc.23422

Antifouling membranes for sustainable water purification: strategies and mechanisms
journal, January 2016

  • Zhang, Runnan; Liu, Yanan; He, Mingrui
  • Chemical Society Reviews, Vol. 45, Issue 21
  • DOI: 10.1039/C5CS00579E

Conformal Coating on Ultrahigh-Aspect-Ratio Nanopores of Anodic Alumina by Atomic Layer Deposition
journal, September 2003

  • Elam, J. W.; Routkevitch, D.; Mardilovich, P. P.
  • Chemistry of Materials, Vol. 15, Issue 18, p. 3507-3517
  • DOI: 10.1021/cm0303080

A Novel Superhydrophilic and Underwater Superoleophobic Hydrogel-Coated Mesh for Oil/Water Separation
journal, August 2011


Mussel-Inspired Surface Chemistry for Multifunctional Coatings
journal, October 2007


An Intelligent Superwetting PVDF Membrane Showing Switchable Transport Performance for Oil/Water Separation
journal, February 2014


Progress in the production and modification of PVDF membranes
journal, June 2011


Templating Sub-10 nm Atomic Layer Deposited Oxide Nanostructures on Graphene via One-Dimensional Organic Self-Assembled Monolayers
journal, March 2013

  • Alaboson, Justice M. P.; Sham, Chun-Hong; Kewalramani, Sumit
  • Nano Letters, Vol. 13, Issue 12
  • DOI: 10.1021/nl4000932

Zwitterionic Nanohydrogel Grafted PVDF Membranes with Comprehensive Antifouling Property and Superior Cycle Stability for Oil-in-Water Emulsion Separation
journal, August 2018

  • Zhu, Yuzhang; Wang, Jinliang; Zhang, Feng
  • Advanced Functional Materials, Vol. 28, Issue 40
  • DOI: 10.1002/adfm.201804121

Ion sieving in graphene oxide membranes via cationic control of interlayer spacing
journal, October 2017


Resistance Of Solid Surfaces To Wetting By Water
journal, August 1936

  • Wenzel, Robert N.
  • Industrial & Engineering Chemistry, Vol. 28, Issue 8, p. 988-994
  • DOI: 10.1021/ie50320a024

Surface and interface engineering for organic–inorganic composite membranes
journal, January 2016

  • Yang, Hao-Cheng; Hou, Jingwei; Chen, Vicki
  • Journal of Materials Chemistry A, Vol. 4, Issue 25
  • DOI: 10.1039/C6TA02844F

Development of the Colle-Salvetti correlation-energy formula into a functional of the electron density
journal, January 1988


Janus Membranes via Diffusion-Controlled Atomic Layer Deposition
journal, June 2018

  • Waldman, Ruben Z.; Yang, Hao-Cheng; Mandia, David J.
  • Advanced Materials Interfaces, Vol. 5, Issue 15
  • DOI: 10.1002/admi.201800658

Particle mesh Ewald: An N ⋅log( N ) method for Ewald sums in large systems
journal, June 1993

  • Darden, Tom; York, Darrin; Pedersen, Lee
  • The Journal of Chemical Physics, Vol. 98, Issue 12
  • DOI: 10.1063/1.464397

Advanced oil sorbents using sequential infiltration synthesis
journal, January 2017

  • Barry, Edward; Mane, Anil U.; Libera, Joseph A.
  • Journal of Materials Chemistry A, Vol. 5, Issue 6
  • DOI: 10.1039/C6TA09014A

Maximizing the right stuff: The trade-off between membrane permeability and selectivity
journal, June 2017


Atomic layer deposition for membrane interface engineering
journal, January 2018

  • Yang, Hao-Cheng; Waldman, Ruben Z.; Chen, Zhaowei
  • Nanoscale, Vol. 10, Issue 44
  • DOI: 10.1039/C8NR08114J

Atomic Layer Deposition of Nanostructured Materials for Energy and Environmental Applications
journal, January 2012

  • Marichy, Catherine; Bechelany, Mikhael; Pinna, Nicola
  • Advanced Materials, Vol. 24, Issue 8, p. 1017-1032
  • DOI: 10.1002/adma.201104129

Surface Modification of Water Purification Membranes
journal, March 2017

  • Miller, Daniel J.; Dreyer, Daniel R.; Bielawski, Christopher W.
  • Angewandte Chemie International Edition, Vol. 56, Issue 17
  • DOI: 10.1002/anie.201601509

Universal polymer coatings and their representative biomedical applications
journal, January 2015


Clam's Shell Inspired High-Energy Inorganic Coatings with Underwater Low Adhesive Superoleophobicity
journal, May 2012


Biomimetic hydrophilization engineering on membrane surface for highly-efficient water purification
journal, November 2019


Review Article: Recommended reading list of early publications on atomic layer deposition—Outcome of the “Virtual Project on the History of ALD”
journal, January 2017

  • Ahvenniemi, Esko; Akbashev, Andrew R.; Ali, Saima
  • Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Vol. 35, Issue 1
  • DOI: 10.1116/1.4971389

PVDF membranes with simultaneously enhanced permeability and selectivity by breaking the tradeoff effect via atomic layer deposition of TiO2
journal, September 2013


Colorless Multifunctional Coatings Inspired by Polyphenols Found in Tea, Chocolate, and Wine
journal, August 2013

  • Sileika, Tadas S.; Barrett, Devin G.; Zhang, Ran
  • Angewandte Chemie International Edition, Vol. 52, Issue 41
  • DOI: 10.1002/anie.201304922

OPLS all-atom force field for carbohydrates
journal, December 1997


Dopamine: Just the Right Medicine for Membranes
journal, January 2018

  • Yang, Hao-Cheng; Waldman, Ruben Z.; Wu, Ming-Bang
  • Advanced Functional Materials, Vol. 28, Issue 8
  • DOI: 10.1002/adfm.201705327

Atomic Layer Deposition and Abrupt Wetting Transitions on Nonwoven Polypropylene and Woven Cotton Fabrics
journal, February 2010

  • Hyde, G. Kevin; Scarel, Giovanna; Spagnola, Joseph C.
  • Langmuir, Vol. 26, Issue 4
  • DOI: 10.1021/la902830d

Materials for next-generation desalination and water purification membranes
journal, April 2016

  • Werber, Jay R.; Osuji, Chinedum O.; Elimelech, Menachem
  • Nature Reviews Materials, Vol. 1, Issue 5
  • DOI: 10.1038/natrevmats.2016.18