skip to main content
DOE PAGES title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Reforming of methane with carbon dioxide over cerium oxide promoted nickel nanoparticles deposited on 4-channel hollow fibers by atomic layer deposition

Abstract

CeO 2 can significantly enhance the catalytic performance of Ni/Al 2 O 3 catalysts prepared by atomic layer deposition for dry reforming of methane.

Authors:
ORCiD logo [1];  [1]; ORCiD logo [2];  [3];  [4]; ORCiD logo [1]
  1. Department of Chemical and Biochemical Engineering, Missouri University of Science and Technology, Rolla, USA
  2. Gas Technology Institute, Des Plaines, USA
  3. TEM Laboratory, University of New Mexico, Albuquerque, USA
  4. State Key Laboratory of Materials-Oriented Chemical Engineering, College of Chemistry and Chemical Engineering, Nanjing Tech University, Nanjing 210009, P.R. China
Publication Date:
Sponsoring Org.:
USDOE
OSTI Identifier:
1606460
Grant/Contract Number:  
FE0029760
Resource Type:
Publisher's Accepted Manuscript
Journal Name:
Catalysis Science and Technology
Additional Journal Information:
Journal Name: Catalysis Science and Technology Journal Volume: 10 Journal Issue: 10; Journal ID: ISSN 2044-4753
Publisher:
Royal Society of Chemistry (RSC)
Country of Publication:
United Kingdom
Language:
English

Citation Formats

Jin, Baitang, Shang, Zeyu, Li, Shiguang, Jiang, Ying-Bing, Gu, Xuehong, and Liang, Xinhua. Reforming of methane with carbon dioxide over cerium oxide promoted nickel nanoparticles deposited on 4-channel hollow fibers by atomic layer deposition. United Kingdom: N. p., 2020. Web. doi:10.1039/D0CY00039F.
Jin, Baitang, Shang, Zeyu, Li, Shiguang, Jiang, Ying-Bing, Gu, Xuehong, & Liang, Xinhua. Reforming of methane with carbon dioxide over cerium oxide promoted nickel nanoparticles deposited on 4-channel hollow fibers by atomic layer deposition. United Kingdom. doi:https://doi.org/10.1039/D0CY00039F
Jin, Baitang, Shang, Zeyu, Li, Shiguang, Jiang, Ying-Bing, Gu, Xuehong, and Liang, Xinhua. Tue . "Reforming of methane with carbon dioxide over cerium oxide promoted nickel nanoparticles deposited on 4-channel hollow fibers by atomic layer deposition". United Kingdom. doi:https://doi.org/10.1039/D0CY00039F.
@article{osti_1606460,
title = {Reforming of methane with carbon dioxide over cerium oxide promoted nickel nanoparticles deposited on 4-channel hollow fibers by atomic layer deposition},
author = {Jin, Baitang and Shang, Zeyu and Li, Shiguang and Jiang, Ying-Bing and Gu, Xuehong and Liang, Xinhua},
abstractNote = {CeO 2 can significantly enhance the catalytic performance of Ni/Al 2 O 3 catalysts prepared by atomic layer deposition for dry reforming of methane.},
doi = {10.1039/D0CY00039F},
journal = {Catalysis Science and Technology},
number = 10,
volume = 10,
place = {United Kingdom},
year = {2020},
month = {5}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record
DOI: https://doi.org/10.1039/D0CY00039F

Save / Share:

Works referenced in this record:

Characterization of Carbonaceous Species Formed during Reforming of CH4with CO2over Ni/CaO–Al2O3Catalysts Studied by Various Transient Techniques
journal, July 1996

  • Goula, M. A.; Lemonidou, A. A.; Efstathiou, A. M.
  • Journal of Catalysis, Vol. 161, Issue 2
  • DOI: 10.1006/jcat.1996.0225

The effect of synthesis gas composition on the Fischer–Tropsch synthesis over Co/γ-Al2O3 and Co–Re/γ-Al2O3 catalysts
journal, July 2007


Transient studies of carbon dioxide reforming of methane over Pt/ZrO2 and Pt/Al2O3
journal, June 2006


Effects of CeO2 addition on Ni/Al2O3 catalysts for the reaction of ammonia decomposition to hydrogen
journal, April 2008


Production of synthesis gas via methane reforming with CO22 on noble metals and small amount of noble-(Rh-) promoted Ni catalysts
journal, April 2006


Temperature-dependent anti-coking behaviors of highly stable Ni-CaO-ZrO 2 nanocomposite catalysts for CO 2 reforming of methane
journal, July 2017


Methane reforming with CO2 to syngas over CeO2-promoted Ni/Al2O3-ZrO2 catalysts prepared via a direct sol-gel process
journal, January 2011


Insight into the effects of the oxygen species over Ni/ZrO2 catalyst surface on methane reforming with carbon dioxide
journal, May 2019


The promoting effect of La, Mg, Co and Zn on the activity and stability of Ni/SiO2 catalyst for CO2 reforming of methane
journal, June 2011


Highly active and stable alumina supported nickel nanoparticle catalysts for dry reforming of methane
journal, February 2017


Kinetic and Stability Studies of Ru/La2O3 Used in the Dry Reforming of Methane
journal, October 2008


Dry Reforming of Shale Gas and Carbon Dioxide with Ni-Ce-Al 2 O 3 Catalyst: Syngas Production Enhanced over Ni-CeO x Formation
journal, September 2018


Genesis and Evolution of Surface Species during Pt Atomic Layer Deposition on Oxide Supports Characterized by in Situ XAFS Analysis and Water−Gas Shift Reaction
journal, May 2010

  • Setthapun, Worajit; Williams, W. Damion; Kim, Seung Min
  • The Journal of Physical Chemistry C, Vol. 114, Issue 21
  • DOI: 10.1021/jp911178m

Ni/CeO2 catalysts for methane partial oxidation: Synthesis driven structural and catalytic effects
journal, July 2016


Characterization of Ni/SiO2 and Ni/Li-SiO2 catalysts for methane dry reforming
journal, October 2005


Structure and surface properties of ceria-modified Ni-based catalysts for hydrogen production
journal, June 2018


Comparison of Nanoscaled and Bulk NiO Structural and Environmental Characteristics by XRD, XAFS, and XPS
journal, November 2012

  • Peck, Matthea A.; Langell, Marjorie A.
  • Chemistry of Materials, Vol. 24, Issue 23
  • DOI: 10.1021/cm300739y

The role of carbonaceous deposits in the activity and stability of Ni-based catalysts applied in the dry reforming of methane
journal, January 2014

  • Düdder, Hendrik; Kähler, Kevin; Krause, Bastian
  • Catal. Sci. Technol., Vol. 4, Issue 9
  • DOI: 10.1039/C4CY00409D

The deactivation of Co/SiO2 catalyst for Fischer–Tropsch synthesis at different ratios of H2 to CO
journal, July 2006


La-promoted Ni-hydrotalcite-derived catalysts for dry reforming of methane at low temperatures
journal, October 2016


High carbon-resistance Ni/CeAlO3-Al2O3 catalyst for CH4/CO2 reforming
journal, June 2013


Structural characterisation of Ni/alumina reforming catalysts activated at high temperatures
journal, September 2013


Carbon dioxide reforming of methane to synthesis gas over supported rhodium catalysts: the effect of support
journal, November 2000


Synthesis of supported Ni catalysts by atomic layer deposition
journal, July 2013


Effects of modifying Ni/Al2O3 catalyst with cobalt on the reforming of CH4 with CO2 and cracking of CH4 reactions
journal, July 2014


Ni nanocluster on modified CeO 2 –ZrO 2 nanoporous composite for tri-reforming of methane
journal, January 2016

  • Singha, Rajib Kumar; Das, Subhasis; Pandey, Monica
  • Catalysis Science & Technology, Vol. 6, Issue 19
  • DOI: 10.1039/C5CY01323B

Structural Characterization of Highly Stable Ni/SBA-15 Catalyst and Its Catalytic Performance for Methane Reforming with CO2
journal, September 2006


A novel catalyst with plate-type anodic alumina supports, Ni/NiAl2O4/γ-Al2O3/alloy, for steam reforming of methane
journal, September 2008


High Carbon-Resistance Ni@CeO2 Core–Shell Catalysts for Dry Reforming of Methane
journal, November 2017


Methane Reforming with Carbon Dioxide. The Behavior of Pd/α-Al 2 O 3 and Pd−CeO x /α-Al 2 O 3 Catalysts
journal, November 2005

  • Schulz, Pablo G.; Gonzalez, María G.; Quincoces, Claudia E.
  • Industrial & Engineering Chemistry Research, Vol. 44, Issue 24
  • DOI: 10.1021/ie050517p

Catalytic activity and effect of modifiers on Ni-based catalysts for the dry reforming of methane
journal, June 2010

  • Barroso-Quiroga, María Martha; Castro-Luna, Adolfo Eduardo
  • International Journal of Hydrogen Energy, Vol. 35, Issue 11
  • DOI: 10.1016/j.ijhydene.2009.12.073

Comparison of reducibility and stability of alumina-supported Ni catalysts prepared by impregnation and co-precipitation
journal, February 2006


Effect of CeO2 addition on Ni/Al2O3 catalysts for methanation of carbon dioxide with hydrogen
journal, November 2012


Remarkable activity and stability of Ni catalyst supported on CeO2-Al2O3 via CeAlO3 perovskite towards glycerol steam reforming for hydrogen production
journal, December 2017

  • Kamonsuangkasem, Krongthong; Therdthianwong, Supaporn; Therdthianwong, Apichai
  • Applied Catalysis B: Environmental, Vol. 218
  • DOI: 10.1016/j.apcatb.2017.06.073

Surface reactions during atomic layer deposition of Pt derived from gas phase infrared spectroscopy
journal, July 2009

  • Kessels, W. M. M.; Knoops, H. C. M.; Dielissen, S. A. F.
  • Applied Physics Letters, Vol. 95, Issue 1
  • DOI: 10.1063/1.3176946

Catalytic partial oxidation of methane to syngas over Ca-decorated-Al2O3-supported Ni and NiB catalysts
journal, September 2005


Effect of NiAl 2 O 4 Formation on Ni/Al 2 O 3 Stability during Dry Reforming of Methane
journal, July 2015


Preparation and characterization of α-Al2O3 hollow fiber membranes with four-channel configuration
journal, January 2015


Surface characterization of alumina-supported ceria
journal, August 1988

  • Shyu, J. Z.; Weber, W. H.; Gandhi, H. S.
  • The Journal of Physical Chemistry, Vol. 92, Issue 17
  • DOI: 10.1021/j100328a029

Synthesis gas production from dry reforming of methane over CeO2 doped Ni/Al2O3: Influence of the doping ceria on the resistance toward carbon formation
journal, September 2005

  • Laosiripojana, N.; Sutthisripok, W.; Assabumrungrat, S.
  • Chemical Engineering Journal, Vol. 112, Issue 1-3
  • DOI: 10.1016/j.cej.2005.06.003

The catalytic methanation of coke oven gas over Ni-Ce/Al2O3 catalysts prepared by microwave heating: Effect of amorphous NiO formation
journal, March 2015


Nano-engineered nickel catalysts supported on 4-channel α-Al 2 O 3 hollow fibers for dry reforming of methane
journal, March 2018

  • Shang, Zeyu; Li, Shiguang; Wang, Qingfa
  • AIChE Journal, Vol. 64, Issue 7
  • DOI: 10.1002/aic.16160

The effect of CeO2 on the surface and catalytic properties of Pt/CeO2–ZrO2 catalysts for methane dry reforming
journal, July 2009


Investigation of mesoporous NiAl 2 O 4 /MO x (M = La, Ce, Ca, Mg)–γ-Al 2 O 3 nanocomposites for dry reforming of methane
journal, January 2017

  • Zhang, Li; Wang, Xueguang; Chen, Chenju
  • RSC Advances, Vol. 7, Issue 53
  • DOI: 10.1039/C7RA04497F

Ni-alumina dry reforming catalysts: Atomic layer deposition and the issue of Ni aluminate
journal, March 2020


Characterizations and activities of the nano-sized Ni/Al2O3 and Ni/La–Al2O3 catalysts for NH3 decomposition
journal, August 2005


Synthesis gas production from dry reforming of methane over Ni/Al2O3 stabilized by ZrO2
journal, February 2008


Characterization of ceria-coated alumina carrier
journal, August 2002