skip to main content
DOE PAGES title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Mechanisms of alumina growth via atomic layer deposition on nickel oxide and metallic nickel surfaces

Abstract

Decomposition of tri-methyl aluminum on catalyst surfaces leads to various products that are precursors of an alumina coating.

Authors:
 [1];  [1]; ORCiD logo [1]
  1. Department of Chemical Engineering, Texas A&M University, College Station, USA
Publication Date:
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES)
OSTI Identifier:
1572421
Grant/Contract Number:  
SC00193979
Resource Type:
Publisher's Accepted Manuscript
Journal Name:
Physical Chemistry Chemical Physics. PCCP (Print)
Additional Journal Information:
Journal Name: Physical Chemistry Chemical Physics. PCCP (Print) Journal Volume: 21 Journal Issue: 44; Journal ID: ISSN 1463-9076
Publisher:
Royal Society of Chemistry (RSC)
Country of Publication:
United Kingdom
Language:
English

Citation Formats

Ospina-Acevedo, Francisco Alejandro, Perez Beltran, Saul, and Balbuena, Perla B. Mechanisms of alumina growth via atomic layer deposition on nickel oxide and metallic nickel surfaces. United Kingdom: N. p., 2019. Web. doi:10.1039/C9CP05688B.
Ospina-Acevedo, Francisco Alejandro, Perez Beltran, Saul, & Balbuena, Perla B. Mechanisms of alumina growth via atomic layer deposition on nickel oxide and metallic nickel surfaces. United Kingdom. doi:10.1039/C9CP05688B.
Ospina-Acevedo, Francisco Alejandro, Perez Beltran, Saul, and Balbuena, Perla B. Wed . "Mechanisms of alumina growth via atomic layer deposition on nickel oxide and metallic nickel surfaces". United Kingdom. doi:10.1039/C9CP05688B.
@article{osti_1572421,
title = {Mechanisms of alumina growth via atomic layer deposition on nickel oxide and metallic nickel surfaces},
author = {Ospina-Acevedo, Francisco Alejandro and Perez Beltran, Saul and Balbuena, Perla B.},
abstractNote = {Decomposition of tri-methyl aluminum on catalyst surfaces leads to various products that are precursors of an alumina coating.},
doi = {10.1039/C9CP05688B},
journal = {Physical Chemistry Chemical Physics. PCCP (Print)},
number = 44,
volume = 21,
place = {United Kingdom},
year = {2019},
month = {11}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record
DOI: 10.1039/C9CP05688B

Save / Share:

Works referenced in this record:

CO 2 Reforming of CH 4 on Ni(111):  A Density Functional Theory Calculation
journal, May 2006

  • Wang, Sheng-Guang; Cao, Dong-Bo; Li, Yong-Wang
  • The Journal of Physical Chemistry B, Vol. 110, Issue 20
  • DOI: 10.1021/jp060992g

Generalized Gradient Approximation Made Simple
journal, October 1996

  • Perdew, John P.; Burke, Kieron; Ernzerhof, Matthias
  • Physical Review Letters, Vol. 77, Issue 18, p. 3865-3868
  • DOI: 10.1103/PhysRevLett.77.3865

LDA+U calculated electronic and structural properties of NiO(001) and NiO(111) p(2×2) surfaces
journal, May 2002


Porous Alumina Protective Coatings on Palladium Nanoparticles by Self-Poisoned Atomic Layer Deposition
journal, May 2012

  • Lu, Junling; Liu, Bin; Greeley, Jeffrey P.
  • Chemistry of Materials, Vol. 24, Issue 11
  • DOI: 10.1021/cm300203s

Alumina coated nickel nanoparticles as a highly active catalyst for dry reforming of methane
journal, December 2015


Stabilization of Copper Catalysts for Liquid-Phase Reactions by Atomic Layer Deposition
journal, November 2013

  • O'Neill, Brandon J.; Jackson, David H. K.; Crisci, Anthony J.
  • Angewandte Chemie International Edition, Vol. 52, Issue 51
  • DOI: 10.1002/anie.201308245

First-Principles Predictions and in Situ Experimental Validation of Alumina Atomic Layer Deposition on Metal Surfaces
journal, November 2014

  • Lu, Junling; Liu, Bin; Guisinger, Nathan P.
  • Chemistry of Materials, Vol. 26, Issue 23
  • DOI: 10.1021/cm503178j

Projector augmented-wave method
journal, December 1994


Carbon Dioxide Reforming of Methane To Produce Synthesis Gas over Metal-Supported Catalysts:  State of the Art
journal, January 1996

  • Wang, Shaobin; Lu, G. Q. (Max); Millar, Graeme J.
  • Energy & Fuels, Vol. 10, Issue 4
  • DOI: 10.1021/ef950227t

Dry reforming of methane over nickel catalysts supported on magnesium aluminate spinels
journal, October 2004


Dry reforming of methane: Influence of process parameters—A review
journal, May 2015

  • Usman, Muhammad; Wan Daud, W. M. A.; Abbas, Hazzim F.
  • Renewable and Sustainable Energy Reviews, Vol. 45
  • DOI: 10.1016/j.rser.2015.02.026

Structural investigation of the NiO(111) single crystal surface
journal, December 1997


Implementation of the projector augmented-wave LDA+U method: Application to the electronic structure of NiO
journal, December 2000


Atomic Layer Deposition of Ta–N-Based Thin Films Using a Tantalum Source
journal, January 2010

  • Schmidt, D.; Knaut, M.; Hossbach, C.
  • Journal of The Electrochemical Society, Vol. 157, Issue 6
  • DOI: 10.1149/1.3353230

Atomic layer deposition—Sequential self-limiting surface reactions for advanced catalyst “bottom-up” synthesis
journal, June 2016


Special points for Brillouin-zone integrations
journal, June 1976

  • Monkhorst, Hendrik J.; Pack, James D.
  • Physical Review B, Vol. 13, Issue 12, p. 5188-5192
  • DOI: 10.1103/PhysRevB.13.5188

Molecular adsorption on the surface of strongly correlated transition-metal oxides: A case study for CO/NiO(100)
journal, February 2004


Reconstruction of NaCl surfaces from a dipolar solution to the Madelung problem
journal, June 1992


Toward atomically-precise synthesis of supported bimetallic nanoparticles using atomic layer deposition
journal, February 2014

  • Lu, Junling; Low, Ke-Bin; Lei, Yu
  • Nature Communications, Vol. 5, Issue 1
  • DOI: 10.1038/ncomms4264

Molecular dynamics simulations of reconstructed NiO surfaces
journal, April 2004


Coking- and Sintering-Resistant Palladium Catalysts Achieved Through Atomic Layer Deposition
journal, March 2012


Band theory and Mott insulators: Hubbard U instead of Stoner I
journal, July 1991

  • Anisimov, Vladimir I.; Zaanen, Jan; Andersen, Ole K.
  • Physical Review B, Vol. 44, Issue 3, p. 943-954
  • DOI: 10.1103/PhysRevB.44.943

A fast and robust algorithm for Bader decomposition of charge density
journal, June 2006


Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process
journal, June 2005

  • Puurunen, Riikka L.
  • Journal of Applied Physics, Vol. 97, Issue 12, Article No. 121301
  • DOI: 10.1063/1.1940727

Atomic layer deposition (ALD): from precursors to thin film structures
journal, April 2002


Trimethylaluminum as a Reducing Agent in the Atomic Layer Deposition of Ti(Al)N Thin Films
journal, September 2001


Atomic Layer Deposition of Ta(Al)N(C) Thin Films Using Trimethylaluminum as a Reducing Agent
journal, January 2001

  • Alén, Petra; Juppo, Marika; Ritala, Mikko
  • Journal of The Electrochemical Society, Vol. 148, Issue 10
  • DOI: 10.1149/1.1401082

A climbing image nudged elastic band method for finding saddle points and minimum energy paths
journal, December 2000

  • Henkelman, Graeme; Uberuaga, Blas P.; Jónsson, Hannes
  • The Journal of Chemical Physics, Vol. 113, Issue 22, p. 9901-9904
  • DOI: 10.1063/1.1329672

Improved grid-based algorithm for Bader charge allocation
journal, January 2007

  • Sanville, Edward; Kenny, Steven D.; Smith, Roger
  • Journal of Computational Chemistry, Vol. 28, Issue 5
  • DOI: 10.1002/jcc.20575

Well-Ordered Transition Metal Oxide Layers in Model Catalysis – A Series of Case Studies
journal, December 2012

  • Kuhlenbeck, Helmut; Shaikhutdinov, Shamil; Freund, Hans-Joachim
  • Chemical Reviews, Vol. 113, Issue 6
  • DOI: 10.1021/cr300312n

High-precision sampling for Brillouin-zone integration in metals
journal, August 1989


Perfectly Conformal TiN and Al2O3 Films Deposited by Atomic Layer Deposition
journal, January 1999


First-principles study of the reconstruction and hydroxylation of the polar NiO(111) surface
journal, July 2011

  • Ebensperger, Christina; Meyer, Bernd
  • physica status solidi (b), Vol. 248, Issue 10
  • DOI: 10.1002/pssb.201147104

Stability of the polar NiO(111) surface
journal, March 2008

  • Zhang, Wei-Bing; Tang, Bi-Yu
  • The Journal of Chemical Physics, Vol. 128, Issue 12
  • DOI: 10.1063/1.2835544

Hydroxyl groups on oxide surfaces: NiO(100), NiO(111) and Cr2O3(111)
journal, November 1993


Improved tangent estimate in the nudged elastic band method for finding minimum energy paths and saddle points
journal, December 2000

  • Henkelman, Graeme; Jónsson, Hannes
  • The Journal of Chemical Physics, Vol. 113, Issue 22
  • DOI: 10.1063/1.1323224

DFT studies of dry reforming of methane on Ni catalyst
journal, November 2009


Thermal decomposition of methanol absorbed on palladium{111}. A new reaction pathway involving methyl formation
journal, June 1989

  • Levis, Robert J.; Zhicheng, Jiang; Winograd, Nicholas
  • Journal of the American Chemical Society, Vol. 111, Issue 13
  • DOI: 10.1021/ja00195a013

Methanol decomposition on Pd(111) single crystal surfaces
journal, November 1990


Improved tetrahedron method for Brillouin-zone integrations
journal, June 1994


A review of dry (CO 2 ) reforming of methane over noble metal catalysts
journal, January 2014

  • Pakhare, Devendra; Spivey, James
  • Chem. Soc. Rev., Vol. 43, Issue 22
  • DOI: 10.1039/C3CS60395D

Stabilizing Ni Catalysts by Molecular Layer Deposition for Harsh, Dry Reforming Conditions
journal, July 2014

  • Gould, Troy D.; Izar, Alan; Weimer, Alan W.
  • ACS Catalysis, Vol. 4, Issue 8
  • DOI: 10.1021/cs500809w