Application of finite element, phase-field, and CALPHAD-based methods to additive manufacturing of Ni-based superalloys
Journal Article
·
· Acta Materialia
Not Available
- Sponsoring Organization:
- USDOE
- Grant/Contract Number:
- AC02-06CH11357
- OSTI ID:
- 1550537
- Alternate ID(s):
- OSTI ID: 1399128
- Journal Information:
- Acta Materialia, Journal Name: Acta Materialia Journal Issue: C Vol. 139; ISSN 1359-6454
- Publisher:
- ElsevierCopyright Statement
- Country of Publication:
- United States
- Language:
- English
Similar Records
Application of finite element, phase-field, and CALPHAD-based methods to additive manufacturing of Ni-based superalloys
Unexpected δ-Phase Formation in Additive-Manufactured Ni-Based Superalloy
Microstructure-property gradients in Ni-based superalloy (Inconel 738) additively manufactured via electron beam powder bed fusion
Journal Article
·
2017
· Acta Materialia
·
OSTI ID:1399128
+11 more
Unexpected δ-Phase Formation in Additive-Manufactured Ni-Based Superalloy
Journal Article
·
2016
· JOM. Journal of the Minerals, Metals & Materials Society
·
OSTI ID:1324794
+6 more
Microstructure-property gradients in Ni-based superalloy (Inconel 738) additively manufactured via electron beam powder bed fusion
Journal Article
·
2021
· Additive Manufacturing
·
OSTI ID:1797347
+6 more