Diffusion-coupled cohesive interface simulations of stress corrosion intergranular cracking in polycrystalline materials
Journal Article
·
· Acta Materialia
Not Available
- Sponsoring Organization:
- USDOE Office of Nuclear Energy (NE); USDOE Office of Science (SC), Basic Energy Sciences (BES)
- Grant/Contract Number:
- AC05-00OR22725
- OSTI ID:
- 1550387
- Journal Information:
- Acta Materialia, Journal Name: Acta Materialia Journal Issue: C Vol. 136; ISSN 1359-6454
- Publisher:
- ElsevierCopyright Statement
- Country of Publication:
- United States
- Language:
- English
Similar Records
Diffusion-coupled cohesive interface simulations of stress corrosion intergranular cracking in polycrystalline materials
How irradiation promotes intergranular stress corrosion crack initiation
Computer Simulation of Intergranular Stress Corrosion Cracking via Hydrogen Embrittlement
Journal Article
·
2017
· Acta Materialia
·
OSTI ID:1389308
+1 more
How irradiation promotes intergranular stress corrosion crack initiation
Journal Article
·
2024
· Progress in Materials Science
·
OSTI ID:2305778
+17 more
Computer Simulation of Intergranular Stress Corrosion Cracking via Hydrogen Embrittlement
Journal Article
·
2000
· Modelling and Simulation in Materials Science and Engineering
·
OSTI ID:766121