DOE PAGES title logo U.S. Department of Energy
Office of Scientific and Technical Information

Title: Effects of titanium substitutions for aluminum and tungsten in Co-10Ni-9Al-9W (at%) superalloys

Authors:
; ; ; ;
Publication Date:
Sponsoring Org.:
USDOE Office of Science (SC), Basic Energy Sciences (BES)
OSTI Identifier:
1550023
Grant/Contract Number:  
FG02-98ER45721
Resource Type:
Publisher's Accepted Manuscript
Journal Name:
Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing
Additional Journal Information:
Journal Name: Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing Journal Volume: 705 Journal Issue: C; Journal ID: ISSN 0921-5093
Publisher:
Elsevier
Country of Publication:
Netherlands
Language:
English

Citation Formats

Bocchini, Peter J., Sudbrack, Chantal K., Noebe, Ronald D., Dunand, David C., and Seidman, David N. Effects of titanium substitutions for aluminum and tungsten in Co-10Ni-9Al-9W (at%) superalloys. Netherlands: N. p., 2017. Web. doi:10.1016/j.msea.2017.08.034.
Bocchini, Peter J., Sudbrack, Chantal K., Noebe, Ronald D., Dunand, David C., & Seidman, David N. Effects of titanium substitutions for aluminum and tungsten in Co-10Ni-9Al-9W (at%) superalloys. Netherlands. https://doi.org/10.1016/j.msea.2017.08.034
Bocchini, Peter J., Sudbrack, Chantal K., Noebe, Ronald D., Dunand, David C., and Seidman, David N. Fri . "Effects of titanium substitutions for aluminum and tungsten in Co-10Ni-9Al-9W (at%) superalloys". Netherlands. https://doi.org/10.1016/j.msea.2017.08.034.
@article{osti_1550023,
title = {Effects of titanium substitutions for aluminum and tungsten in Co-10Ni-9Al-9W (at%) superalloys},
author = {Bocchini, Peter J. and Sudbrack, Chantal K. and Noebe, Ronald D. and Dunand, David C. and Seidman, David N.},
abstractNote = {},
doi = {10.1016/j.msea.2017.08.034},
journal = {Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing},
number = C,
volume = 705,
place = {Netherlands},
year = {2017},
month = {9}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record
https://doi.org/10.1016/j.msea.2017.08.034

Citation Metrics:
Cited by: 57 works
Citation information provided by
Web of Science

Save / Share:

Works referenced in this record:

A new approach of designing superalloys for low density
journal, January 2010


Cobalt-Base High-Temperature Alloys
journal, April 2006


Modelling of the influence of alloy composition on flow stress in high-strength nickel-based superalloys
journal, August 2014


Effects of quaternary alloying elements on the γ′ solvus temperature of Co–Al–W based alloys with fcc/L12 two-phase microstructures
journal, October 2010

  • Ooshima, Masahiro; Tanaka, Katsushi; Okamoto, Norihiko L.
  • Journal of Alloys and Compounds, Vol. 508, Issue 1
  • DOI: 10.1016/j.jallcom.2010.08.050

Alloying effects in polycrystalline γ′ strengthened Co–Al–W base alloys
journal, May 2014


Creep deformation-induced antiphase boundaries in L1 2 -containing single-crystal cobalt-base superalloys
journal, September 2014


Creep properties of different γ′-strengthened Co-base superalloys
journal, July 2012


Determination of phase equilibria in the Co-rich Co–Al–W ternary system with a diffusion-couple technique
journal, December 2009


Solute partitioning and site preference in γ/γ′ cobalt-base alloys
journal, November 2012


Partition behavior of alloying elements and phase transformation temperatures in Co–Al–W-base quaternary systems
journal, January 2013


A new tungsten-free γ–γ’ Co–Al–Mo–Nb-based superalloy
journal, March 2015


The physical meaning of indentation and scratch hardness
journal, May 1956


Ductility enhancement by boron addition in Co–Al–W high-temperature alloys
journal, September 2009


High resolution energy dispersive spectroscopy mapping of planar defects in L12-containing Co-base superalloys
journal, May 2015


Phase equilibria in the Co-rich Co-Al-W-Ti quaternary system
journal, December 2011


Stacking faults in gamma prime Ni3(Al,Ti) precipitation hardened nickel-base alloys
journal, September 1970

  • Kear, Bernard H.; Oblak, John M.; Giamei, Anthony F.
  • Metallurgical and Materials Transactions B, Vol. 1, Issue 9
  • DOI: 10.1007/BF03038373

The creep deformation behavior of a single-crystal Co–Al–W-base superalloy at 900°C
journal, May 2015


Discontinuous precipitation in ? dilute Co-3% Ti-2% Nb ternary alloy
journal, August 1987

  • Ogender Singh, J.; Purdy, G. R.
  • Journal of Materials Science, Vol. 22, Issue 8
  • DOI: 10.1007/BF01086491

Temperature dependence of deformation behavior in a Co–Al–W-base single crystal superalloy
journal, January 2015


Plastic deformation mechanisms in a crept L12 hardened Co-base superalloy
journal, June 2013


Phase Equilibria and Microstructure on γ′ Phase in Co-Ni-Al-W System
journal, January 2008


Effects of a tungsten addition on the morphological evolution, spatial correlations and temporal evolution of a model Ni–Al–Cr superalloy
journal, February 2008


New Quantitative Analysis of Contributing Factors to Strength of Disk Superalloys
conference, January 2012


High Temperature Creep of New L12 Containing Cobalt-base Superalloys
conference, January 2012


Flow stress anomalies in γ/γ′ two-phase Co–Al–W-base alloys
journal, March 2007


Creep behavior in a γ′ strengthened Co–Al–W–Ta–Ti single-crystal alloy at 1000 °C
journal, March 2015


Synthesis of a new tungsten-free γ–γ′ cobalt-based superalloy by tuning alloying additions
journal, February 2015


Creep deformation of single crystals of new Co–Al–W-based alloys with fcc/L1 2 two-phase microstructures
journal, November 2012


Precipitation and dissolution processes in γ / γ ′ single crystal nickel-based superalloys
journal, November 1998


The mechanism of morphogenesis in a phase-separating concentrated multicomponent alloy
journal, February 2007

  • Mao, Zugang; Sudbrack, Chantal K.; Yoon, Kevin E.
  • Nature Materials, Vol. 6, Issue 3
  • DOI: 10.1038/nmat1845

Microstructural and creep properties of boron- and zirconium-containing cobalt-based superalloys
journal, January 2017

  • Bocchini, Peter J.; Sudbrack, Chantal K.; Noebe, Ronald D.
  • Materials Science and Engineering: A, Vol. 682
  • DOI: 10.1016/j.msea.2016.10.124

Microstructure and creep strength of different γ/γ′-strengthened Co-base superalloy variants
journal, December 2010


Plastic deformation of polycrystals of Co 3 (Al,W) with the L1 2 structure
journal, October 2011


Creep-induced planar defects in L12-containing Co- and CoNi-base single-crystal superalloys
journal, January 2015


Atom-probe tomographic study of γ/γ′ interfaces and compositions in an aged Co–Al–W superalloy
journal, April 2013


New Co-based γ-γ′ high-temperature alloys
journal, January 2010


Creep and directional coarsening in single crystals of new γ–γ′ cobalt-base alloys
journal, April 2012


The kinetics of precipitation from supersaturated solid solutions
journal, April 1961


γ′ Phase Stability and Phase Equilibrium in Ternary Co-Al-W at 900 °C
journal, October 2014

  • Lass, Eric A.; Williams, Maureen E.; Campbell, Carelyn E.
  • Journal of Phase Equilibria and Diffusion, Vol. 35, Issue 6
  • DOI: 10.1007/s11669-014-0346-2

Creep Strength and Microstructure of Polycrystalline γ' - Strengthened Cobalt-base Superalloys
conference, January 2012


Influence of ruthenium on microstructural evolution in a model Co Al W superalloy
journal, September 2016


Improved high temperature γ′ stability of Co–Al–W-base alloys containing Ti and Ta
journal, December 2013