The insulating effect of the low thermal conductivity of epoxy on the resolution of the heat of reaction during polymerization by differential scanning calorimetry
- Authors:
- Publication Date:
- Sponsoring Org.:
- USDOE National Nuclear Security Administration (NNSA)
- OSTI Identifier:
- 1549999
- Grant/Contract Number:
- NA0003525
- Resource Type:
- Publisher's Accepted Manuscript
- Journal Name:
- Thermochimica Acta
- Additional Journal Information:
- Journal Name: Thermochimica Acta Journal Volume: 656 Journal Issue: C; Journal ID: ISSN 0040-6031
- Publisher:
- Elsevier
- Country of Publication:
- Netherlands
- Language:
- English
Citation Formats
Arechederra, Gabriel K., Draelos, Lara R., Ancipink, Windy B., McCoy, John D., and Kropka, Jamie M. The insulating effect of the low thermal conductivity of epoxy on the resolution of the heat of reaction during polymerization by differential scanning calorimetry. Netherlands: N. p., 2017.
Web. doi:10.1016/j.tca.2017.09.001.
Arechederra, Gabriel K., Draelos, Lara R., Ancipink, Windy B., McCoy, John D., & Kropka, Jamie M. The insulating effect of the low thermal conductivity of epoxy on the resolution of the heat of reaction during polymerization by differential scanning calorimetry. Netherlands. https://doi.org/10.1016/j.tca.2017.09.001
Arechederra, Gabriel K., Draelos, Lara R., Ancipink, Windy B., McCoy, John D., and Kropka, Jamie M. Sun .
"The insulating effect of the low thermal conductivity of epoxy on the resolution of the heat of reaction during polymerization by differential scanning calorimetry". Netherlands. https://doi.org/10.1016/j.tca.2017.09.001.
@article{osti_1549999,
title = {The insulating effect of the low thermal conductivity of epoxy on the resolution of the heat of reaction during polymerization by differential scanning calorimetry},
author = {Arechederra, Gabriel K. and Draelos, Lara R. and Ancipink, Windy B. and McCoy, John D. and Kropka, Jamie M.},
abstractNote = {},
doi = {10.1016/j.tca.2017.09.001},
journal = {Thermochimica Acta},
number = C,
volume = 656,
place = {Netherlands},
year = {2017},
month = {10}
}
Free Publicly Available Full Text
Publisher's Version of Record
https://doi.org/10.1016/j.tca.2017.09.001
https://doi.org/10.1016/j.tca.2017.09.001
Other availability
Cited by: 1 work
Citation information provided by
Web of Science
Web of Science
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.