Creep‐fatigue behaviour of single‐crystal Ni‐base superalloy CMSX‐8
- Authors:
-
- The George W. Woodruff School of Mechanical Engineering Georgia Institute of Technology Atlanta Georgia
- The George W. Woodruff School of Mechanical Engineering Georgia Institute of Technology Atlanta Georgia, School of Materials Science and Engineering Georgia Institute of Technology Atlanta Georgia
- Publication Date:
- Sponsoring Org.:
- USDOE
- OSTI Identifier:
- 1544443
- Grant/Contract Number:
- DE‐FE0011722
- Resource Type:
- Publisher's Accepted Manuscript
- Journal Name:
- Fatigue and Fracture of Engineering Materials and Structures
- Additional Journal Information:
- Journal Name: Fatigue and Fracture of Engineering Materials and Structures Journal Volume: 42 Journal Issue: 9; Journal ID: ISSN 8756-758X
- Publisher:
- Wiley-Blackwell
- Country of Publication:
- United Kingdom
- Language:
- English
Citation Formats
Estrada Rodas, Ernesto A., Gorgannejad, Sanam, and Neu, Richard W. Creep‐fatigue behaviour of single‐crystal Ni‐base superalloy CMSX‐8. United Kingdom: N. p., 2019.
Web. doi:10.1111/ffe.13098.
Estrada Rodas, Ernesto A., Gorgannejad, Sanam, & Neu, Richard W. Creep‐fatigue behaviour of single‐crystal Ni‐base superalloy CMSX‐8. United Kingdom. https://doi.org/10.1111/ffe.13098
Estrada Rodas, Ernesto A., Gorgannejad, Sanam, and Neu, Richard W. Tue .
"Creep‐fatigue behaviour of single‐crystal Ni‐base superalloy CMSX‐8". United Kingdom. https://doi.org/10.1111/ffe.13098.
@article{osti_1544443,
title = {Creep‐fatigue behaviour of single‐crystal Ni‐base superalloy CMSX‐8},
author = {Estrada Rodas, Ernesto A. and Gorgannejad, Sanam and Neu, Richard W.},
abstractNote = {},
doi = {10.1111/ffe.13098},
journal = {Fatigue and Fracture of Engineering Materials and Structures},
number = 9,
volume = 42,
place = {United Kingdom},
year = {2019},
month = {7}
}
Free Publicly Available Full Text
Publisher's Version of Record
https://doi.org/10.1111/ffe.13098
https://doi.org/10.1111/ffe.13098
Other availability
Cited by: 1 work
Citation information provided by
Web of Science
Web of Science
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.
Works referenced in this record:
Mean stress effects in strain-life fatigue: MEAN STRESS EFFECTS IN STRAIN-LIFE FATIGUE
journal, October 2009
- Dowling, N. E.
- Fatigue & Fracture of Engineering Materials & Structures, Vol. 32, Issue 12
Mechanism-based life model for out-of-phase thermomechanical fatigue in single crystal Ni-base superalloys: MECHANISM-BASED LIFE MODEL FOR OUT-OF-PHASE THERMOMECHANICAL FATIGUE
journal, March 2012
- Amaro, R. L.; Antolovich, S. D.; Neu, R. W.
- Fatigue & Fracture of Engineering Materials & Structures, Vol. 35, Issue 7
Effects of microstructure in high temperature fatigue: Lifetime to crack initiation of a single crystal superalloy in high temperature low cycle fatigue
journal, December 2013
- Rémy, L.; Geuffrard, M.; Alam, A.
- International Journal of Fatigue, Vol. 57
Elevated-temperature fatigue crack growth
journal, April 1987
- Chan, K. S.; Leverant, G. R.
- Metallurgical and Materials Transactions A, Vol. 18, Issue 4
Thermomechanical fatigue of a directionally-solidified Ni-base superalloy: Smooth and cylindrically-notched specimens
journal, August 2010
- Kupkovits, Robert A.; Neu, Richard W.
- International Journal of Fatigue, Vol. 32, Issue 8
Crack paths in single-crystal Ni-base superalloys under isothermal and thermomechanical fatigue
journal, June 2019
- Neu, Richard W.
- International Journal of Fatigue, Vol. 123
An Experimental Study of the Role of Plasticity in the Rafting Kinetics of a Single Crystal Ni-Base Superalloy
conference, January 1996
- Fahrmann, M.; Fahrmann, E.; Paris, O.
- Superalloys 1996 (Eighth International Symposium)
Low cycle fatigue damage in nickel-base superalloy single crystals at elevated temperature
journal, August 1993
- Fleury, E.; Rémy, L.
- Materials Science and Engineering: A, Vol. 167, Issue 1-2
Tension/compression asymmetry in yield and creep strengths of Ni-based superalloy with a high amount of tantalum
journal, July 2006
- Yamashita, M.; Kakehi, K.
- Scripta Materialia, Vol. 55, Issue 2
Development of the Rhenium Containing Superalloys CMSX-4 & CM 186 LC for Single Crystal Blade and Directionally Solidified Vane Applications in Advanced Turbine Engines
conference, January 1992
- Harris, K.; Erickson, G. L.; Sikkenga, S. L.
- Superalloys 1992 (Seventh International Symposium)
Rhenium additions to a Ni-base superalloy: Effects on microstructure
journal, November 1985
- Giamei, A. F.; Anton, D. L.
- Metallurgical Transactions A, Vol. 16, Issue 11
A microstructure-sensitive constitutive modeling of the inelastic behavior of single crystal nickel-based superalloys at very high temperature
journal, August 2014
- le Graverend, J. -B.; Cormier, J.; Gallerneau, F.
- International Journal of Plasticity, Vol. 59
Influence of orientation on the low cycle fatigue of MAR-M 200 single crystals at 650 °C I: Fatigue life behaviour
journal, July 1991
- Chieragatti, R.; Remy, L.
- Materials Science and Engineering: A, Vol. 141, Issue 1
Fatigue behaviour and lifing of two single crystal superalloys
journal, August 2001
- MacLachlan, D. W.; Knowles, D. M.
-
Fatigue
Fracture of Engineering Materials and Structures, Vol. 24, Issue 8
Formation of Topologically Closed Packed Phases in Nickel Base Single Crystal Superalloys
conference, January 1988
- Darolia, R.; Lahrman, D. F.; Field, R. D.
- Superalloys 1988 (Sixth International Symposium)
The influence of temperature and cyclic frequency on the fatigue fracture of cube oriented nickel-base superalloy single crystals
journal, February 1975
- Leverant, G. R.; Gell, M.
- Metallurgical Transactions A, Vol. 6, Issue 2
Ageing kinetics of Ni-base superalloys
journal, May 2016
- Gorgannejad, Sanam; Estrada Rodas, Ernesto A.; Neu., Richard W.
- Materials at High Temperatures, Vol. 33, Issue 4-5
Creep damage of single-crystal nickel base superalloys: mechanisms and effect on low cycle fatigue
journal, March 2010
- Epishin, Alexander; Link, Thomas; Klingelhöffer, Hellmuth
- Materials at High Temperatures, Vol. 27, Issue 1
The Hotter the Engine, the Better
journal, November 2009
- Perepezko, J. H.
- Science, Vol. 326, Issue 5956
Crystal viscoplasticity model for the creep-fatigue interactions in single-crystal Ni-base superalloy CMSX-8
journal, January 2018
- Estrada Rodas, Ernesto A.; Neu, Richard W.
- International Journal of Plasticity, Vol. 100
Dependence of the high-temperature low-cycle fatigue behaviour of the monocrystalline nickel-base superalloys CMSX-4 and CMSX-6 on the γ/γ′-morphology
journal, November 1999
- Ott, M.; Mughrabi, H.
- Materials Science and Engineering: A, Vol. 272, Issue 1
The Effect of Orientation, Temperature and Gamma Prime Size on the Yield Strength of a Single Crystal Nickel Base Superalloy
conference, January 1984
- Shah, D. M.; Duhl, D. N.
- Superalloys 1984 (Fifth International Symposium)
Thermal barrier coatings for enhanced efficiency of gas turbine engines
journal, December 2006
- Gurrappa, I.; Sambasiva Rao, A.
- Surface and Coatings Technology, Vol. 201, Issue 6
Thermomechanical fatigue and bithermal–thermomechanical fatigue of a nickel-base single crystal superalloy
journal, September 2012
- Amaro, R. L.; Antolovich, S. D.; Neu, R. W.
- International Journal of Fatigue, Vol. 42
Development of Single Crystal Alloys for Specific Engine Applications
conference, January 1984
- Ford, D. A.; Arthey, R. P.
- Superalloys 1984 (Fifth International Symposium)
Fatigue crack path prediction in UDIMET 720 nickel-based alloy single crystals
journal, January 2000
- Reed, P. A. S.; Sinclair, I.; Wu, X. D.
- Metallurgical and Materials Transactions A, Vol. 31, Issue 1
A mechanism governing oxidation-assisted low-cycle fatigue of superalloys
journal, June 2009
- Evans, A. G.; He, M. Y.; Suzuki, A.
- Acta Materialia, Vol. 57, Issue 10
Orientation and temperature dependence of some mechanical properties of the single-crystal nickel-base superalloy René N4: Part II. Low cycle fatigue behavior
journal, March 1986
- Gabb, T. P.; Gayda, J.; Miner, R. V.
- Metallurgical Transactions A, Vol. 17, Issue 3
Low cycle fatigue of MAR-M 200 single crystals with a bimodal γ′ distribution at 760 and 870°C
journal, September 1986
- Milligan, Walter W.; Jayaraman, N.; Hill, Robert C.
- Materials Science and Engineering, Vol. 82
Fatigue Crack Growth Behavior of PWA 1484 Single Crystal Superalloy at Elevated Temperatures
journal, April 1996
- Telesman, J.; Ghosn, L. J.
- Journal of Engineering for Gas Turbines and Power, Vol. 118, Issue 2
A comparative study on thermomechanical and low cycle fatigue failures of a single crystal nickel-based superalloy
journal, December 2011
- Hong, H. U.; Kang, J. G.; Choi, B. G.
- International Journal of Fatigue, Vol. 33, Issue 12
Oxidation-Assisted Crack Growth in Single-Crystal Superalloys during Fatigue with Compressive Holds
journal, November 2017
- Lafata, M. A.; Rettberg, L. H.; He, M. Y.
- Metallurgical and Materials Transactions A, Vol. 49, Issue 1
Understanding the yield behaviour of L1 2 -ordered alloys
journal, August 2016
- Wang-Koh, Y. M.
- Materials Science and Technology, Vol. 33, Issue 8
The Effect of Composition, Misfit, and Heat Treatment on the Primary Creep Behavior of Single Crystal Nickel Base Superalloys PWA 1480 and PWA 1484
conference, January 2008
- Wilson, B. C.; Fuchs, G. E.
- Superalloys 2008 (Eleventh International Symposium)
Interdiffusion in the face-centred cubic phase of the Ni–Re, Ni–Ta and Ni–W systems between 900 and 1300°C
journal, April 2000
- Karunaratne, M. S. A.; Carter, P.; Reed, R. C.
- Materials Science and Engineering: A, Vol. 281, Issue 1-2
The Effect of Secondary Gamma-Prime on the Primary Creep Behavior of Single-Crystal Nickel-Base Superalloys
journal, September 2009
- Wilson, B. C.; Fuchs, G. E.
- Metallurgical and Materials Transactions A, Vol. 41, Issue 5
On the role of incomplete Kear-Wilsdorf locks in the yield stress anomaly of Ni3Al
journal, August 1997
- Caillard, D.; Molénat, G.; Paidar, V.
- Materials Science and Engineering: A, Vol. 234-236
Interaction between oxidation and thermo-mechanical fatigue in IN738LC superalloy — I
journal, June 1995
- Esmaeili, S.; Engler-Pinto, C. C.; Ilschner, B.
- Scripta Metallurgica et Materialia, Vol. 32, Issue 11
Behavior of nickel-base superalloy single crystals under thermal-mechanical fatigue
journal, December 1994
- Fleury, E.; Rémy, L.
- Metallurgical and Materials Transactions A, Vol. 25, Issue 1
Thermo-mechanical fatigue failure of a single crystal Ni-based superalloy
journal, February 2008
- Okazaki, M.; Sakaguchi, M.
- International Journal of Fatigue, Vol. 30, Issue 2
Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
journal, February 2005
- Shenoy, M. M.; Gordon, A. P.; McDowell, D. L.
- Journal of Engineering Materials and Technology, Vol. 127, Issue 3
Low cycle fatigue characteristics of 〈001〉 and randomly aligned superalloy single crystals
journal, October 1984
- Anton, D. L.
- Acta Metallurgica, Vol. 32, Issue 10
Yield stress anomalies in ordered alloys: a review of microstructural findings and related hypotheses
journal, July 2001
- Veyssière, Patrick
- Materials Science and Engineering: A, Vol. 309-310
Thermal Barrier Coatings for Gas-Turbine Engine Applications
journal, April 2002
- Padture, N. P.
- Science, Vol. 296, Issue 5566