Title: Mesopore differences between pillared lamellar MFI and MWW zeolites probed by atomic layer deposition of titania and consequences on photocatalysis

Journal Article · · Microporous and Mesoporous Materials

The pillared MWW (PMWW or MCM-36) and pillared MFI (PMFI) are two prominent representatives of meso-/microporous lamellar zeolites, which are made by pillaring of layered MCM-22(P) and multilamellar MFI precursors, respectively. They both consist of a 10-membered ring sinusoidal micropore channel within each zeolitic layer and mesopore voids created by pillars between two adjacent zeolitic layers. Although catalytic activities of PMWW and PMFI have been compared, identification of mesopore differences between these two pillared lamellar zeolites has not been attempted. In this work, we report the differences in mesopore characteristics between PMWW and PMFI zeolites probed by atomic layer deposition (ALD) of titania (ALD-TiO2) species and a combination of structural, textural, composition and catalytic property analyses of the samples before and after ALD treatment, respectively. The results suggest PMFI has cylindrical mesopores with uniform sizes from pore entrance to main body, while PMWW has ink-bottle mesopores with the neck size much smaller than pore body. The communication between micropore and mesopore in PMFI is direct, but no communication exists in PMWW zeolites. Here, the ALD-TiO2 process considerably modified external surface composition of PMFI and PMWW zeolites, which consequently led to a new application of the pillared lamellar zeolite materials, i.e., photo-catalytically active meso-/microporous zeolites for environmental remedy reactions.

Research Organization:
Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
Sponsoring Organization:
USDOE Office of Energy Efficiency and Renewable Energy (EERE)
Grant/Contract Number:
AC05-00OR22725
OSTI ID:
1507866
Journal Information:
Microporous and Mesoporous Materials, Journal Name: Microporous and Mesoporous Materials Journal Issue: C Vol. 276; ISSN 1387-1811
Publisher:
ElsevierCopyright Statement
Country of Publication:
United States
Language:
English

References (57)

Solution-processable exfoliated zeolite nanosheets purified by density gradient centrifugation journal May 2013
2D Zeolite Coatings: Langmuir-Schaefer Deposition of 3 nm Thick MFI Zeolite Nanosheets journal April 2015
Nanoscale Control of Homoepitaxial Growth on a Two-Dimensional Zeolite journal December 2016
Delaminated Zeolites: Combining the Benefits of Zeolites and Mesoporous Materials for Catalytic Uses journal August 1999
Physical adsorption characterization of nanoporous materials: progress and challenges journal February 2014
Beta Zeolite-Supported Iridium Catalysts by Gas Phase Deposition journal June 2009
Atomic Layer Deposition of Zinc Oxide on HZSM-5 Template and Its Methanol Aromatization Performance journal February 2015
MCM-36: The first pillared molecular sieve with zeoliteproperties book January 1995
Photocatalytic decomposition of 4-nitrophenol over titanium silicalite (TS-1) catalysts journal January 2003
Pore size determination in modified micro- and mesoporous materials. Pitfalls and limitations in gas adsorption data analysis journal June 2003
Synthesis, characterization and catalytic activity of the pillared molecular sieve MCM-36 journal December 1998
Textural and catalytic properties of Mo loaded hierarchical meso-/microporous lamellar MFI and MWW zeolites for direct methane conversion journal January 2014
Influence of layer structure preservation on the catalytic properties of the pillared zeolite MCM-36 journal June 2010
Tuning external surface of unit-cell thick pillared MFI and MWW zeolites by atomic layer deposition and its consequences on acid-catalyzed reactions journal May 2016
Activity and selectivity differences of external Brønsted acid sites of single-unit-cell thick and conventional MFI and MWW zeolites journal December 2014
Effects of TiO 2 in Low Temperature Propylene Epoxidation Using Gold Catalysts journal January 2018
Synthesis and Stabilization of Supported Metal Catalysts by Atomic Layer Deposition journal March 2013
Control of Acid−Base Properties of New Nanocomposite Derivatives of MCM-36 by Mixed Oxide Pillaring journal February 2004
Tuning the Pore Size of Ink-Bottle Mesopores by Atomic Layer Deposition journal May 2012
Synthesis of Organic Pillared MFI Zeolite as Bifunctional Acid–Base Catalyst journal February 2015
Mesopore-Modified Zeolites:  Preparation, Characterization, and Applications journal March 2006
Understanding TiO 2 Photocatalysis: Mechanisms and Materials journal May 2014
Atomic Layer Deposition: An Overview journal January 2010
Catalytic Behavior of Brønsted Acid Sites in MWW and MFI Zeolites with Dual Meso- and Microporosity journal December 2010
Catalyst Design with Atomic Layer Deposition journal February 2015
Vibrational Structure of Titanium Silicate Catalysts. A Spectroscopic and Theoretical Study journal November 2001
Layer Structure Preservation during Swelling, Pillaring, and Exfoliation of a Zeolite Precursor journal January 2008
Multifunctional Hybrid Organic−Inorganic Catalytic Materials with a Hierarchical System of Well-Defined Micro- and Mesopores journal October 2010
Delamination of Layered Zeolite Precursors under Mild Conditions: Synthesis of UCB-1 via Fluoride/Chloride Anion-Promoted Exfoliation journal March 2011
Hierarchical Hybrid Organic–Inorganic Materials with Tunable Textural Properties Obtained Using Zeolitic-Layered Precursor journal January 2014
Pillared MFI Zeolite Nanosheets of a Single-Unit-Cell Thickness journal March 2010
New Aluminosilicate and Titanosilicate Delaminated Materials Active for Acid Catalysis, and Oxidation Reactions Using H 2 O 2 journal March 2000
Adsorption by MFI-type zeolites examined by isothermal microcalorimetry and neutron diffraction. 2. Nitrogen and carbon monoxide journal July 1993
Adsorption Hysteresis of Nitrogen and Argon in Pore Networks and Characterization of Novel Micro- and Mesoporous Silicas journal January 2006
Delaminated zeolite precursors as selective acidic catalysts journal November 1998
Stable single-unit-cell nanosheets of zeolite MFI as active and long-lived catalysts journal September 2009
Structural analysis of hierarchically organized zeolites journal October 2015
Catalytic activation of OKO zeolite with intersecting pores of 10- and 12-membered rings using atomic layer deposition of aluminium journal January 2014
Catalytic consequences of micropore topology, mesoporosity, and acidity on the hydrolysis of sucrose over zeolite catalysts journal January 2014
Application of quasi-equilibrated thermodesorption of linear and di-branched paraffin molecules for detailed porosity characterization of the mono-layered zeolite MCM-56, in comparison with MCM-22 and ZSM-5 journal January 2014
High-resolution adsorption analysis of pillared zeolites IPC-3PI and MCM-36 journal January 2014
Synthesis and catalytic properties of multilayered MEL-type titanosilicate nanosheets journal January 2015
Tailoring and visualizing the pore architecture of hierarchical zeolites journal January 2015
Layer like porous materials with hierarchical structure journal January 2016
Recent advances in the textural characterization of hierarchically structured nanoporous materials journal January 2017
External surface and pore mouth catalysis in hydrolysis of inulin over zeolites with different micropore topologies and mesoporosities journal January 2017
Surfactant-free synthesis of hollow mesoporous organosilica nanoparticles with controllable particle sizes and diversified organic moieties journal January 2016
Synthesis of titanosilicate pillared MFI zeolite as an efficient photocatalyst journal January 2017
Exfoliation of two-dimensional zeolites in liquid polybutadienes journal January 2017
Degradation reaction of monoethanolamine using TS-1 zeolite as a photocatalyst journal January 1999
Tailoring nanoporous materials by atomic layer deposition journal January 2011
Layered zeolitic materials: an approach to designing versatile functional solids journal January 2014
Dispersible Exfoliated Zeolite Nanosheets and Their Application as a Selective Membrane journal October 2011
Synthesis of Self-Pillared Zeolite Nanosheets by Repetitive Branching journal June 2012
Two-Stage Crystallization of Meso- and Macroporous MFI and MEL Zeolites Using Tributylamine-Derived Diquaternary Ammonium Cations as Organic Structure-Directing Agents journal May 2017
Physisorption of gases, with special reference to the evaluation of surface area and pore size distribution (IUPAC Technical Report) journal October 2015
Layered Materials with Catalytic Applications: Pillared and Delaminated Zeolites from MWW Precursors journal January 2012

Cited By (1)