Synthesis Gas Conversion over Rh-Mn-WxC/SiO2 Catalysts Prepared by Atomic Layer Deposition
- Univ. of Wisconsin, Madison, WI (United States). Dept. of Chemical and Biological Engineering; University of Wisconsin-Madison Department of Chemical and Biological Engineering
- Univ. of Wisconsin, Madison, WI (United States). Dept. of Chemical and Biological Engineering
- Univ. of Wisconsin, Madison, WI (United States). Dept. of Chemical and Biological Engineering. Dept. of Chemistry
The catalytic conversion of synthesis gas to value-added oxygenates and light hydrocarbons was studied here on Rh and Rh–Mn clusters on tungsten carbide-overcoated silica (WxC/SiO2) at 523 K, 580 psi, and CO/H2 = 1/1. The WxC-modified SiO2 support was prepared by the overcoating of WOx on SiO2 using atomic layer deposition (ALD) followed by carburization. The reactivities of Rh/WxC/SiO2 catalysts with varying number of ALD cycles (number of cycles = 2, 5, 10, 20, and 30) were measured and showed that 5 ALD cycles of WxC suppressed the formation of methane. All WxC-modified catalysts showed enhancement in selectivity toward methanol and ethanol through CO hydrogenation and acetaldehyde hydrogenation, respectively. These catalysts also improved the overall turnover frequency (TOF). The addition of Mn species further promoted the activity and the selectivity toward ethanol and C2+ hydrocarbons, especially light alkenes. The best performing Rh-2Mn/5cycle-WxC/SiO2 catalyst (Rh:Mn molar ratio = 1:2) achieved 84.7% selectivity toward valuable oxygenates and C2+ hydrocarbons with a ratio of alkenes to alkanes equal to 1.7, compared to Rh/SiO2 which exhibited 80.4% selectivity toward the products aforementioned with a ratio of 0.5. The overall TOF was 20 times higher than that over Rh/SiO2 (i.e., 5.6 × 10–2 s–1 vs 2.9 × 10–3 s–1). X-ray diffraction revealed that the existence of W2C, which was the dominant phase in Rh/5cycle-WxC/SiO2, favored the suppression of methane and enhanced the production of alcohols and C2+ hydrocarbons compared to the WC support. Density functional theory calculations for Rh19, Rh31, and Rh37 clusters on various WC surfaces suggested that the shape of Rh clusters is condition dependent and subject to H2 pressure. The C- and O- binding energies on various sites for the clusters were used with scaling relations to probe their catalytic activity. With the use of this approach, the increase in the O binding energy when moving from the SiO2-supported Rh37 cluster to the WC-supported cluster leads to an increase in the activity of Rh/WxC/SiO2 at the expense of the reduction in the number of sites that are selective toward C2 oxygenates.
- Research Organization:
- Univ. of Wisconsin, Madison, WI (United States)
- Sponsoring Organization:
- USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22); USDOE Office of Energy Efficiency and Renewable Energy (EERE), Bioenergy Technologies Office (EE-3B); USDOE Office of Science (SC), Biological and Environmental Research (BER) (SC-23); National Science Foundation (NSF) (United States)
- Grant/Contract Number:
- FG02-05ER15731; EE0006878; AC02-06CH11357; AC02-05CH11231
- OSTI ID:
- 1494808
- Journal Information:
- ACS Catalysis, Journal Name: ACS Catalysis Journal Issue: 11 Vol. 8; ISSN 2155-5435
- Publisher:
- American Chemical Society (ACS)Copyright Statement
- Country of Publication:
- United States
- Language:
- English
Similar Records
Spectroscopic evidence for Rh-CO-Zr sup 4+ surface species formed on Rh/ZrO sub 2 catalyst
Identifying higher oxygenate synthesis sites in Cu catalysts promoted and stabilized by atomic layer deposited Fe2O3