Title: Atomic layer deposition of titanium nitride for quantum circuits

Journal Article · · Applied Physics Letters
DOI: https://doi.org/10.1063/1.5053461 · OSTI ID:1488382

Superconducting thin films with high intrinsic kinetic inductance are of great importance for photon detectors, achieving strong coupling in hybrid systems, and protected qubits. We report on the performance of titanium nitride resonators, patterned on thin films (9–110 nm) grown by atomic layer deposition, with sheet inductances of up to 234 pH/. For films thicker than 14 nm, quality factors measured in the quantum regime range from 0.2 to 1.0 × 106 and are likely limited by dielectric two-level systems. Additionally, we show characteristic impedances up to 28 kΩ, with no significant degradation of the internal quality factor as the impedance increases. In conclusion, these high impedances correspond to an increased single photon coupling strength of 24 times compared to a 50 Ω resonator, transformative for hybrid quantum systems and quantum sensing.

Research Organization:
Argonne National Lab. (ANL), Argonne, IL (United States)
Sponsoring Organization:
Army Research Office; National Science Foundation (NSF); USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22). Materials Sciences & Engineering Division
Grant/Contract Number:
AC02-06CH11357
OSTI ID:
1488382
Journal Information:
Applied Physics Letters, Journal Name: Applied Physics Letters Journal Issue: 21 Vol. 113; ISSN 0003-6951
Publisher:
American Institute of Physics (AIP)Copyright Statement
Country of Publication:
United States
Language:
English

References (46)

Kinetic Inductance Parametric Up-Converter journal November 2015
Room temperature oxidation behavior of TiN thin films journal January 1999
A broadband superconducting detector suitable for use in large arrays journal October 2003
Coherent suppression of electromagnetic dissipation due to superconducting quasiparticles journal April 2014
Superconducting nanowires as quantum phase-slip junctions journal February 2006
A wideband, low-noise superconducting amplifier with high dynamic range journal July 2012
Charge quantum interference device journal April 2018
Coherent spin–photon coupling using a resonant exchange qubit journal July 2018
Improving the coherence time of superconducting coplanar resonators journal December 2009
Titanium nitride oxidation chemistry: An x‐ray photoelectron spectroscopy study journal October 1992
Low loss superconducting titanium nitride coplanar waveguide resonators journal December 2010
Study of loss in superconducting coplanar waveguide resonators journal March 2011
Planar superconducting resonators with internal quality factors above one million journal March 2012
Etch induced microwave losses in titanium nitride superconducting resonators journal June 2012
Radiation-suppressed superconducting quantum bit in a planar geometry journal February 2013
Improved superconducting qubit coherence using titanium nitride journal July 2013
Room temperature deposition of sputtered TiN films for superconducting coplanar waveguide resonators journal December 2013
High-Kinetic-Inductance Superconducting Nanowire Resonators for Circuit QED in a Magnetic Field journal April 2016
Structure and properties of TiN ( 111 ) ∕ Si x N y ∕ TiN ( 111 ) interfaces in superhard nanocomposites: First-principles investigations journal July 2006
Direct observation of the superconducting gap in a thin film of titanium nitride using terahertz spectroscopy journal November 2012
Electrodynamic response and local tunneling spectroscopy of strongly disordered superconducting TiN films journal November 2013
Understanding degenerate ground states of a protected quantum circuit in the presence of disorder journal September 2014
Universal scaling of the critical temperature for thin films near the superconducting-to-insulating transition journal December 2014
Metastable Superconducting Qubit journal January 2010
Strongly Disordered TiN and NbTiN s -Wave Superconductors Probed by Microwave Electrodynamics journal September 2012
Protected Josephson Rhombus Chains journal April 2014
Demonstration of Protection of a Superconducting Qubit from Energy Decay journal April 2018
Realization of a Λ System with Metastable States of a Capacitively Shunted Fluxonium journal April 2018
Anomalous Proximity Effect in an Inhomogeneous Disordered Superconductor journal November 2004
Hybrid quantum circuits: Superconducting circuits interacting with other quantum systems journal April 2013
Microwave Properties of Superconducting Atomic-Layer Deposited TiN Films journal June 2013
Superconducting TiN Films Sputtered Over a Large Range of Substrate DC Bias journal June 2015
Stress modulation of titanium nitride thin films deposited using atomic layer deposition
  • Nahar, Manuj; Rocklein, Noel; Andreas, Michael
  • Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Vol. 35, Issue 1 https://doi.org/10.1116/1.4972859
journal January 2017
Strong spin-photon coupling in silicon journal January 2018
A Wideband, Low-Noise Superconducting Amplifier with High Dynamic Range text January 2012
A metastable superconducting qubit text January 2009
Low Loss Superconducting Titanium Nitride Coplanar Waveguide Resonators text January 2010
Planar Superconducting Resonators with Internal Quality Factors above One Million text January 2012
Hybrid quantum circuits: Superconducting circuits interacting with other quantum systems text January 2012
Strongly disordered TiN and NbTiN s-wave superconductors probed by microwave electrodynamics text January 2012
Etch Induced Microwave Losses in Titanium Nitride Superconducting Resonators text January 2012
Direct observation of the superconducting gap in thin film of titanium nitride using terahertz spectroscopy text January 2012
Protected Josephson Rhombi Chains text January 2013
Superconducting TiN Films Sputtered over a Large Range of Substrate DC Bias text January 2014
Strong spin-photon coupling in silicon text January 2017
Anomalous proximity effect in an inhomogeneous disordered superconductor text January 2004

Cited By (14)

Coupling a single electron on superfluid helium to a superconducting resonator journal November 2019
Materials loss measurements using superconducting microwave resonators journal September 2020
Electrically driven optical interferometry with spins in silicon carbide text January 2019
Measurement-induced steering of quantum systems text January 2019
Cryogenic microwave-to-optical conversion using a triply-resonant lithium niobate on sapphire transducer preprint January 2020
Coupling a single electron on superfluid helium to a superconducting resonator journal November 2019
Granular aluminium as a superconducting material for high-impedance quantum circuits journal April 2019
An aluminium superinductor journal July 2019
High kinetic inductance microwave resonators made by He-Beam assisted deposition of tungsten nanowires journal March 2019
Simple non-galvanic flip-chip integration method for hybrid quantum systems journal April 2019
Scanning tunneling Andreev microscopy of titanium nitride thin films journal December 2019
Electrically driven optical interferometry with spins in silicon carbide journal November 2019
Cryogenic characterization of titanium nitride thin films journal January 2019
Electrically driven optical interferometry with spins in silicon carbide text January 2019