Title: Temporal and thermal evolutions of surface Sr-segregation in pristine and atomic layer deposition modified La 0.6 Sr 0.4 CoO 3−δ epitaxial films

The bulk-to-surface Sr segregation vs. temperature and time in La 0.6 Sr 0.4 CoO 3−δ have been studied. The atomic fraction of surface-Sr was effectively reduced by atomic layer deposition of ZrO 2 overcoat.
Authors:
ORCiD logo [1] ; ORCiD logo [1] ; ORCiD logo [2] ; ORCiD logo [3] ; ORCiD logo [4] ; ORCiD logo [1]
  1. Department of Mechanical Engineering, University of South Carolina, Columbia, USA
  2. Department of Mechanical Engineering, University of South Carolina, Columbia, USA, Materials Sciences and Technology Division
  3. Materials Sciences and Technology Division, Oak Ridge National Laboratory, Oak Ridge, USA
  4. Advanced Light Source, Lawrence Berkeley National Laboratory, Berkeley, USA
Publication Date:
Grant/Contract Number:
AC02-05CH11231
Type:
Publisher's Accepted Manuscript
Journal Name:
Journal of Materials Chemistry A
Additional Journal Information:
Journal Name: Journal of Materials Chemistry A Journal Volume: 6 Journal Issue: 47; Journal ID: ISSN 2050-7488
Publisher:
Royal Society of Chemistry (RSC)
Sponsoring Org:
USDOE Office of Science (SC), Basic Energy Sciences (BES) (SC-22)
Country of Publication:
United Kingdom
Language:
English
OSTI Identifier:
1482846

Wen, Yeting, Yang, Tianrang, Lee, Dongkyu, Lee, Ho Nyung, Crumlin, Ethan J., and Huang, Kevin. Temporal and thermal evolutions of surface Sr-segregation in pristine and atomic layer deposition modified La 0.6 Sr 0.4 CoO 3−δ epitaxial films. United Kingdom: N. p., Web. doi:10.1039/C8TA08355J.
Wen, Yeting, Yang, Tianrang, Lee, Dongkyu, Lee, Ho Nyung, Crumlin, Ethan J., & Huang, Kevin. Temporal and thermal evolutions of surface Sr-segregation in pristine and atomic layer deposition modified La 0.6 Sr 0.4 CoO 3−δ epitaxial films. United Kingdom. doi:10.1039/C8TA08355J.
Wen, Yeting, Yang, Tianrang, Lee, Dongkyu, Lee, Ho Nyung, Crumlin, Ethan J., and Huang, Kevin. 2018. "Temporal and thermal evolutions of surface Sr-segregation in pristine and atomic layer deposition modified La 0.6 Sr 0.4 CoO 3−δ epitaxial films". United Kingdom. doi:10.1039/C8TA08355J.
@article{osti_1482846,
title = {Temporal and thermal evolutions of surface Sr-segregation in pristine and atomic layer deposition modified La 0.6 Sr 0.4 CoO 3−δ epitaxial films},
author = {Wen, Yeting and Yang, Tianrang and Lee, Dongkyu and Lee, Ho Nyung and Crumlin, Ethan J. and Huang, Kevin},
abstractNote = {The bulk-to-surface Sr segregation vs. temperature and time in La 0.6 Sr 0.4 CoO 3−δ have been studied. The atomic fraction of surface-Sr was effectively reduced by atomic layer deposition of ZrO 2 overcoat.},
doi = {10.1039/C8TA08355J},
journal = {Journal of Materials Chemistry A},
number = 47,
volume = 6,
place = {United Kingdom},
year = {2018},
month = {12}
}

Works referenced in this record:

Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides
journal, September 1976

Enhanced oxygen reduction activity on surface-decorated perovskite thin films for solid oxide fuel cells
journal, January 2011
  • Mutoro, Eva; Crumlin, Ethan J.; Biegalski, Michael D.
  • Energy & Environmental Science, Vol. 4, Issue 9, p. 3689-3696
  • DOI: 10.1039/c1ee01245b