Title: Janus Membranes via Diffusion-Controlled Atomic Layer Deposition

Authors:
 [1] ;  [2] ;  [3] ;  [4] ;  [3] ; ORCiD logo [5]
  1. Institute for Molecular Engineering, University of Chicago, 5640 South Ellis Avenue Chicago IL 60637 USA, Center for Nanoscale Materials, Argonne National Laboratory, 9700 South Cass Avenue Argonne IL 60439 USA
  2. Center for Nanoscale Materials, Argonne National Laboratory, 9700 South Cass Avenue Argonne IL 60439 USA
  3. Applied Materials Division, Argonne National Laboratory, 9700 South Cass Avenue Argonne IL 60439 USA
  4. Institute for Molecular Engineering, University of Chicago, 5640 South Ellis Avenue Chicago IL 60637 USA, Materials Science Division, Argonne National Laboratory, 9700 South Cass Avenue Argonne IL 60439 USA
  5. Institute for Molecular Engineering, University of Chicago, 5640 South Ellis Avenue Chicago IL 60637 USA, Center for Nanoscale Materials, Argonne National Laboratory, 9700 South Cass Avenue Argonne IL 60439 USA, Institute for Molecular Engineering, Argonne National Laboratory, 9700 South Cass Avenue Argonne IL 60439 USA
Publication Date:
Grant/Contract Number:
AC02-06CH11357
Type:
Publisher's Accepted Manuscript
Journal Name:
Advanced Materials Interfaces
Additional Journal Information:
Journal Volume: 5; Journal Issue: 15; Related Information: CHORUS Timestamp: 2018-08-09 06:41:28; Journal ID: ISSN 2196-7350
Publisher:
Wiley Blackwell (John Wiley & Sons)
Sponsoring Org:
USDOE
Country of Publication:
Germany
Language:
English
OSTI Identifier:
1452659