Atomic layer deposition of alternative glass microchannel plates
Journal Article
·
· Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
- Incom, Inc., 294 Southbridge Road, Charlton, Massachusetts 01507
- Argonne National Laboratory, 9700 S. Cass Ave., Argonne, Illinois 60439
- Space Sciences Laboratory, University of California, 7 Gauss Way, Berkeley, California 94720
Not Available
- Sponsoring Organization:
- USDOE
- Grant/Contract Number:
- SC0009717; SC0011262
- OSTI ID:
- 1421138
- Journal Information:
- Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Journal Name: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films Journal Issue: 1 Vol. 34; ISSN 0734-2101; ISSN JVTAD6
- Publisher:
- American Vacuum SocietyCopyright Statement
- Country of Publication:
- United States
- Language:
- English
Similar Records
Atomic layer deposition of alternative glass microchannel plates
Application of atomic layer deposited microchannel plates to imaging photodetectors with high time resolution
Performance studies of atomic layer deposited microchannel plate electron multipliers
Journal Article
·
2016
· Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films
·
OSTI ID:22489761
+11 more
Application of atomic layer deposited microchannel plates to imaging photodetectors with high time resolution
Journal Article
·
2015
· Nuclear Instruments and Methods in Physics Research. Section A, Accelerators, Spectrometers, Detectors and Associated Equipment
·
OSTI ID:1247270
+11 more
Performance studies of atomic layer deposited microchannel plate electron multipliers
Journal Article
·
2017
· Nuclear Instruments and Methods in Physics Research. Section A, Accelerators, Spectrometers, Detectors and Associated Equipment
·
OSTI ID:1500110
+4 more